IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 198 documents. Displaying 25 entries per page.


Inhibition of Basidiospore Germination by Copper from MCQ, ACQ and CCA Leachates
2012 - IRG/WP 12-10778
The long-term decay resistance of refractory wood shell-treated with chromated copper arsenate (CCA) in above-ground exposures has been attributed to mobile copper that migrates into checks and inhibits the germination of basidiospores. Copper from micronized copper quat (MCQ) has also been shown to migrate into checks suggesting similar performance as a shell treatment, but questions have been ra...
R Stirling, J Drummond, P I Morris


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


The effects of acetylation level on the growth of Postia placenta over 36 weeks
2012 - IRG/WP 12-40589
Genomic sequencing gives us a tool to systematically and rapidly discover novel genes, how their products function in the cell, and explore their interactions. When the DNA sequences are known, primers can be designed to detect transcripts of genes with gene products related to basic cellular processes and hyphal growth. The characteristic gene products induced in different fungi by different wood...
A Pilgård, G Alfredsen, C G Fossdal, C J Long II


Effect of growth rate and radial position on the natural durability of Douglas-fir
2012 - IRG/WP 12-10791
In terms of natural durability, Douglas-fir (Pseudotsuga menziesii (Mirb.) Franco) fame owns to the favourable characteristics of centuries-old trees harvested in old-growth North American forests. The properties of wood coming from plantations harvested between 50 and 100 years-old are likely to be different. In such stands, plantation density and thinning intensity may have a large impact on the...
C Pollet, J-M Henin, B Jourez, J Hébert


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Service life evaluation of wood - an engineering approach
2013 - IRG/WP 13-20515
A performance-based service life design format based on climatic exposure on one hand and “biological wood resistance” on the other hand is presented in this paper. Important concepts are the introduction of limit states as well as reliable performance models for the biological processes, by which onset of deterioration can be predicted for arbitrary climate histories. Examples of applications...
S Thelandersson


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


A guideline for sorting easy to impregnate Scots pine sapwood based on three treatability studies from Northern Europe
2014 - IRG/WP 14-40669
Scots pine sapwood is generally considered an easy to impregnate wood species, though it reportedly faces challenges towards a homogeneous impregnation and large variations in treatability are reported for the material. This study comprises the results of three treatability tests that were performed on Scots pine (Pinus sylvestris) sapwood. The material impregnated was originated from a large ...
K Zimmer, E Larnøy, A Treu


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Interaction between Aspergillus niger fungus and other filamentous fungi on salt-agar medium and their growth on natural wood and wood treated with fungicide
2015 - IRG/WP 15-20569
Aspergillus niger (An) is very often used alone or in mixture with other filamentous fungi of the genus in testing biocides in disinfection procedures, safety, hygiene, medical fields as well as for testing resistance of wood and wood-based materials to moulds. Softwood species as well as hardwood are overgrown with An fungus very easily, causing drop of mainly the aesthetic value of wood product....
A Fojutowski, A Kropacz, A Koziróg


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Formation of biofinishes on outdoor exposed wood; the impact of wood-oil combination and geographical location
2016 - IRG/WP 16-10864
Growth of dark moulds enables the use of a decorative and protective biofinish for wood, showing advantages compared to traditional wood-coatings in terms of sustainability and self-repair. Based on the formation of a uniform mould covering on oil treated wood during outdoor exposure, the utilisation of a biofinish is in development. Basic information is lacking on the correlation between exposure...
E J van Nieuwenhuijzen, L Ross Gobakken, M F Sailer, R A Samson, O C G Adan


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Studying fungal growth using automated image analysis and computer simulations
2016 - IRG/WP 16-20590
Wooden materials are prone to fungal attack resulting in damage and economic losses. Therefore many efforts have been made to understand the degradation of wood and to avoid the adverse effect of fungi. Even though the extent of degradation of a material is inversely proportional to the extension of the fungi attacking it, most researchers focus mainly on the former, leaving the study of the latte...
G Vidal-Diez de Ulzurrun, J M Baetens, J Van den Bulcke, B De Baets


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Previous Page | Next Page