Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


Upgrading the fungal resistance of OSB
1999 - IRG/WP 99-40138
There is a perception that oriented strand board (OSB) is less resistant to fungl than plywood under conditions of moderate exposure to moisture. Douglas fir-faced plywood (DFP) has been suggested as a benchmark for acceptable durability under such conditions. This project was initiated to determine the minimum level of low-toxicity chemical treatment needed to upgrade the fungal resistance of OSB...
P I Morris, J E Clark, D Minchin, R Wellwood


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Performance of above ground decay test units treated with a substituted isothiazolone
1989 - IRG/WP 3503
RH 287, a substituted isothiazolone, was evaluated for efficacy against decay fungi in an above ground test in Mississippi. After 45 months of exposure, all test units that were pressure treated with this biocide at levels of 0.026 pcf and higher have no deterioration. In addition, the test units that were dip-treated with a solution concentration of 0.5% also have no deterioration. Compared to pe...
D D Nicholas, J A Wilson, D E Greenley


Acoustic technique for assessing decay in preservative treated wood
1998 - IRG/WP 98-20138
This study investigated the suitability of vibration techniques to assess the performance of wood preservatives in ground contact. Small stakes (10 x 5 x 100 mm3) of treated and untreated Scots pine sapwood were exposed to decay in lab-scale terrestrial ecosystems. Tests were conducted using three different soils including a garden compost soil, and soils obtained from a test field and a conifer f...
L Machek, M-L Edlund, R Sierra-Alvarez, H Millitz


Influence of the nature of the substrate and the method of inoculation on the degradative activity of soft rot fungi
1998 - IRG/WP 98-20133
The European Standard (ENV-807) determines the threshold of effectiveness of wood preservatives against the action of soft rot Ascomycetes fungi. Its application in the treatment of wood used in the hazard class 4 does not always offer repeatable results, which could be expected in an experimental norm. For this reason, in this paper, we have evaluated the diverse variables that might influence t...
M T De Troya, A M Navarrete, F Rubio, J Jiménez, D Muñoz-Mingarro, C Rodríguez-Borrajo, F Llinares, M Yuste


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


New method to find out the volatile organic compounds (VOC) of wooden material
2000 - IRG/WP 00-20189
Volatile organic compounds (VOC) of pine, spruce and larch wood were studied using a new technique developed at VTT Chemical Technology. 50 mg of crushed wood material was placed into glass tubes. The tubes were closed with a glass wool, which is pressed with a tube cap. Wood samples were analysed with a gas chromatograph after thermal desorption using four different temperatures (50°C, 100°C, 1...
H Viitanen, K Villberg, K Saarela


Estimating the size of subterranean termite colonies by a release-recapture technique
1980 - IRG/WP 1112
The technique is described and the results of an exploratory field trial are presented. The colony size estimate from weekly termite collections varied considerably, but nevertheless permitted assigning termites at three locations to three categories of greatly different colony size. The sizes of the three estimates were much greater than anticipated and included a multimillion termite complex of ...
G R Esenther


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


The results of detection on CCA components of the soils contacted with CCA-treated woods - A trial study for the availability of the burial Method as a disposal CCA treated wood waste
1993 - IRG/WP 93-50005
The objecteve of this experiment is to get a knowledge that, when CCA treated wood wastes were buried in a soil as a disposal, the soil would be or not be contaminated by the components of CCA preservatives in wood wastes. The specimens used were cutting logs and chips made of the CCA treated electric pole waste. The soil was buried to the 15 cm depth and the log specimens were set in the soil for...
K Suzuki, H Sonobe


Termite resistance of borate-treated lumber in a three-year above-ground field test in Hawaii
2000 - IRG/WP 00-30236
A protected above-ground field test simulating the sill plate (dodai) used in conventional Japanese housing construction was established in both Hawaii and Japan to examine the efficacy of disodium octaborate tetrahydrate (DOT, 2% and 3% shell and through) wood treatments. In Hawaii, chromated copper arsenate (CCA, 4 kg/m3) and ammoniacal copper zinc arsenate (ACZA, 4 kg/m3) were included in the t...
J K Grace, R J Oshiro, A Byrne, P I Morris, K Tsunoda


Borate Protection and Termites: Variation in Protection Thresholds Explained
2006 - IRG/WP 06-20324
Laboratory and field data reported in the literature are confusing with regard to ‘adequate’ protection thresholds for borate timber preservatives against subterranean termites. The confusion is compounded by differences in termite species, timber species and test methodology. Laboratory data indicate a borate retention of 0.5% mass/mass (m/m) boric acid equivalent (BAE) would cause > 90% t...
B C Peters, C J Fitzgerald


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Predicting the decay resistance of timber above-ground: 1. Climate effects
2006 - IRG/WP 06-20330
Despite the benefits of using timber as a building product, it is disadvantaged by current Australian Standard durability classifications which lack the sensitivity desired by engineers and architects. To address the need for more sensitive timber service-life information in Australia, an above-ground durability research program was established in 1987. One focus of research is the relationship be...
L P Francis, J Norton


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...