BRE Experience in monitoring decay in out-of-ground exposure trials
1995 - IRG/WP 95-20077
The outdoor field trial has always been regarded as the ultimate test of performance for assessing the effectiveness of a wood preservative. For this reason, the Building Research Establishment (BRE) has invested much effort in such trials over many years. Emphasis in early trials was on ground contact tests which were the basis both for assessing the likely performance of a preservative in protec...
J K Carey, R J Orsler


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


A below-ground exposure method for determining the resistance of woody and non-woody materials to attack by subterranean termites
1993 - IRG/WP 93-10012
With existing field test procedures, in which specimens are installed vertically to some of their length into the ground and spaced out from each other ("grave-yard" tests), variations in the rate of contact by termites between replicates can be common. Mechanical damage to specimens during inspection and re-installation may also be difficult to avoid. A new field test method, evaluated in Austral...
M Lenz, J W Creffield


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 476
Results of a detailed study on the vertical distribution of fouling and wood-boring organisme of Trondheimefjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15-3-1977 to 15-7-1977 (Series I) and from 22-7-1977 to 13-3-1978 (Series II). The intensity of fouling generally decreased with increasing...
L N Santhakumaran


Marine trials with ammoniacal wood preservatives
1980 - IRG/WP 423
Ammoniacal wood preservatives have been known for many years and are considered among the best water-borne systems for protecting wood in ground contact. In recent years attention has been increasingly focussed on these preservatives because of their ability to penetrate difficult-to-treat species better than most other fixed water-borne preservatives. This is particularly important for example, i...
M A Hulme, D P Ostaff


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 2: Comparison of Static and Dynamic Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20320
In routine in-ground stake tests of wood preservatives at the BAM test field Horstwalde and in the BAM fungus cellar periodical determinations of both static moduli of elasticity (MOE) on the basis of bending tests and dynamic MOE on the basis of the vibration method were performed as a possible method for the assessment of fungal attack. As expected from other publications, the absolute values of...
M Grinda, S Göller


Raising of the grain and deformation of Scots pine (Pinus sylvestris) treated with water-borne preservatives
1987 - IRG/WP 3456
In Sweden partial impregnation to 10 mm depth of the pine sapwood (class B in the Nordic preservation standard) of joineries was introduced during the seventies. To avoid product quality problems, organic solvent-based systems have been used. However, the Swedish industry today has problems with organic solvents, mainly for environmental reasons. We have studied raising of the grain and deformatio...