IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 919 documents. Displaying 25 entries per page.


A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Proposing innovative technologies in the control of dry-wood insects
1985 - IRG/WP 1262
This paper discusses the social-economic problems involved in the biological evaluation of dry-wood insects with particular reference to Nigeria. It also discusses prospects of applying non-conventional methods of control against such insects, integrating these with the conventional preservatives as a control strategy. This discussion follows attempts made to identify the major dry-wood insects in...
M O Akanbi


The effect of composition on the effectiveness and fixation of CCA and copper/chrome preservatives. Part 1: Effectiveness. Part 2: Selective absorption and fixation
1973 - IRG/WP 324
A preliminary study of a wide range of copper-chrome-arsenic formulations indicates that the most effective are in the region, CuSO4 · 5H2O - 35 to 45 per cent; K2Cr2O7 - 40 per cent and above; As2O5 · 2H2O - 25 to 15 per cent or less. Effectiveness appears to depend more on the copper content than the copper - arsenic. Observations on selective absorption and leaching suggest that the chromium ...
D N R Smith, A I Williams


Treatment of refractory timbers
1993 - IRG/WP 93-40001
Worldover crisis of wood is being felt due to the global environmental problems. Wood preservation technology plays a good role in curtailing the demands of wood for replacement by prolonging the service life of the timber and thus indirectly helps in saving the environment. Some species of timbers which could not be treated to the desired level by virtue of their refractory nature by any of the c...
I Dev, S Kumar


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


A suggested method to ascertain the toxicity of wood preservatives against the house longhorn beetle
1976 - IRG/WP 271
This abstract is given to let IRG members know about a method sometimes used in the Institute for Wood Technology in Sarajevo for obtaining rapid information on the toxicity of insecticides and ready made wood preservatives against the house longhorn beetle, which is the most common insect found attacking timber roof constructions in houses in Yugoslavia. In this method, 8-10 months' old ...
N Vidovic


Natural durability of Norwegian wood species for above ground applications – Project presentation and preliminary results
2006 - IRG/WP 06-10594
In Norway exterior wood structures have traditionally nearly exclusively been made of treated and untreated Norway spruce (Picea abies (L.) Karst) and Scots pine (Pinus sylvestris L.). In recent years there has been a tendency that other tree species, like various domestic hardwoods and imported species have been used in exterior above ground applications, often unfinished. For several wood speci...
P O Flæte, G Alfredsen, F G Evans


Losses of preservatives from treated wood during service. Results from a questionnaire
1994 - IRG/WP 94-50031
From environmental as well as from performance point of view it is of interest to know how much of the preservatives in treated wood that is leached out or evaporated from the wood during service. Many laboratory studies are carried out on leaching from small samples in distilled water or water with different pH. These studies give a good picture of the relative leaching from wood treated with dif...
M-L Edlund


Determination of chlorine-containing wood preservatives in art objects using Micro-XRF
2003 - IRG/WP 03-20266
The applicability of a mobile energy-dispersive micro X-ray fluorescence (μ-XRF) spectro-meter for the analysis of organochlorine-containing wood preservatives in art objects was tested. Information about the relative degree of contamination and the efficacy of detoxification measures with emulsive solvent systems can be gained using the intensity of the chlorine signals. μ-XRF t...
J Bartoll, A Unger, S Krug, K Püschner, H Bronk


Wood Preservation in the United Kingdom
1979 - IRG/WP 385
This is only the first of several reports in English currently being prepared about wood preservation in Europe. The report deals with the extent of industrial impregnation and the number of impregnation plants in use today in Great Britain. Timbers which are treated for various end uses and their life expectancies are discussed. The market for wood preservatives, the size of the motorway fencing ...
R Cockcroft


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Comparison between two laboratory test methods for determining the effectiveness on wood preservatives against blue stain in fresh wood
1987 - IRG/WP 2289
Most of the work done on determination of the effectiveness of new formulae for treating fresh wood against blue stain have been focussed on their use in the manufacture of saw timber. This work explains two laboratory methods, one which simulates the working and climatological conditions of factories making packages for fruit and vegetables in the Spanish Levante, showing that contamination of wo...
A M Navarrete, M T De Troya


Emissions from the combustion of wood treated with organic and inorganic preservatives
1994 - IRG/WP 94-50019
Wood waste and industrial wood residues often contain various preservatives. The waste management for these residuals can be recycling, deposition or combustion. Among the three possibilities, combustion seems to be the most efficient way of usage. To obtain more information about the emission properties of treated wood, different materials were incinerated in different furnaces after mixing with ...
T Salthammer, H Klipp, R-D Peek, R Marutzky


Laboratory evaluation of copper naphthenate pressure treatments against the Formosan subterranean termite
1993 - IRG/WP 93-10005
Southern pine wafers and Douglas-fir cubes pressure treated with copper naphthenate in AWPA P9 Type A oil or in toluene were evaluated for resistance to attack by the Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae). Wood samples were pressure treated to target copper retentions of 0.040, 0.075, 0.095, or 0.150 pcf, conditioned to simulate field exposure, a...
J K Grace, R T Yamamoto, P E Laks


The registration of wood preservatives in Canada
1977 - IRG/WP 394
The Pest Control Products Act in Canada is a part of Federal Agricultural legislation affecting chemicals for wood protection. Other parts of Federal legislation include Canadian Fisheries Act, Fed. Food and Drug act, Environmental Contaminants Act, Clear Air Act, Navigable Waters Protection Act and the Criminal Code Section 165. Some of the main excerpts from the Pest Control Products Act are as ...
J Rak, J K Shields


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 6: The length of the primary precipitation period
1975 - IRG/WP 359
The end of the primary precipitation fixation period of CCA preservatives coincides with the first peak in pH versus time. This offers a simple way of estimating the duration of the period. The duration is determined by a number of factors and their interactions, the most important of which are: wood species (anatomy, natural pH, accessibility of reducing agents), preservative type, preservative c...
S-E Dahlgren


Leaching amount of wood preservatives from treated wood in different size during outdoor exposure for 6 months
2000 - IRG/WP 00-50160
Eighteen impregnated specimens with CCA, ACQ, and BAAC preservatives were subjected to a outdoor leaching test. Test specimens, 10 x 10 x 25 cm3, 5 x 10 x 25 cm3, 2 x 10 x 25 cm3 in size, were cut from Japanese cedar (Cryptomeria japonica). Both of end surfaces were sealed with a silicone sealer in the half number of specimens. Total leaching amounts of copper from the open-end ACQ specimens of 10...
K Yamamoto, S Motegi, A Inai


The role of contact chemoreception in location of wood by the marine borer Limnoria (Isopoda)
1996 - IRG/WP 96-10157
This paper investigates the ability of Limnoria (Isopoda: Limnoriidae) to determine chemical differences in wood substrates, while in contact with the substrates. Test substrates were chosen on the basis of previous arguments concerning the chemical state of wood prior to Limnoria attack: microbial, ergosterol, metabolite, humic, extract and control (autoclaved) veneers were used as experimental s...
S M Henderson, S M Cragg


Test methods for wood preservatives against Lyctus: (1) Testing of treated veneer. (2) Testing of glue-line treated plywood. (Laboratory methods)
1977 - IRG/WP 293
Powder-post beetles destroy large quantities of veneer and plywood. Two test procedures are described which can be used to support application-oriented research into veneer and plywood preservatives. These procedures simulate practical conditions on a laboratory scale. Their characteristic feature is that wood species of special susceptibility are used for the tests; the susceptibility of the spec...
S Cymorek


Water-borne DNBP wood preservatives - Preparation and performance
1987 - IRG/WP 3407
Three waterborne wide-spectrum ground-contact DNBP (2-sec-butyl-4,6-dinitrophenol) wood preservative formulations and their performance are presented. Two are double-treatment formulations in which insolubilization and precipitation of the preservative is attained by salt formation or by formation of a water insoluble Cu/NH3/DNBP complex of formula [DNBP]2 [Cu(NH3)2]2 the clarified structure of wh...
W E Conradie, A Pizzi


Incidence of soft rot in creosoted poles
1992 - IRG/WP 92-1554
A further population of creosote-treated poles has been assessed for the occurrence of soft rot, as a continuation of work reported in IRG Document No. IRG/WP/1368. The outer 1 cm of each core was assessed microscopically and graded for the presence of soft rot cavities in the wood cell walls; with further assessments taken at a consecutive 1cm interval for cores showing positive findings. Followi...
D J Dickinson, P W McCormack, B Calver


The fate of salt preservatives in facility yard soils and decontamination of soils and drainage waters
1993 - IRG/WP 93-50001-25
Extensive studies during the past 10 to 15 years revealed that noticeable amounts of preservative components may be released in the environment by dripping off or by rain prior to fixation unless adequate precautions are taken. Therefore, soil and groundwater contamination especially from chromium-VI compounds but also from other inorganic and organic constituents exist in impregnation plants, pos...
R-D Peek, H Klipp, K Brandt


Previous Page | Next Page