IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 624 documents. Displaying 25 entries per page.


The resistance of high performance acetylated wood to attack by wood-destroying fungi and termites
2013 - IRG/WP 13-40621
The resistance of high acetyl solid timber (Accoya) and medium density fibreboard (Tricoya) to attack by wood-destroying fungi and termites was investigated under both laboratory and field conditions. Laboratory studies were conducted in Japan, New Zealand and USA. Field studies were conducted in Australia, Japan, New Zealand, Thailand and UK. The results of the laboratory and field studies agains...
J Alexander, J Hague, M Roberts, Y Imamura, F Bongers, E Suttie


Decay resistance of thermally modified Scots pine after 6 years’ exposure above ground
2013 - IRG/WP 13-40624
In the present study the performance of boards treated by ThermoWood process were studied above ground and the results given are based on a “modified” horizontal double- layer test. The base layer of boards was in direct contact with ground and the conditions were much harder than in the standard method. After six years’ exposure clear differences were found between untreated Scots pine and ...
H Viitanen, S Metsä-Kortelainen, A Nurmi, S Jämsä


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Performance of Coatings on Wood Treated with Carbon-Based Preservatives
2013 - IRG/WP 13-40638
Wood treated with carbon-based preservatives is often used in applications where coatings are required, yet few studies have examined the effect of such treatment on coating performance. Users need to be confident that coatings on carbon-based preservative-treated wood will perform as well as or better than those on untreated wood. The present study examines the performance of three coatings on un...
R Stirling, P I Morris


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
While not a new preservative system, Ammoniacal Copper Zinc Arsenate (ACZA), had not previously been used to protect crossties. Its performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercia...
T Carey


Copper naphthenate treatment for wood crossties and timbers
2014 - IRG/WP 14-30647
Copper naphthenate (CuN) has a long history in wood preservation and is recently finding increased usage as a treatment for wooden crossties and timbers. One of the principal reasons that CuN has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity and environmental impact. CuN is a well proven non-restricted use pres...
J Brient


Borate Redistribution in Glulam in an Above Ground Field Test
2014 - IRG/WP 14-30652
Researchers have refocused on the use of boratesin the wood protection industry in the last two decades due to their broad spectrum effectiveness against fungi and insects, and favourable environmental characteristics. This study was designed to determine borate distribution in a limited number of samples from a large field test of composites protected by a combination of coating and borate treatm...
P I Morris, A Temiz, J Ingram


Performance of some wood modification treatments against marine borers
2014 - IRG/WP 14-40668
Since some years, new treatment technology to protect wood against wood destroying fungi is introduced. Limited knowledge on their resistance to water organisms is available. Therefore, the resistance of chemically modified wood was assessed in a field test according to the European Standard EN 275 over a period of 3 resp. 5 years at sites in the North Sea and the Baltic Sea. Scots pine (Pinus syl...
A Klüppel, C Mai, H Militz, S Cragg


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Interpretation of moisture monitoring data - Relevance of moisture content thresholds for fungal decay
2015 - IRG/WP 15-10839
It is widely accepted that besides temperature wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. Many approaches to predict the service life of wooden structures have therefore been based on using wood MC as one major input-variable to develop dose-response relationships between material climate and decay response. However, to impr...
L Meyer, C Brischke


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


The combined effect of wetting ability and durability on field performance – verification of a new prediction approach
2015 - IRG/WP 15-20565
Comprehensive approaches to predict performance of wood products are requested by international standards and the first attempts have been made in the frame of European research projects. However, there is still an immanent need for a methodology to implement the durability and moisture performance of wood in a performance classification system. The aim of this study was therefore to establish an ...
C Brischke, G Alfredsen, P-O Flæte, M Humar, T Isaksson, L Meyer


Introduction of the COST FP 1303 Cooperative Performance Test
2015 - IRG/WP 15-20567
COST Action FP 1303 “Performance of bio-based building materials” successfully started in October 2013 and an ambitious program was set up for the four year programme. COST Actions provide an excellent opportunity for collaborative research, e.g. in the frame of Round Robin tests. The idea of this respective test was to distribute a fairly simple test set up to as many places in Europe as poss...
M Humar, C Brischke, L Meyer, B Lesar, N Thaler, D Jones, S Bardage, C Belloncle, J Van den Bulcke, J M Abascal, G Alfredsen, D Baisch, B Brunnhuber, G Cofta, E Grodås, E Frühwald Hansson, M Irle, H Kallakas, J Kers, M Klamer, P Larsson Brelid, A B Maider, K C Mahnert, E Melcher, R Möller, M Noël, L Nunes, G A Ormondroyd, S Palanti, N Pfabigan, A Pilgård, A O Rapp, P Schumacher, E Suttie, T Teppand, M Touza, J Van Acker


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Previous Page | Next Page