The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski
Remedial treatments of glulam = diffusion of active ingredients through glue lines from solid wood diffusable preservatives
1996 - IRG/WP 96-30117
Diffusable preservatives are very suitable for use in remedial treatments of laminated beams in which too high moisture content involves the development of wood destroying fungi. The diffusion of active ingredients (boric acid, disodium octoborate, bifluoride) is well observed in solid wood but in a composite wood, the glue lines may appear not only as a barrier for the diffusion but also, may be ...
D Dirol, S Mouras
The effect of glycol additives on diffusion of boron through Douglas-fir
2000 - IRG/WP 00-30235
Boron is highly effective against a variety of fungi and insects and is able to diffuse with moisture through wood. Diffusion decreases sharply at lower moisture contents, a characteristic that limits the potential use of this material as a remedial treatment for arresting internal decay. One approach to improvi ng boron diffusion is the simultaneous addition of glycol, which is presumed to enhanc...
C M Freitag, R Rhatigan, J J Morrell
A study of poplar LVL durability improvement:
1999 - IRG/WP 99-40148
The aim of this study was to optimise the durability of LVL panels by adding boron during the gluing process. Poplar veneers (2,6 mm thickness ) were selected by ISORY a French company . Two types of glue were tested : Phenol resorcine and Melamine Urea Formaldehyde. Each of them was mixed with various concentrations of borax (for the first one) and Boric acid(for the second one). Mechanical prope...
B Charrier, V Bridaux, N Fauroux, F Charrier
A field trial of water repellents as anti-sapstain treatment additives
1987 - IRG/WP 3417
The assessment of water repellents as anti-sapstain treatment additives has been included in a recent FRI research programme investigating improved surface protection of New Zealand Pinus radiata. Laboratory work has shown variation in water repellent effectiveness with chemical type and subsequently a field trial was established to examine the performance of selected water repellent/anti-sapstain...
J A Drysdale, D V Plackett
Further progress towards a cleaner creosote treatment - Summarised report
1984 - IRG/WP 3304
This document provides an up-dated progress report on our development of pigment emulsified creosote (PEC) used as a cleaner alternative to conventional high temperature creosote. A range of commodities (both hardwood and softwood) has now been satisfactorily treated in pilot plant and full scale commercial operations. Both brown (PEC 30B) and white (PEC 30W) formulations have been used. In additi...
H Greaves, C-W Chin, J B Watkins
Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora
Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora
Evaluation of the biocide diffusion from treated wood in indoor air. Bibliographic study
1990 - IRG/WP 3584
Within the frame of the risk assessment of the wood preservation products for the Health, the treated wood risk particularly when it is installed in dwellings becomes most important. The European directive "Building materials" (89/106/CEE) mentions the basic requirements with the buildings must comply. Annexe l states in particular that "the building must be conceived and built in order not to bec...
A Pichard
The efficacy of preservatives into the glue-line of plywood
1993 - IRG/WP 93-30002
This research is anti-termite/decay preservatives mixed with resin to produce the plywood. Thereafter, anti-decay/termite plywood were produced by the ordinary methods. To produce suitable plywood in the utilization and certified performance, the preservatives should be 0.3 to 0.4 kg/m³ of Chlorpyrifos; 0.88 and 1.10 kg/m³ of mix preservatives of Chlorpyrifos + IF-1000. Laboratories decay test (...
S Fushiki, T Saito, Y Katuzawa, Y Imamura, S Yusuf, B Subiyanto
Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens
Glue laminated poles - Progress report after 12 years' testing
1992 - IRG/WP 92-3685
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and under a power line just south of the Arctic circle in order to study their resistance against biological degradation. The tests have shown that the comparatively best performance will be obtained if each laminate is first treated wi...
J Jermer, Ö Bergman
Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden
Influence of water-borne preservatives on water repellency and the impact of addition of water repellent additives
1992 - IRG/WP 92-3704
The primary goal of a desirable wood preservative system is to effectively control decay fungi and other biodeteriogens in service. The water repellent nature of a given system may play an important role in the protection of wood. In this study, the water repellency of several water-borne preservative systems has been evaluated by measurements of tangential swelling during immersion. The systems i...
L Jin, D M Roberts, A F Preston
Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum
A simple field apparatus for measuring relative gaff penetration and assessing the effect of additives for improving pole climbability
2000 - IRG/WP 00-20187
A simple apparatus for measuring and comparing the relative "hardness" of utility poles is described. This "slide-hammer" gaff penetration apparatus was designed as a field testing unit to measure the depth of gaff penetration into test poles after application of a uniform and reproducible force to the gaff. The apparatus is simple to use in both the laboratory and field. Data is provided for resu...
A R Zahora
Stability of bifenthrin in a commercial phenol-formaldehyde plywood glue
2003 - IRG/WP 03-30311
Liquid phenol formaldehyde (PF) glue mixes used for plywood manufacture are strongly alkaline. At this pH insecticidal additives may not be stable for long periods. In order to establish practical working life of the synthetic pyrethroid insecticide, bifenthrin, in liquid PF glues the concentration of bifenthrin in the glue mix was measured under laboratory conditions over a 24 hour period. Glu...
M J Kennedy, P A Collins, R D Vella
Bifenthrin recovery from glue-line-treated plywood
2007 - IRG/WP 07-20355
Plywood and laminated veneer lumber (LVL) can be protected from termite damage by addition of bifenthrin to the adhesive used in product manufacture. However, conditions associated with this manufacturing process may lead to deterioration or immobilisation of the active ingredient. In order to determine compliance with treatment specifications, it is important that the concentration of a preservat...
J Norton, L Stephens
The effect of additives on copper losses from alkaline copper treated wood
2007 - IRG/WP 07-50246
The replacement of chromated copper arsenate (CCA) by alkaline copper compounds has heightened awareness of the potential impact of copper losses on aquatic organisms. While there remains a healthy debate concerning the actual risk of copper leaching from wood preservatives into aquatic ecosystems, it is clear that reducing these losses will be necessary to avoid continued regulatory actions aga...
J Mitsuhashi, J J Morrell, L Jin, A F Preston
Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston
Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin
Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung
Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter
Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska
Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston