IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 531 documents. Displaying 25 entries per page.


Termite legislation in France: Termite control measures and prevention rules in building construction
2010 - IRG/WP 10-20448
Reticulitermes subterranean termites are considered as urban pests in France because they are harmful for wood-based in the South and the southwestern quarter of the country. Since November 2006 new protective measures of building construction have been introduced by the French parliament which must be applied across the country and in overseas territories to prevent termite infestations. All new ...
M Kutnik, M Jequel, I Paulmier, D Ansard


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Laboratory evaluation of borate amine: Copper derivatives in wood for fungal decay
2010 - IRG/WP 10-30543
The aims of this study were to evaluate borate: amine: copper derivatives in wood for fungal decay protection as well as the permanence of copper and boron in wood. Wood treated with each of four derivatives of borate:amine:copper prevented fungal decay. Disodium tetraborate ecahydrate (Borax):amine:copper derivatives with retentions of 0.61 to 0.63% after water leaching prevented decay by Gloeo...
G Chen


Preventing decay in termite monitoring stations
2010 - IRG/WP 10-30546
In-ground monitoring stations and termite baits are widely used in the southern United States with the intent of detecting and eradicating subterranean termite activity near buildings. These stations comprise a wood (or other cellulose material) substrate (monitor) and perhaps a termiticidal toxicant (bait) held in a plastic cage that allows for both easy examination and access by termites. The us...
A M Taylor, Jae-Woo Kim, S Duarte, L Nunes, J D Lloyd


Fungal decay resistance and mechanical properties of plywood panels made from maritime pine (Pinus pinaster) and bonded with cornstarch-quebracho tannin-phenol formaldehyde adhesive
2010 - IRG/WP 10-40490
The aim of this work is to demonstrate the performances of cornstarch-quebracho tannin-based resins designed as adhesive in the plywood production. In this way, the cornstarch and quebracho tannin was introduced in the classic adhesive formulation in order to supply a part of phenol-formaldehyde (PF). In order to evaluate the mechanical performances of optimal cornstarch-quebracho tannin-PF, plywo...
F Charrier, A Moubarik, A Allal, A Pizzi, B Charrier


TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Fungal biodegradation of CCA-treated wood wastes
2011 - IRG/WP 10-50276
Fungal biodegradation could be employed as a pretreatment method to alleviate problems caused by landfill disposal of CCA-treated wood wastes (e.g. a shortage of landfill space and a release of leacheate). It could be used to decrease the volume of waste and to remove metals from waste simultaneously. We have screened hundreds of decay fungi, including fungi isolated from CCA-treated wood in servi...
Gyu-Hyeok Kim, Yong-Seok Choi, Jae-Jin Kim


Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter


Measuring fungal cellulolytic enzyme activity in degrading wood
2011 - IRG/WP 11-10753
An enzyme assay which measures enzyme activity directly from wood will assist in the fundamental understanding of the enzyme components of the decay mechanism of rot fungi and any changes in the presence of wood protectants. At present, to measure fungal carbohydrate degrading enzyme activity in the presence of wood, two methods are used: either 1) the enzyme is measured in the growth media contai...
S M Duncan, J S Schilling


Molecular investigation of Postia placenta growing in modified wood
2011 - IRG/WP 11-10756
Brown rot is the most common and destructive type of fungal decay for wood in service. These fungi depolymerize preferentially the structural carbohydrates, cellulose and hemicellulose in the cell wall leaving oxidized lignin behind. Modified wood can provide protection against a variety of wood deteriorating organisms, including decay fungi. However, there is still little known about the mode of ...
B Schmöllerl, G Alfredsen, C G Fossdal, M Westin, A Steitz


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


The influence of moisture content and wood pH variation on fungal melanin formation in wood substrates
2011 - IRG/WP 11-10759
Wood decay patterns are strongly influenced by the conditions of the wood substrate, including moisture content and pH. In an antagonistic environment some fungi respond with pigment formation that helps to isolate and protect their mycelium. This is often associated with slower fungal growth and delay of wood mass loss. Dark colored melanin is the most common pigment formed by wood decay fungi, a...
D Tudor, S C Robinson, P A Cooper


Durability testing of coconut shell according to ENV 807
2011 - IRG/WP 11-10761
Coconut shell was tested in the laboratory according to the European standard ENV 807 with three different soil types: compost soil, brown rot/soft rot rich soil and white rot/soft rot rich soil. Mass losses between 14 and 16 % were achieved with all three soils, indicating that the decay type is of little importance in the degradation process. Somewhat higher mass losses, 19-22 % were obtained fo...
J Jermer, A H H Wong, K Segerholm, T Nilsson


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip, flood coat or spray, and rapidly penetrates to the centre of timber substrates, whether containing sapwood or heartwood. However, section ...
B M Ahmed (Shiday), J R J French


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Implementation of a Quality Assurance System for thermally modified timber (TMT) by the Association of Central European TMT-Producers
2011 - IRG/WP 11-40558
Due to increasing market shares of thermally modified timber (TMT) in Europe, a working group of ten central European TMT manufacturers (TMT-WG) was founded in 2010 to cover public relations and marketing activities. Since the present level of product testing and property declaration was not satisfying, a “task group TMT-quality” was put into action in 2010 to develop a comprehensive quality a...
C R Welzbacher, W Scheiding


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Decay factors in termite in-ground monitoring stations
2012 - IRG/WP 12-10775
Subterranean termites are serious pests of wood in service in much of the world. One of the most common techniques for monitoring and controlling termites is the use of in-ground monitoring stations which comprise a wood or other cellulosic material monitor (cellulosic matrix) and/or a termiticide bait held in a open plastic holder so facilitates examination and the termite access. Wood and other ...
S Duarte, A M Taylor, Jae-Woo Kim, J D Lloyd, M Duarte, L Nunes


Connecting fungal genomic variations to wood chemical composition: A way to understand the adaptation of wood decaying fungi
2012 - IRG/WP 12-10776
The development of new sequencing methods allows now exploring the detoxication systems of wood-decaying fungi. These systems, called xenome, are mainly composed of oxidative enzymes (phase I) and of conjugation enzymes (phase II). These enzymes belong to superfamilies, which are extended in the plant cell-wall interacting fungi. From different approaches coupling in particular comparative genomic...
E Gelhaye, Y Mathieu, E Meux, A Thuillier, M Mélanie


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Previous Page | Next Page