Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


Control de calidad eficiente de proteccion superficial sobre madera
2008 - IRG/WP 08-20397
Quality control is important to assure efficient protection of wood surfaces. When wood is exposed to the environment, it degrades due to weathering or environmental factors alone. Aging tests are utilized to test coating products. Quality control techniques are performed on exposed products according to standardized methods (NCh, ASTM, ISO, DIN, EN, FTMS, NTF, NBINT, or equivalents). Certified l...
A M Fernández S


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Isolation and identification of stain fungi and mould fungi on bamboo wood in China
2009 - IRG/WP 09-10703
One hundred and seventeen isolations were isolated from 150 specimens of mildewed or stained bamboo wood and bamboo products from 9 locations in north, south and central China. The molecular (ribosomal DNA Internal Transcribed Spacer, rDNA-ITS) and morphological identification results showed these fungi could be categorized 2 phyla, 2 classes, 4 subclasses, 10 orders, 15 families, 22 genera, 56 sp...
Xingxia Ma, Mingliang Jiang, Daochun Qin


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Utilidad práctica de mini estacas en ensayos de campo
2008 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Modelling hyphal growth of the bio-incising fungus Physisporinus vitreus
2010 - IRG/WP 10-10710
The white-rot fungus Physisporinus vitreus preferentially degrades the pit membranes of bordered pits in tracheids and subsequently enhances wood permeability. Thus, P. vitreus can be used to improve the uptake of wood preservatives and environmentally-benign wood modification substances. This process can be used to enhance the use and sustainability of native conifer wood species by the wood indu...
M Fuhr, C Stührk, F W M R Schwarze, M Schubert, H J Herrmann


A genomic sequencing approach to study wood decay and copper tolerance in the brown rot fungus, Antrodia radiculosa
2010 - IRG/WP 10-10720
We used Illumina paired-end short read sequencing (76 nt, 300 bp insert size) to produce a de novo assembly of the genome of Antrodia radiculosa, a copper-tolerant brown rot fungus that is capable of aggressive wood decay. Quality analysis of the base calls in the dataset (8.95 Gb) showed that the majority of the nucleotide sequence was of the highest quality with 5% in the lowest quality group. ...
J D Tang, T Sonstegard, S Burgess, S V Diehl


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Analyzing hyphal growth of the bio incising fungus Physisporinus vitreus with light-, confocal laser scanning- and, Synchrotron X-ray tomographic microscopy
2010 - IRG/WP 10-20438
Norway spruce wood is an important building material for the forest and wood industry. To improve wood permeability and uptake of wood modification substances Physisporinus vitreus is employed as a bioincising agent. In this study wood specimens were incubated with P. vitreus to assess hyphal colonisation and structural alterations of Norway spruce wood. After different incubation periods, semi-th...
C Stührk, M Fuhr, M Schubert, F W M R Schwarze


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski


Ten Year Field Tests of Borate-Treated Wood Against Subterranean Termites
2011 - IRG/WP 11-30557
In the mid 1990s, Forintek Canada Corp. initiated a study of the termite resistance of borate-treated lumber above ground, protected from rain in Canada, Japan and Hawaii. Predominant termite species at three test were Reticulitermes flavipes in Canada, and Coptotermes formosanus in both Japan and Hawaii. The material included hemlock and amabilis fir lumber treated with disodium octaborate tetrah...
P I Morris, J K Grace, K Tsunoda


Standardized Field Trials with Micronized Copper
2011 - IRG/WP 11-30564
In 2008, an extensive review of all available data from standardized tests of micronized copper systems was published and there has been considerable work since then. This paper discusses over 20 field stake trials underway in well-known sites such as Gainesville, FL, Hilo, HI and the Dorman and Saucier sites in MS as well as tests from Australia and New Zealand. In addition, 4 ground proximity ...
C R McIntyre, M H Freeman


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Previous Page | Next Page