The Impact of Cryopreservation Techniques and of Water Quality on the Wood Degrading Ability of Fungal Strains: Recommendations for Maintenance and Culturing Procedures
2018 - IRG/WP 18-20636
In order to establish an optimal cryopreservation method, strains of Basidiomycete and Ascomycete fungi, which are among the most frequently used for wood durability testing, were evaluated using three cryopreservation procedures at -80°C. The main objective was to prevent decrease of the fungal virulence that may occur due to repeated routine sub-culturing procedures and to optimize the reactiva...
A Stum, M Montibus, I le Bayon, M Kutnik


Liquefied wood polyols: a bio-based preservative for protection of wood from fungal decay
2018 - IRG/WP 18-30725
The liquefaction of wood is one of promising approaches in utilization of woody waste which is generated during primary and secondary processing of wood and liquefied wood having various application including bio-based preservatives. The biological degradation of wood due to fungi is the major problem encountered in indoor and outdoor utilization of wood. In this study, woody waste recovered from ...
A Kumar, G Vijaylakshmi, S Singh Chauhan


Non-stochiometric oxidation and ROS generation promoted by guaiacol lignin structures and lignocelluose surfaces may be a component of brown rot fungal degradation mechanisms
2019 - IRG/WP 19-10937
Model guaiacol compounds representing lignin monomers, as well as DHP-lignin and wood flour of controlled particle size were used to assess iron reduction at the pH of the natural wood cell wall. All compounds functioned as electron donors for ferric iron, with the lignin monomers demonstrating capacity for non-stochiometric reduction of iron with multiple moles of ferric ion reduced per mole of l...
Y Tamarua, M Yoshidaa, L D Eltisb, B Goodell


Identifying the fungal community on western redcedar (Thuja plicata) wood in field tests above and in ground contact exposure: preliminary results
2019 - IRG/WP 19-10939
Western redcedar (Thuja plicata) is a high value species in the Canadian forest industry due in large part to the natural durability of its heartwood. Western redcedar heartwood contains extractives that are inhibitory to the growth of many fungi responsible for decay. In order to gain insights into which extractives are important in long term durability, and which fungi are important to decay of ...
A Dale, S Kus, R Stirling


Natural durability of four Tunisian Eucalyptus wood species and their respective compositions in extractives
2019 - IRG/WP 19-10942
In the 50’s, Tunisia government introduced more than 11 Eucalyptus wood species. Eucalyptus species were planted in Tunisia in different arboreta throughout the country for close observation and adaptation to climate and soil. These fast-growing wood species were mainly used as fire wood, for the production of mine wood and to fight against the erosion. These tree species were adapted themselve...
S Ben Ayed, M T Elaieb, S Dumarçay, B De Freitas Homen De Faria, M-F Thévenon, P Gerardin, K Candelier


From fungal detoxification systems to wood durability in neotropical forests
2019 - IRG/WP 19-10946
White-rot fungi are able to mineralize all the wood components due in particular to an efficient detoxification system. We hypothesised that components of this detoxification systems, glutathione transferases, could be used as tools to explore the natural durability of neotropical wood species. Analysis of the interactions between six glutathione transferases of Trametes versicolor and extracts of...
T Perrot, G Salzet, N Amusant, J Duchene, E Gelhaye


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


Using X-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
2019 - IRG/WP 19-40854
Chemical modification of the hydroxyl groups of wood can improve the properties of wood by providing moisture and biological resistance, as well as dimensional stability. Southern pine solid wood was chemically modified to various weight percentage gains (WPG) with epoxybutene (EpB, 8%-38% WPG). After modification, specimens were extracted with a toluene: ethanol (2:1) solution for 2 hours or wate...
R E Ibach, N Plaza


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Study on the ability of wood-destroying fungi to grow through chemically modified wood
2019 - IRG/WP 19-40858
Over the last decades, chemical wood modification technologies were developed to increase the resistance against attack by wood-destroying organisms without using biocides. Most of those technologies are based on an impregnation step initially. In most treated wood products, mainly by using solid wood in thicker dimensions as in posts, poles, sleepers, deckings etc. it is known that wood impregnat...
L Emmerich, S Strohbusch, C Brischke, S Bollmus, H Militz


Potential Use of the Pigment from Scytalidium cuboideum and Chlorociboria aeruginosa as an UV-light Protection Additive in Oil Finishes
2019 - IRG/WP 19-40868
UV-light degradation of wood is one of the top reasons for consumer replacement of outdoor wooden structures. This type of degradation is seldom mechanical, and is instead often motivated by loss of aesthetics (graying). There are numerous commercial products available on the market that deal with this loss of color, many of which contain added pigments to ‘rejuvenate’ or ‘revitalize’ grey...
S M Vega Gutierrez, D W Stone, R He3, P T Vega Gutierrez, Z M Walsh, S C Robinson


Fungal damages in Norwegian massive timber elements – causes and measures
2019 - IRG/WP 19-40879
Massive wood elements are relatively new in Norway but the use is growing quickly, primarily the use of cross-laminated timber (CLT). Moisture performance of massive timber elements has been examined by some researchers, but more knowledge is needed. There is uncertainty regarding the need for vapour barriers or retarders in roof assemblies, and for practical reasons buildings are rarely assembled...
M S Austigard, J Mattsson


Effect of pretreatment of wood surfaces with a copper monoethanolamine solution on the natural weathering performance of semitransparent stains
2019 - IRG/WP 19-40881
Semitransparent stains for wood products are favored for outdoor applications in Japan because these finishes do not hide the wood grain. However, the photoprotective effects of wood surfaces are low, therefor there is a need to improve the weathering performance. We examined the natural weathering performance of semitransparent stains on wood pretreated with a copper monoethanolamine solution (Cu...
S Isaji, H Shibui, Y Hirabayashi


Pigment production by the spalting fungus Scytalidium ganodermophthorum and its industry potential
2020 - IRG/WP 20-10957
Scytalidium ganodermophthorum is best known as a pathogen of cultivated mushrooms, with infected cultures turning yellow in color. The fungus is also used in the art form known as ‘spalting’ to produce yellow, green, and purple colors in wood for decorative purposes. Wood colored by fungus in this manner has been traditionally used in the creation of fine art and woodworking since the 16th cen...
R C Van Court, P Vega Gutierrez, S C Robinson


Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson


Profiling fungal degradation of Scots pine sapwood by short wave infrared hyperspectral image analysis
2020 - IRG/WP 20-20667
Hyperspectral image analysis of Scots pine sapwood wood affected by decay fungi has been carried out as part of a Ph.D. thesis within the project Remote Inspection of Wooden Utility Poles (RIWUP). In a lab experiment, Petri-dishes with Scots pine sapwood samples on malt agar medium were infected with two types of decay fungi, a brown rot and a white rot. The wood samples were scanned with a HySpe...
A Jochemsen, G Alfredsen, I Burud


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Biological durability of sapling wood
2020 - IRG/WP 20-10967
Sapling-wood products from different wood species such as willow (Salix spp.) and Common hazel (Corylus avellana) are frequently used for gardening and outdoor decoration purposes. Remaining bark is suggested to provide additional biological durability. Even for temporary outdoor use it seemed questionable that durability of juvenile sapwood can provide acceptably long service lives of horticultur...
C Brischke, L Emmerich, D G B Nienaber, S Bollmus


Modelling decay rates of timber exposed above ground on four different continents
2020 - IRG/WP 20-20670
Durability performance data from an international decking trial were analysed to explore relationships with climate variables, particularly those related to temperature and rainfall. Matched decking samples of slash pine (Pinus elliottii) sapwood and heartwood, spotted gum (Corymbia citriodora), Norway spruce (Picea abies) and Scots pine sapwood (Pinus sylvestris) were exposed to the weather above...
L P Francis, J J Morrell, C Brischke, P B Van Niekerk, J Norton


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Fungal colonisations in and on industrially manufactured acetylated glulam in UC 3
2020 - IRG/WP 20-40900
This poster paper describes one of the first cases where industrially acetylated glulam was colonized by wood-destroying fungi after less than 10 years of exposure in use class 3.2. Remarkable is that fruiting bodies of white as well as brown rot fungi were found on one and the same bench element. The first visible wood destroying fungi was the white rot fungus Schizophyllum commune followed by th...
J Müller, E Melcher, T Potsch


NewSiest-Enhancement of UV stability of thermally modified wood through envelope impregnation with nanobased stabilisers
2020 - IRG/WP 20-40909
Thermal modification is a process which improves the properties of wood, resulting in a material that can be disposed at the end of the product life cycle without presenting an environmental hazard. Thermally modified wood retains as a natural product and the grain, original colour variances and characteristics of wood are still present. However, exposure to daylight causes brightening or greying ...
K Srinivasa, M Petrič


Assessing the risk of marine borer attack of the timber trestles and decay of timber above the intertidal zone of the Barmouth Viaduct
2021 - IRG/WP 21-10974
The Barmouth Viaduct is a Grade II* listed structure which carries the single track of the Dovey Junction to Pwllheli line and footway over the Mawddach estuary. It is in a marine environment where timber below the high tide mark is at most risk in Use Class 5 and all timber above in Use Class 3.2, permanently exposed to the risk of wetting. The structure consists of a timber trestle viaduct of ...
J R Williams


Evaluation of decay and energy properties from thermally modified biomasses during fungal deterioration by NIR-spectrometry
2021 - IRG/WP 21-40922
This study is focused on the prediction of fungal weight loss (WL) and high heating value (HHV) from raw and torrefied waste lignocellulosic feedstocks, according to their exposure duration to wood-destroying fungi, using near infrared spectroscopy (NIR) and chemometrics models. Sugarcane bagasse, coffee husk, eucalyptus and pine shavings were torrefied at 290 °C in a screw reactor, during 5, 7...
B de Freitas Homem de Faria, P Santana Barbosa, J Valente Roque, A de Cassia Oliveira Carneiro, P Rousset, K Candelier, R F Teofilo