Time-lapse evaluation of Aureobasidium pullulans growth on selected lignin derivatives and chitosan
2024 - IRG/WP 24-11032
Wood, often referred to as the “building material of the 21st century”, has gained recognition as an attractive alternative to several traditional building solutions. To enlarge the application of wood, several properties including biotic and abiotic degradation resistance need to be improved. Consequently, new solutions are available on the market that ensure expected properties and functiona...
Gubensek, F Poohphajai, A Tosic, K Butina Ogorelek, W Pajerski, A Cernosa, V Hribljan, A Sandak


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell


Cellulose nanomaterials in growth media for wood decay fungi
2024 - IRG/WP 24-11035
Cellulose nanofibrils (CNFs) were investigated as a partial substitution for agar in growth media for wood decay fungi. Radial growth measurements of eight basidiomycete fungi were taken on solid growth media with and without CNFs. Additionally, fungal strain virulence was evaluated using the European CSN Standard EN 113-2 wood decay durability test. The inclusion of CNFs did not significantly aff...
K M Ohno, R A Arango, R Sabo, C M Clemons, G T Kirker, A B Bishell


On the use of miniaturized wood specimens in fungal decay experiments – mini-blocks versus EN 113 test specimens
2024 - IRG/WP 24-11044
Preliminary evaluation and classification of wood durability against decay fungi using laboratory monoculture experiments has been a longstanding practice because these tests offer quicker results than field tests. Various methods, including miniaturized specimen formats and different incubation periods, have been explored to expedite decay processes and assess wood preservation efficacy. The 'min...
C Brischke, G Alfredsen


Investigating moisture dynamics and fungal decay risk: integrating X-ray CT visualization and simulation benchmarks through a Fungal Control Unit
2024 - IRG/WP 24-11045
Wood is susceptible to fungal attack and over time the structural integrity can be compromised. This risk is of course strongly related to moisture dynamics, as moisture is needed for fungal growth. While existing methodologies, such as lab and field tests, provide valuable insights into wood decay, they often fall short in replicating real-life conditions, particularly within the intricacies of t...
J Van den Bulcke, J Van Acker, M Delbeke, A Blommaert, N Van Den Bossche, M Steeman, L De Ligne


Suberinic acid from birch bark and its suitability in wood protection
2024 - IRG/WP 24-20708
This study investigated the effect of different concentrations of suberinic acid (SA) on the growth of two fungi species. Initial radial growth tests showed a slightly slower growth rate for brown rot, whereas white rot exhibited faster growth than the untreated reference. In contrast, a commercial wood preservative significantly reduced the radial growth of both fungi species. Evidence of cell wa...
A Treu, M Altgen, J Rizikovs


Studies on the treatability of selected pine species and corresponding efficacies of a new non-biocidal treatment
2024 - IRG/WP 24-20721
Wood decay caused by fungi may reduce the service life of wood in outdoor applications. Since moisture conditions in wood occur as one of the most crucial parameters for fungal decay, chemical modifications, which affect the latter, may increase the resistance of wood against such organisms. Usually, pine sapwood is easier to chemically treat than heartwood, as the former generally shows good perm...
T R da Silva Lins, L Emmerich, H Militz, P H Gonzales de Cademartoni, R J Klizke, M Pereira da Rocha


The potential of Wacapou (Vouacapoua americana) extracts to develop new biobased protective solutions for white woods
2024 - IRG/WP 24-20724
The valorisation of Amazonian wood residues into active chemical compounds could be an eco-friendly, cost effective and valuable way to develop wood preservatives formulations in order to enhance the decay and termite resistances of low durable wood species, by impregnation processes. Wacapou (Vouacapoua spp., Fabaceae) is a well-known Guianese wood species for its use in local wood construction ...
E Kieny, K Candelier, L Milhe, Y Estevez, C Sophie, R Lehnebach, J Damay, D Florez, E Hoël, M-F Thevenon, J Bossu


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


Bio-durability and weathering performances of cardanol-treated wood
2024 - IRG/WP 24-30809
Cardanol is an excellent insecticide, fungicide, and termiticide derived from thermally treated cashew nutshell liquid (CNSL) and has been extensively explored in the chemical industry and for medicinal uses. However, its potential for wood protection remains unexplored. This study aims to understand the bio-durability and weathering properties of cardanol-treated wood. The southern pine and yello...
L Liang, McDonald, A G, L Cai


Shelling of flat and profiled western larch deck-boards exposed to natural weathering
2024 - IRG/WP 24-40997
Shelling is a severe type of raised grain that occurs at the surface of deck-boards made from wood species that have growth rings with pronounced differences in density between earlywood and latewood, for example southern pine (Pinus spp.). Shelling is more severe in deck-boards fixed with their growth rings oriented pith-side-up (concave) rather than bark-side-up (convex). Far less is known about...
L H Leung, P D Evans


How personality traits influence the perception of fungal decay in a wooden cladding – A survey in three Modelling wood moisture content in outdoor conditions from measured data
2024 - IRG/WP 24-41002
This study examined perceptions of fungal decay damage on wooden cladding across Norway, Sweden, and Germany. The majority of respondents across all countries did not find the fungal decay damage in question acceptable, with the least acceptance in Norway. This could be due to Norway having the highest frequency of wooden residential buildings and the most experience with maintaining wooden claddi...
G W Gustavsen, G Alfredsen, P B van Niekerk, J Niklewski, C Brischke