Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Biological performance of wood- and bamboo-polypropylene composites: Effects of particle content, particle size and Zn borate
2012 - IRG/WP 12-40577
Particle content and size of wood material in wood plastic composites (WPCs) can affect efficacy of WPCs against fungi and termites. This study evaluated fungal and termite resistance of WPCs manufactured by using two different levels of particle content (50 and 70%) and three different particle sizes (30, 60, and 100 mesh). In fungal resistance tests, Tyromyces palustris, a standardized test fung...
S N Kartal, S Aysal, E Terzi, T Yoshimura, K Tsunoda


Biodegration of treated wood waste by native fungal communities of tropical soil in French Guiana
2012 - IRG/WP 12-50285
Woods have been protected with fungicides for a long time, and the effects of these fungicides on soil after being leached into the ground have turned out to be a true environmental issue. It is in this perspective that we are proposing to study fungal communities of these contaminated woods in a purpose of bioremediation. Most of precedent studies have focused on ability of some Basidiomycetes an...
A Zaremski, L Gastonguay, C Zaremski, F Chaffannel, J Beauchêne, G LeFloch


Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


Use of Acoustic Emission (AE) to detect activity of common European dry-woodboring insects: some practical considerations
2013 - IRG/WP 13-10803
Old house borer (Hylotrupes bajulus), Furniture beetle (Anobium punctatum), and Deathwatch beetle (Xestobium rufovillosum) are common dry-woodboring insects occurring throughout Europe. With the aim to prevent unnecessary use of biocidal products, to protect valuable wooden elements and objects from unwanted influences, and to have a more objective method, SHR has started to study the use of acous...
J G M Creemers


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


What molecular biology can tell us about the biodegradation of lignocellulose: the utilization of molecular techniques for the detection, identification and enhanced understanding of wood degrading organisms
2013 - IRG/WP 13-20528
Molecular techniques are now routinely used in the identification, detection and analysis of wood degrading organisms. An overview of some of the early work on nucleic acid isolation and characterization will be followed by a discussion of the power of sequencing and other procedures for better understanding: the mechanisms involved in the biological degradation of wood, the metabolic basis of pre...
J Jellison, B Goodell, G Alfredsen, D Eastwood, G Daniel, S M Cragg, J K Grace


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Fungal laccases as a tool for wood functionalization
2013 - IRG/WP 13-20533
Wood degrading fungi are the most important production organisms for laccase, a promising oxidative biocatalyst with numerous biotechnological applications in the forest products industry. Laccases are multi-copper containing oxidases (EC 1.10.3.2), which catalyse mono-electronic oxidation of phenols, polyphenols and anilines at the expense of molecular oxygen. Interest in these essentially ‘eco...
M Schubert


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
2013 - IRG/WP 13-40648
Evaluating the fungal durability of wood-plastic composites (WPCs) is complicated by the influence of slow moisture sorption. Recently, the American Wood Protection Association (AWPA) Standard Method E10, Testing Wood Preservatives by Laboratory Soil-Block Cultures, was modified to incorporate not only solid wood, but also wood-based composites and WPCs. To simulate long term WPC performance, cond...
B K Segerholm, R E Ibach


Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack). In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar