Marine performance of preservative treated Southern pine panels. Part 2: Exposure at Mourilyan Harbour, Queensland, Australia
2000 - IRG/WP 00-10337
Southern yellow pine panels treated with ACQ type B, ACQ type A, CCA type C, creosote, and copper naphthenate have been exposed at Mourilyan Harbour, north Queensland, Australia for almost 6 years. These panels have been inspected and rated for fouling and attack by Teredinid, Limnoria, Martesia, and Sphaeroma during this exposure. After 70 months exposure, overall performance of ACQ type B was eq...
A R Zahora, A F Preston, K J Archer, S Kleinschmidt


Investigation of some technical properties of heat-treated wood
2003 - IRG/WP 03-40266
The objective of this study was to investigate some technical properties of heat-treated wood. Wood heat-treated according to a process intended for wood in above-ground end-uses (European hazard class 3) was subject to the following: · A delamination test according to EN 391 with glulam beams made of heat-treated pine (Pinus sylvestris) and spruce (Picea abies) laminations, assembled with PR...
C Bengtsson, J Jermer, A Clang, B Ek-Olausson


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


Dimensional stability, biological resistance, and mechanical properties of phenol-resin-treated particleboard
1990 - IRG/WP 3622
Particleboards were treated with a low molecular-weight phenol-formaldehyde (PF) resin and their enhanced properties were evaluated. Besides dipping of particles in aqeous solutions of resin, and spraying of resin solutions before spray of the conventional phenol-formaldehyde resin for adhesive binder, one step treatment by spraying of the mixture of the low molecular-weight resin and the adhesive...
Y Imamura, H Kajita


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura


Testing a diffusion and reaction model for the leaching of CCA components from unfixed CCA-treated wood
2002 - IRG/WP 02-50193
A previously described physical model applicable to the leaching of any substance undergoing a first-order fixation reaction with wood is applied to the leaching of CCA components from unfixed wood. Using this model and laboratory leaching experiments with small wood samples immersed in water, the diffusion coefficients and reaction rate constant of Cr6+, total Cr, Cu and As in unfixed CCA-treated...
L Waldron, P A Cooper


Highly virulent wood-rotting Basidiomycetes in cooling tower timbers
1995 - IRG/WP 95-10125
Over the past ten years most industrial cooling towers changed their water treatment systems in order to meet environmental requirements. Since this alterations wood rot attack has been reported more frequently. Several Basidiomycete fungi were isolated and determined. Amongst the most important ones are strains of Physisporinus vitreus (Pers.:Fr.) P. Karst., Phellinus contiguus (Fr.) Pat. and Don...
J Van Acker, M Stevens, V Rijckaert


Wood preservation in Thailand
1983 - IRG/WP 3265
The report gives a background to Thailand and its timber resources, production and consumption. The history of wood preservation in the country and its modern industrial development are described. Its 19 preservation plants are listed and the production figures of the two major ones given. The wood preservatives in use are noted and the costs of treating a railway sleeper in three different ways c...
A Rananand, R Cockcroft


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 20: Report on the inspection of specimens at Sekondi, Ghana after 48 months
1985 - IRG/WP 4116
The results of the second inspection of CCA- and CCB-treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. The panels of Pinus sylvestris treated with 3% CCA are stil unattacked after 48 months. Panels treated with 10% CCA and still in test (Fagus sylvatica, Pinus sylvestris and Alstonia scholaris) are still free of attack. Locol species treated with 3% CCB have all been dest...
F F K Ampong, N Asare-Nyadu


Preservative performance of copper naphthenate (SANPRESER-OGR) in brush treatment of timber
1991 - IRG/WP 3663
Preservative efficacy of copper naphthenate (SANPRESER-OGR) was evaluated in the laboartory and field trials when timber was treated by brushing. Results of field trial indicated that service life of the brush-treated timber could be approximately 10 years or longer under ground contact conditions, although life span was slightly varied with timber species and test sites. After four years&apos...
Y Sugai, K Hamada, M Kitada, K Tomoi


Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer


Bending properties of treated western hemlock plywood
1996 - IRG/WP 96-40064
This study investigated the mechanical properties of western hemlock plywood after treatment with waterborne preservatives and redrying. Unlike previously reported results for southern pine plywood, western hemlock plywood was more sensitive to redrying temperature than to preservative treatment. Generally, western hemlock plywood was affected by temperature and other variables. Losses in mechanic...
H M Barnes, A Khouadja, D E Lyon


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


Isolation and identification of bacteria from CCA-treated eucalypt power transmission poles
1987 - IRG/WP 1317
Bacteria have been isolated from CCA treated Eucalyptus maculata poles which possessed characteristic bacterial decay patterns. Cultures were isolated on a number of different media which had been inoculated with a splinter of degraded wood. Primary tests indicated that most isolates belonged to the genera Pseudomonas and Bacillus. The species Pseudomonas cepacia was most frequently isolated....
G A Willoughby, A C Hayward, L E Leightley


Volumes and weights of different CCA-C treated wood poles, anchor logs and crossarms of REB at air dry condition
1996 - IRG/WP 96-40073
Researches revealed the unit volumes and weights at air-dry condition (12% MC) of different poles, anchor logs and crossarms species of REB from this world. The softwood products are lighter than hardwood products. Inversely the unit volumes of softwood poles are higher than those of hardwood poles. Red pine (Pinus resinosa), radiata pine (Pinus radiata), blue pine (Pinus wallichiana), fir (Abies ...
A K Lahiry


Leaching of CCA components from treated wood under acidic conditions
1993 - IRG/WP 93-50004
The leaching of CCA components from treated wood under acidic conditions were investigated. Western hemlock treated with three types of CCA and two levels of target retention was subjected to leaching at four different levels of pH. After leaching tests, leached samples were subjected to laboratory decay and soft rot tests. The amount of CCA components leached was dependent on acidity of leaching ...
Jae-Jin Kim, Gyu-Hyeok Kim


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Incursion of Hylotrupes bajulus Linnaeus (European House Borer) into Western Australia
2005 - IRG/WP 05-10558
In January 2004, an adult Hylotrupes bajulus Linnaeus was detected emerging from a beam of Pinus pinaster in a house in Perth, Western Australia. The timber had been locally grown and milled. Surveys to define the extent of the infestation show it is restricted to dead pine trees in 28 sites around Perth. The biological and economic feasibility of eradication is being assessed. Since about 2001, k...
M Grimm


The hydrolysis of organo-boron compounds in treated particleborard
2000 - IRG/WP 00-40180
Standard particleboard (manufactured for interior applications) was treated with trimethylborate and modified trimethylborate and then left to hydrolyse for specified periods. The percentage residual trimethylborate was determined by placing samples in kerosene and analysing the kerosene for boron after 3 days of leaching. There was a significant correlation between the percentage hydrolysis of tr...
K M Filcock, P Vinden


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...