Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


Prefacricated modular wooden bridges
2017 - IRG/WP 17-40785
The bridge consists of simple, identical pre-fabricated triangular wooden panels joined top and bottom to make up trusses. These trusses are in turn joined together side by side in pairs and are braced to one another to create a girder construction. The deck is carried on top of the trusses, an arrangement which has several advantages for such an uncomplicated structure. It is built up on site, af...
L Jayanetti


Solid Timber Bridges – Latest Developments
2017 - IRG/WP 17-40788
The technology of gluing in wood construction has evolved considerably in recent years. This has been shown especially in timber bridges that Glulam is now the main building material. A further development is the so-called block gluing, which provides a good basis for supporting structures. Numerous bridges, especially in central Europe, appeal by unique design and monolithic and solid construction. These structures base on two main developments: block lamination of glulam and the composite of timber and concrete to one structural system.
F Miebach


The potential and the challenges of acetylated wood in timber bridges - experiences from an ongoing project
2017 - IRG/WP 17-40792
Acetylated wood is known to be a durable and dimensional stable alternative for high performance materials, and has high potential for exterior timber structures. Research has shown that acetylated wood can be effectively bonded by various adhesive types. However, one of the most common used adhesives for timber constructions, Melamine Urea Formaldehyde (MUF), shows a high degree of delamination o...
A Treu, R Bredesen, F Bongers


In-service performance of treated plywood bridge decks in Australia
2017 - IRG/WP 17-40794
Engineered wood products have a long history of use in bridge construction in Australia. The first bridges incorporating chemically protected engineered wood components were installed in the 1850’s and some survive to this day. Preservative treated plywood bridge deck panels have been employed since the 1980’s as a replacement for the more traditional hardwood plank decks. This paper report...
M A Powell


The Effects of Pre-Microwave Treatment on Retention Levels And Some Mechanical Properties of Spruce Wood Treated with CCA
2017 - IRG/WP 17-40800
Microwave (MW) treatment of wood has been evaluated in recent years for different purposes by several scientists. Microwave conditioning improves permeability, reduces density and heat conductivity and changes dimensional stability. Furthermore, it could even improve the permeability of refractory wood species such as spruce and Douglas fir. In this study, MW pre-treatment was applied to spruce wo...
E D Gezer, S Kuştaş, S Durmaz


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Review on protection of timber bridges in Norway and other countries
2017 - IRG/WP 17-40809
Wood plays a major role in design and construction of modern bridges in Norway. Typical elements of those bridges are double impregnated glued laminated members, stress laminated timber decks, slotted-in steel plates, metal cladding of the surfaces of loadbearing members, and cross girders made of steel. Selected examples of timber bridges in Norway are presented. This review paper gives an overvi...
K-C Mahnert, U Hundhausen


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


A Green and Novel Technology for Recovering Copper and Wood from Treated Wood Waste – Part II: Optimization, copper metal recovery, and process design
2017 - IRG/WP 17-50326
The US consumes 70 million pounds of copper and produces 580 million cubic feet treated wood annually. The EPA disallows burning and reusing treated wood waste due to health/environmental concerns. Vast quantities of copper and wood are landfilled. Two safe and low cost extraction systems, citric acid and ammonium citrate, were identified in Part I of this study. In Part II of the study, effects o...
S Chen, R Patel


Review of Leaching Experiments of CCA-Treated Wood and Wood Treated with Copper-based Alternatives
2017 - IRG/WP 17-50330
The objective of this study was to compare leaching rates of various wood preservatives from treated wood and the tests used to gather this information. The preservatives compared included CCA and the copper-based alternatives, MCQ, ACQ, and MCA. The tests compared included AWPA E11, SPLP, TCLP, and environmental leaching tests. Among all of the tests evaluated, environmental tests most closely si...
A Jones, J Marini, H Solo-Gabriele


Uncertainty in life cycle assessment of preservative treated wood – copper and freshwater ecotoxicity
2017 - IRG/WP 17-50331
Life cycle assessment (LCA) is a method for quantifying the environmental impacts of a product over the life cycle. In the last years, there have been a growing application of LCA in developments of environmental product declaration (EPD), which is utilised by professional procurement of materials for buildings. For legislative issues, LCA have also been used to assess application of creosote to t...
L G F Tellnes


Evaluation of coating applied in treated wood: experiences in Brazil
2017 - IRG/WP 17-40814
Weathering assays study the coating degradation caused by its exposure to the action of ultraviolet radiation, winds, heat and humidity. The use of test specimens in different arrangements and exposure angles is intended to reproduce various conditions in which a product can be used. The purpose of this paper is to present the efficacy of an oil-borne varnish applied on treated wood exposed to wea...
M F Natale, J M Vidal


Corrosion verification experiment of the screw driven into CLT
2017 - IRG/WP 17-40816
Japan has abundant forest resources, but we depend on import for 70 percent of the consumed timber. Japan has the vision which promotes the timber self-sufficiency rate 30% to 50% by 2020. Therefore CLT attracts attention as a new timber material. Japan has a climate with high temperature and humidity, and wooden buildings are often treated with chemicals as a measure against biological deteriorat...
N Wada, H Ishiyama, S Yamamoto


Influence of sea water on timber and metal joints
2017 - IRG/WP 17-40818
In the Great East Japan Earthquake that occurred in March 2011, many buildings suffered from seawater immersion caused by the tsunami. Saito's study revealed that corrosion progresses on metal plate that experienced seawater immersion 1). However, the detailed mechanism of corrosion progresses has not yet been clarified. Therefore, in this study, salinity which is one of causes of corrosion w...
T Nishimura, H Ishiyama, F Hirose, N Wada


Five-year evaluation of a field trial of Eucalyptus grandis poles treated with zinc and boron
2017 - IRG/WP 17-30721
Round Eucalyptus wood treatment in sequential stages with inorganic borates and metal salts (zinc sulfate and boric acid+borax) was studied; the aims were to form an insoluble precipitate of zinc borate inside wood and to reduce treatment costs by performing the first treatment by simple ascent and diffusion of the preservative, at the same time as it was sought to impregnate the heartwood. The se...
C Ibáñez, A Camargo, C Mantero, M Rabinovich


The impact of coatings on the service life of wood decking
2018 - IRG/WP 18-20635
The durability of wood decks depends on the nature of the environment in which they are exposed to, the dimensions and configuration of the components, the resistance of the wood to degrading factors in that environment, and the maintenance performed on the deck. The present work seeks to better understand the performance of selected wood decking systems when maintained and unmaintained. This expe...
R Stirling, D Wong


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Towards durability classification of preservative treated wood – first attempts using different European standards
2018 - RG/WP 18-20638
EN 350 (2016) gives guidance on methods for determining and classifying the durability of wood and wood-based material against biological wood destroying agents. “Wood-based materials are those derived from trees and include amongst others: untreated wood, heat treated wood, chemically modified wood, glue laminated wood, wood-based panels, wood polymer composites and wood treated with wood prese...
S Bollmus, A Gellerich, C Brischke, H Militz


Certification system for treated wood and wood preservative in the relation to regulations in Japan
2018 - RG/WP 18-20639
Certification system about wood protection products in Japan is described to understand the interaction between regulations and certifying organizations. Major regulations are Building Standard Law, Chemical Substances Control Law, Poisonous Deleterious Substances Control Act, Japanese Industrial Standards, and Japanese Agricultural Standard (JAS). Treated wood products are certified with JAS mark...
K Yamamoto, I Momohara


Self-Extinguishment Phenomena of Mass Timber in Medium-Scale Compartment Fires
2018 - IRG/WP 18-30729
This paper presents a review of the fire safety risks that mass timber construction may introduce in buildings, with special consideration to medium- and high-rise buildings. These main risks are represented by an effect to the classical fire safety strategy for buildings: (1) Compartmentalisation, to ensure that the fire will not spread farther than the compartment of origin, (2) Preventing verti...
C Gorska, J P Hidalgo


Long-term performance of DMDHEU-treated wood exposed in ground, above ground and in the marine environment
2018 - IRG/WP 18-40825
Chemical wood modification with N-methylol compounds such as 1.3-dimethylol-4.5-dihydroxyethyleneurea (DMDHEU) has been studied intensively since the 1990s. Research of the past years focused on treatment of Scots pine (Pinus sylvestris L.) and European beech wood (Fagus sylvatica L.) and was shown to be applicable to improve specific material properties. A high resistance against wood-destroying ...
L Emmerich, H Militz, C Brischke


Declaring life cycle inventory of toxicity related emissions in environmental product declarations of preservative treated wood products
2018 - IRG/WP 18-50339
Life cycle assessment (LCA) including impacts on toxicity for preservative treated wood has been shown to have large uncertainties. With the growing demand for verified LCA in environmental product declarations (EPD), the need for reliable data is crucial for realistic assessment of wood products. Uncertainty is caused by several issues such as service life prediction, leaching rates and calculati...
L G F Tellnes, C Askham, P-O Flæte, M Klamer


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes