Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


Frequency of fungal decay in softwood windows in Germany
2010 - IRG/WP 10-10725
Knowing how often fungal decay occurs is a fundamental basis for general recommendations of preservative measures. To optimize the German recommendations for chemical wood preservation of windows made out of pine or spruce more than 2000 windows have been inspected. All windows had an opaque coating and were between 2 and 17 years old. The selection of the inspected windows was kept as randomly as...
D Lukowsky, O Moarcas, A Luette


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Adsorption of ionic liquids by Scots pine wood (Pinus sylvestris L.) and beech (Fagus sylvatica L.): equilibrium and kinetic modeling
2010 - IRG/WP 10-20447
In this paper methods for the adsorption study of quaternary ammonium-based ionic liquids on Scots pine (Pinus sylvestris L.) and beech (Fagus sylvatica L) are presented. Kinetic and equilibrium adsorption of compounds were evaluated. The equilibrium data fitted very well to the Langmuir adsorption models. The highest correlation coefficients determined from the pseudo-second order kinetic model ...
J Zabielska-Matejuk, A Stangierska, M Kot


Use of Internal Remedial Treatment to Extend Wood Life at the Fort Vancouver National Historic Site
2010 - IRG/WP 10-30525
The condition of wood in a reconstructed fur trading fort was assessed over a 30 year period. Poor initial treatment had resulted in the development of extensive early decay. While supplemental treatment with chloropicrin and methylisothiocyanate had arrested the attack, the results suggested that remedial treatments were unable to completely overcome the initial problems associated with treatmen...
C S Love, C Freitag, J J Morrell


A comparison of the chemistry of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-30528
This paper discusses the chemistry of the reaction of alkaline copper and micronized copper with wood. The objective of this study is to examine the copper species produced in wood during the fixation reaction using electron paramagnetic resonance (EPR) spectroscopy. The initial experiments (phases 1 to 2) were designed to confirm the effect of time of treatment and solution concentration on the s...
Wei Xue, P Kennepohl, J N R Ruddick


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Copper nanoparticles in southern pine wood treated with a micronised preservative: Can nanoparticles penetrate the cell walls of tracheids and ray parenchyma?
2010 - IRG/WP 10-30547
This study tests the hypothesis that copper nanoparticles can penetrate the cell walls of southern pine wood treated with a micronised preservative. We examined the nanodistribution of particles in tracheid and ray parenchyma cell walls using state-of-the-art HR (High Resolution)-TEM and HR-STEM (Scanning Transmission Electron Microscope)-EDX. These devices are capable of atomic-scale resolution. ...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


The kinetics of catalytic acetylation of Pinus radiata (D. Don) using conventional and microwave heating
2010 - IRG/WP 10-40485
This study outlines the effect of catalyst and microwave heating on the degree of acetylation in radiata pine. Samples of radiata pine sapwood were impregnated with potassium acetate (KAc) dissolved in two different solvents (water and methanol). Impregnated samples were dried and subjected to acetic anhydride loading followed by conventional and microwave heating. The degree of acetylation was ev...
A Kumar Sethy, P Vinden, G Torgovnikov, S Przewloka


Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod). The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov


Fungal decay resistance and mechanical properties of plywood panels made from maritime pine (Pinus pinaster) and bonded with cornstarch-quebracho tannin-phenol formaldehyde adhesive
2010 - IRG/WP 10-40490
The aim of this work is to demonstrate the performances of cornstarch-quebracho tannin-based resins designed as adhesive in the plywood production. In this way, the cornstarch and quebracho tannin was introduced in the classic adhesive formulation in order to supply a part of phenol-formaldehyde (PF). In order to evaluate the mechanical performances of optimal cornstarch-quebracho tannin-PF, plywo...
F Charrier, A Moubarik, A Allal, A Pizzi, B Charrier


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Microwave-Assisted Organic Acids Extraction of Chromate Copper Arsenate (CCA)-Treated Southern Pine
2010 - IRG/WP 10-50267
The extraction effects of acid concentration, reaction time and temperature in a microwave reactor on recovery of CCA-treated wood were evaluated. Extraction of copper, chromium, and arsenic metals from chromated copper arsenate (CCA)-treated southern pine wood samples with two different organic acids (i.e., acetic acid and oxalic acid) was investigated using a microwave reactor. Oxalic acid was e...
Bin Yu, Chung Y Hse, T F Shupe


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter


The effects of acetylation level on the growth of Postia placenta
2011 - IRG/WP 11-10751
To understand the defence mechanisms utilized by decay fungi when exposed to different wood protection systems the study of gene expression can give us some answers. When the DNA sequences are known, primers can be designed to detect transcripts of genes with gene products related to basic cellular processes and hyphal growth. The characteristic gene products induced in different fungi by differen...
A Pilgård, G Alfredsen, C G Fossdal, C J Long II


Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in wood protection are being tested and introduced, older systems are being improved, but questions still arise concerning some elements curren...
K Kängsepp. E Larnøy, P Meier


The durability of acetylated radiata pine sapwood (Accoya). Results from five years testing
2011 - IRG/WP 11-30560
New Zealand grown radiata pine sapwood was modified using the Accsys PLC acetylation process (Accoya). Following treatment, various test samples were exposed in the Scion Accelerated Field Test facility (Fungus Cellar) and in exterior ground contact field tests. In the Fungus Cellar, performance was compared with that of radiata pine treated with CCA to Hazard Classes H3.2 (0.37% m/m Cu+Cr+As) and...
M Hedley, D Page, J van der Waals, K Nasheri, G Durbin


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Copper Nanoparticles in Southern Pine Wood Treated with a Micronised Preservative: Nanodistribution of Copper in the Pit Membrane and Border of an Earlywood Bordered Pit
2011 - IRG/WP 11-30566
Copper nanoparticles can penetrate the cell walls of unlignified parenchyma cells in southern pine wood treated with a micronised wood preservative, but they are excluded from lignified tracheid walls. This paper extends these observations to include the cell wall layers of the bordered pit. Focused ion beam and ion milling were used to make an ultra-thin section of the cell wall layers of an earl...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier