IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 48 documents. Displaying 25 entries per page.


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Preservative effectiveness of medium temperature creosote oil
1990 - IRG/WP 3597
Medium temperature creosote oil (MTC) was prepared by removing light naphthalene oil and heavy anthracene oil from the coal tar by means of fractional distillation. We conducted the effectiveness test of MTC in accordance with the JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi. The soil treatment test against Serpula lacrymans was also carried out ...
S Doi, A Yamada, Y Suda


Immunolocalization of extracellular metabolites from Tyromyces palustris
1991 - IRG/WP 1491
Polyclonal antisera produced to extracellular metabolites from the brown-rot fungus Tyromyces palustris was used in immunogold TEM studies. Gold labelling was detected in the fungal cell wall and extracellular slime layer but little or sporadic labelling was noted within the cytoplasm of the fungal hyphae. Gold particles were also found within the wood cell wall of Pinus densiflora decayed by Tyro...
Yoon Soo Kim


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


Comparative studies on the species effects of wood preservatives
1989 - IRG/WP 3521
For the examination of the resistance against fungal attack, wood blocks of 3 softwood species were treated with CCA (type 3), CFK, AAC and IF-1000 independently. The wood blocks were exposed to the fungal decay with Tyromyces palustris. The degradation of the wood blocks treated with these preservatives was quite widely different among wood species examined in this study. Hem-fir treated with CCA...
K Yamamoto, S Matsuoka


Difference of CCA efficacy among coniferous wood species
1990 - IRG/WP 3601
Wood blocks of Cryptomeria japonica, Tsuga heterophylla, and Pinus radiata successively extracted with n-hexane, ether, and methanol were treated with various concentrations of CCA type 3, which were subjected to the decay by Tyromyces palustris. The weight loss were different among species and kinds of extraction. Cryptomeria japonica treated with CCA had higher fungal resistance than Tsuga heter...
K Yamamoto, M Inoue


Properties-enhanced albizzia particleboards by incorporating fungicide and insecticide in the glue
1994 - IRG/WP 94-30060
Preservative-treated particleboards were prepared by using tropical fast-growing albizzia and adding fungicides and insecticides to the adhesive-glue. the physical and biological properties of these boards were evaluated. No significant reduction in bending or internal-bond strength due to incorporation of the chemicals was detected. Treated particleboards effectively resisted attack by Coptoterme...
B Subiyanto, S Yusuf, Y Imamura, S Fushiki, T Saito, T Katuzawa


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Biological resistance of furfuryl alcohol-treated wood
1992 - IRG/WP 92-3703
Biological resistance of FFA (furfuryl alcohol)-treated wood was investigated in relation to the rise of ASE (anti-swelling efficiency) resulting from the treatment. Sapwood blocks of Japanese red pine, cedar and beech were vacuum-impregnated with various concentrations of aqueous FFA solutions to get the target levels of% (w/w) RL (resin loading). Air-dried blocks were kept in an oven at 120°C f...
J Y Ryu, Y Imamura, M Takahashi


Preliminary evaluation of new quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate for preventing fungal decay and termite attack
2005 - IRG/WP 05-30375
This study evaluates the decay and termite resistance of wood treated with didecyl dimethyl ammonium tetrafluoroborate (DBF), a recently developed quaternary ammonia compound containing boron. DBF contains boric tetrafluoride as a counter ion in its chemical structure. Laboratory decay resistance tests were performed using brown-rot fungus, Fomitopsis palustris and white-rot fungus, Trametes versi...
S N Kartal, W J Hwang, Y Imamura


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Effects of boron formulation on specific timber types used in ships of historical importance
1991 - IRG/WP 3676
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
B King, G M Smith, J W Palfreyman, S McCutcheon


The role of oxalic acid in tolerance to N’N-naphthaloylhydroxylamine in Tyromyces palustris
2006 - IRG/WP 06-10584
Certain wood decay fungi exhibit tolerance to one or more wood preservatives. Copper tolerance of brown-rot fungi has been studied in our laboratory for the past six years. We have observed some degree of tolerance to N’N-naphthaloylhydroxamine (NHA), a recently patented termite bait, by the brown-rot fungus Tyromyces palustris TYP-6137. In an effort to try and confirm this tolerance in other is...
R A Arango, C A Clausen, F Green III


Preliminary evaluation of efficacy of copper in combination with boron and NHA (N'-N-(1, 8-naphthalyl) hydroxylamine) against wood decay
2008 - IRG/WP 08-30452
In this study, efficacy of various combinations of copper sulfate with either boric acid or calcium precipitating agent, NHA-Na (N'-N-(1, 8-naphthalyl) hydroxylamine) was evaluated. Wood specimens were treated with either 1%, 0.5%, or 0.1% concentrations of copper sulfate, boric acid, NHA-Na, copper sulfate + boric acid, or copper sulfate + NHA-Na mixtures. Treated specimens were subjecte...
E Terzi, C Köse, S N Kartal


Comparison of untreated plywood and untreated LVL in a field trial against Coptotermes acinaciformis and in laboratory trials against Tyromyces palustris and Coniophora puteana
2014 - IRG/WP 14-40671
In Australasia, efficacy data obtained on plywood is generally acceptable for laminated veneer lumber (LVL) and vice versa. This is particularly the case with glueline treatment approvals. The rationale is that the two wood products have predominately the same basic structure with the key difference being orientation of the veneer. LVL typically has all veneers in parallel while plywood typical...
A Siraa, K Day, S Millward, P Lobb