Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


Effects of Nano-Wollastonite on Ignition Time Reduction in MDF
2012 - IRG/WP 12-40576
Effects of wollastonite nano-fibers on ignition time reduction in medium density fiberboard were studied. Nanowollastonite was applied at 5, 10, 15, and 20 g/kg dry weight basis of wood fibers and compared with control specimens. Two application methods of nanowollastonite were used: surface application, and internal application. Specimens of 150×130×9 mm were prepared and the ignition times wer...
H Reza Taghiyari, H Rangavar, P Noori, A Karimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Fire performance of the wood treated with retardant
2012 - IRG/WP 12-40591
To prepare the eco-friendly fire retardant wood, Japanese red pine (Pinus Densiflora), hemlock (Tsuga Heterophylla), and radiate pine (Pinus Radiata) were treated with inorganic chemicals, such as sodium silicate, ammonium phosphate, and ammonium boric acid. Different combination and concentration of those chemicals were injected by pressure treatment methods. The electron-beam treatment was used ...
Jong In Kim, Mi-ran kang, Sang bum Park, Dong won Son


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Guideline for Environmental Product Declaration for Thermally Modified Timber
2012 - IRG/WP 12-50287
Environmental Product Declarations (EPD) intend to enable the comparison of the environmental attributes of products that meet equivalent functional requirements. This guideline describes the proceedings of EPD for thermally modified timber (TMT). The main objective is the general survey on requirements on EPD which are based on European and international standards.Up to now only a few EPDs for na...
L Clauder


Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto


Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Seed oil and defatted cake proximate composition of non timber product Annona squamosa (Annonaceae) grown in Benin
2012 - IRG/WP 12-30607
Annona squamosa L. is a small tree which grows wild in many places in the tropical regions, locally called “xwingle” in Benin. Its produces edible fruits, typically globular or heart-shaped which are highly appreciated and the seeds are not used. In the course of work about identifying new oil sources from a large number of oil bearing seeds grown in Benin, we report here on the chemical compo...
T S Djenontin, J Dangou, P Lozano, D Pioch, D C K Sohounhloue


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


Survival of Bursaphelenchus xylophilus exposed to different active ingredients of wood protectors
2013 - IRG/WP 13-10802
The pine wilt nematode (PWN) Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken....
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Effect of electron beam irradiation on the fire retardant penetration into wood
2013 - IRG/WP 13-40642
Electron beam processing which can fast and easy change the nature of the material has received considerable attention recently. Studies using electron beam has been conducted in various fields and it has been applied in many industrial sectors. Electron beam has higher energy than other electromagnetic waves. It has excellent object permeability. It affects degradation of intermolecular cross-lin...
Dong won Son, Jong Sin Lee, Mee Ran Kang, Sang Bum Park


Study on Fire Resistance of Lightweight Panels Made of Honeycomb and Polyurethane Cores
2013 - IRG/WP 13-40645
In response to the increasing demand of lightweight and durable materials in furniture manufacture, potential of different skin types and cores were investigated to make proper lightweight panel. Fire resistance of panels made of different skins and cores were studied to elucidate the board’s behavior exposed to fire. Skins were MDF (3, 6 and 8 mm), particle board, plywood (3 and 5 layers) and c...
A Talaei, M Ghofrani, S Pishan


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Efficacy of commercial wood preservatives against Bursaphelenchus xylophilus, a quarantine organism in Europe
2014 - IRG/WP 14-30638
Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970, pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen. Since the nematode was detected in Europe, eradication measures were taken. However, these measures were unsu...
C S Arcos, A Navas, L Robertson, M T Troya, M Conde, F Llinares


Previous Page | Next Page