Above Ground Field Evaluation and GC-MS Analysis of Naturally Durable Wood Species
2012 - IRG/WP 12-10764
Nine wood species are being evaluated in above ground field studies in Mississippi and Wisconsin. Candidate naturally durable wood (NDW) species are being rated at yearly intervals for resistance to decay, cupping, and checking. Field ratings after 12 months exposure are presented. To date, Paulownia tomentosa (PAW) and southern yellow pine (SYP) are least durable and cedars are the most durable i...
G T Kirker, A B Blodgett, S T Lebow, C A Clausen


Preliminary laboratory and field evaluation on the performance of Rubbermite as a graded physical barrier against subterranean termite species in Australia
2012 - IRG/WP 12-10766
This paper describes the performance of Rubbermite as a potential graded particle barrier against two subterranean termite species of Coptotermes in laboratory and field test. The results of these bioassays suggest that Rubbermite is a viable control option against Coptotermes species in Australia, particularly against Coptotermes acinaciformis (Froggatt) and Coptotermes lacteus (Froggatt). Rubber...
B M Ahmed (Shiday), J R J French


Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Novel microscopic approaches to visualise chitosan within impregnated wood
2012 - IRG/WP 12-20485
Chitosan, a deacetylated product of an abundant naturally occurring biopolymer chitin, has been used in a range of applications, particularly in food and health areas, as an antimicrobial agent. In the work reported here Pinus radiata wood was impregnated with chitosan as an environmentally compatible organic biocide. It is important to understand micro-distribution of bioprotectants in impregnate...
A Singh, T Singh


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


In-ground variability of decay intensity within a test field
2012 - IRG/WP 12-20496
Timber exposed in the ground faces most severe conditions in terms of exposure to wetting and fungal decay in the terrestrial environment, therefore wood durability tests are often conducted in test fields preferably ensuring the occurrence of all relevant decay organisms. One can also expect differences in decay within an individual field-test site due to localized distribution of certain organis...
C Brischke, S Olberding, L Meyer, T Bornemann, C R Welzbacher


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Update on "Sandwich" Type Above Ground Field Test Methods
2013 - IRG/WP 13-20506
Our research group has been investigating a number of new designs for above ground field testing to try to provide rapid methods to compare the relative performance of systems in above ground, unprotected exposures. This paper provides an update on what we have found with three variations on a "sandwich" type above ground test arrangement, with comparison to the more traditional lap-joint method ...
A Zahora, L Jin, A Preston


Characterization of test fields
2013 - IRG/WP 13-20508
Test field characteristics and impact of test fields on wood degradation is important when testing wood protection. The current EN 252 standard has no requirement for knowledge of decay hazards, but most commonly a test field is known as a “brown”,- “white”,- or “soft rot” field. To understand which decay hazard wood preservatives are tested against, each test field should be character...
U Råberg, N Terziev, G Daniel


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...