Principles and procedure of the planeing test
1981 - IRG/WP 2162
Small end-sealed samples of pine-sapwood (1.5 x 2.5 x 5 cm³) are treated by brushing and afterwards different parts of the treated surface are removed. The remaining part of the sample is tested against either insects or fungi. If no attack occurs sufficient amounts of biocides have been penetrated at least beyond the zone which has been removed. In spite of some problems the test seems the only ...
H Willeitner, M Gersonde


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


IRG Working Group II. Co-operative leaching tests
1973 - IRG/WP 230
J W W Morgan


Introduction to a field demonstration of various instruments and methods for the detection of defects in poles
1984 - IRG/WP 2228
H Friis-Hansen


Field Testing of Copper Carboxylate Preservatives
2003 - IRG/WP 03-30322
This paper details our ongoing experience with field testing of copper naphthenate and other copper carboxylate preservative systems. Results from field stake tests at an AWPA Hazard Zone 4 test site are presented. In general, copper carboxylates made with ‘synthetics’ yielded results equivalent to or only slightly lower than systems with straight nap acids or nap acids amended with syntheti...
H M Barnes, M G Sanders, T L Amburgey


Coding scheme for samples for IRG world-wide co-operative field experiment
1975 - IRG/WP 360
Each sample has been given a number containing six digits (eg 16 23 05). The first 2 digits indicate the country and person supplying the timber, the second 2 digits indicate the species of timber, and the last two digits indicate the treating concentration. All samples which end with the numbers 26 to 50 are to be placed in one site in the United Kingdom, probably at the Imperial College site at ...
R Cockcroft


CEN Draft (38 N 460E) Standard: Test method for determining the protective effectiveness of a preservative in the marine environment
1986 - IRG/WP 4132
This European Standard describes a marine test method which provides a basis for asseasing the effectiveness of a wood preservative used to prevent attack of timber in sea-water by marine borers. The method is only suitable for testing preservatives which are intended to prevent attack by marine wood boring organisms of treated timber for use in more or less permanent contact with sea-water. It is...
G Castan


Depletion of boron and copper from CCB treated test specimens using different leaching protocols
2004 - IRG/WP 04-50208
The objective of this study was to measure the depletion of inorganic wood preservative components regarding the proposed OECD guideline "Estimation of emissions from preservative-treated wood to the environment: laboratory method for wooden commodities exposed in the use class 4 and 5" as part of the project "Investigations concerning the influence of test parameters on the release of biocidal ac...
E Melcher, R-D Peek, U Schoknecht, R Wegner


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 8: Panama test results
1980 - IRG/WP 458
Summary of damage to ITRG test stakes by pholadidae and teredinidae at the Panama test site - 8 Mar. '78 to 11 Oct. '79...
J R De Palma


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Performance of Tebbacop in laboratory, fungus cellar and field tests
2000 - IRG/WP 00-30222
A novel organo-copper wood preservative ("Tebbacop") has been exposed to 12 years fungus cellar testing and 6 years above ground field testing. In the fungus cellar, Tebbacop at a retention of 0.053% Cu m/m oven dry wood out-performed CCA at a retention of 0.55% m/m oven dry wood. In above ground tests, L-joints treated to a Tebbacop retention of 0.012% Cu are performing as well as joints treated ...
M E Hedley, D R Page, B E Patterson


A new wood preservative based on polymerized complexes of aminotriazole with copper acetate
1998 - IRG/WP 98-30169
This paper presents the results of preliminary fungitoxicity tests as carried out on new polymerized complexes of aminotriazole with copper acetate (PCC) against Coniophora puteana and Trichoderma viride. Laboratory tests on wood confirmed the findings arrived at in the screening test on agar medium. Deep penetration into pine wood of compounds studied was observed and particularly so at humidity...
K J Krajewski, A Lukasiewicz, J Wazny


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


A direct method for testing plywood and particle boards against fungal decay
1984 - IRG/WP 2214
A method directly inspired from the French standard testing method of the resistance of particle boards against fungal decay (AFNOR N° 51.295 May 1980) is described. But in that experimentation, the infestation is localized and realized in non sterile conditions. Small blocks of Fagus sylvatica (60 x 20 x 10 mm³) used as " inoculates " are infested with basidiomycetes, in Kolle flask for 4 to 6 ...
L N Trong


Marine test of synthetic pyrethroids at Sekondi, Ghana
1981 - IRG/WP 478
The trials reported here are part of a new series of marine exposure tests (Ghana Series 80) begun in October 1979 and designed to assess the natural durability if indigenous timber species and the performance of preservatives and preservative combinations in indigenous wood substrates in Ghana's coastal waters....
F F K Ampong


Response of the Formosan Subterranean Termite (Coptotermes formosanus) to Cellulose Insulation Treated with Boric Acid in Choice and No-Choice Tests.
2004 - IRG/WP 04-10532
The tunneling ability of the Formosan subterranean termite Coptotermes formosanus Shiraki through a cellulose insulation material containing11.1% boric acid was tested in choice and no-choice bioassays. We examined tunneling behavior and mortality of termites exposed to treated and untreated insulation material in miniature simulated wall voids. In a choice test termites tunneled through untreat...
M E Mankowski, J K Grace


Letter to the IRG meeting at Peebles, 1978
1978 - IRG/WP 181
J F Levy, R Cockcroft


Preliminary results of investigations on screening test of chemical compounds suitable for the preservation of lignocellulosic materials against biodeterioration
1976 - IRG/WP 262
This paper investigates the possibilities of reducing the time needed for the determination of the effectiveness of chemical compounds from the point of view of their eventual application to lignocellulosic materials for preservation against decay and soft-rot....
K Lutomski, S S Neyman


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


On site test for indicative determination of leaching of components of preservatives from treated timber. Part 2: New data on CCA-C, CC and CCB treated timber
1994 - IRG/WP 94-50025
The 'on site test' was published at the IRG meeting in Cannes in February 1993 (IRG/WP 93-50001/12). Since this publication many on site tests were performed parallel to so-called shower tests. The correlation between the test results of the on site tests and the shower test has been established more clearly. For chromium the correlation between both tests is indistinctive of pre...
W J Homan


Field trials of anti-sapstain products. Part 1
1991 - IRG/WP 3675
The results obtained in two field tests of anti-sapatain products, carried out in four locations in Portugal, are presented. Boards from freshly cut logs were hand-dipped, close staked and left to dry for periods from four to six months. The results obtained seem to indicate that some of the products tested performed at least as well and sometimes better, than a 3% NaPCP solution which was used as...
L Nunes, F Peixoto, M M Pedroso, J A Santos


Collaborative soft rot tests: Proposals for a standardized soil burial test
1971 - IRG/WP 201
A F Bravery


Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland


Changes in the degree of decay of lignocellulosic substrate used in a screening test of fungicidal wood preservatives
1977 - IRG/WP 287
This report contains results of investigations aimed at: a) determination of the effect of the kind of substrate and species of test fungus on quantitative changes in used samples prepared from spruce cardboard, and b) comparison of the threshold fungicidal values of come fungicides determined with accelerated method, with values obtained by block method. During performed investigations, the metho...
K Lutomski


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...