IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3387 documents. Displaying 25 entries per page.


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Baiting techniques for subterranean termite control
1983 - IRG/WP 1205
The use of artificial baits, with and without toxins, have proved effective in attracting large numbers of non-mound and mound building subterranean termites in both urban and rural areas. An outline is presented of a termite baiting program which emphasises concurrent laboratory and field investigations on termite ecology, behaviour and physiology...
J R J French, J P Robinson


Microscopic characteristics of Pinus radiata wood veneers weathered outdoors for one yea
1993 - IRG/WP 93-10018
Radiata pine (Pinus radiata) wood veneers glued to solid wood hacking strips were exposed outdoors at 45° north-facing for one year and then examined by light microscopy (LM) and transmission electron microscopy (TEM). As expected, the exposed wood surfaces were colonised by a variety of microorganisms; however, wood decay was not observed. Ultlaviolet (UV light) radiation and water were the main...
A P Singh, R A B Sweeney, E A Dunningham, D V Plackett


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu


Studies on the foraging of subterranean termites
2000 - IRG/WP 00-10345
To study the foraging galleries of subterranean termites in soil, early researchers painstakingly excavated underground tunneling system of these cryptic insects. Erhorn (1934) listed a report by Oahu Sugar Co., Ltd. in 1928 showing that runway of Coptotermes formosanus may extend up to 50 m long and 0.3 - 3 m deep. Ratcliffe & Greaves (1940) who excavated foraging galleries of Coptotermes lac...
N-Y Su


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


A note on testing the efficacy of wood preservatives above ground
1995 - IRG/WP 95-20078
A number of test methods have been used to evaluate the performance of wood preservatives in above ground situations. These have included EN 113 tests following natural exposure weathering (NEWT), L-joint or T-joint tests, lap-joint tests, and decking tests. A new test referred to as the A-frame test has been developed and is under evaluation. This is based on a sandwich-type test in which a thin ...
G R Williams, J A Drysdale, R F Fox


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


An introduction to environmental aspects of groundwater arsenic and CCA treated wood poles in Bangladesh
1997 - IRG/WP 97-50081
The environment comprises biosphere, lithosphere, atmosphere and hydrosphere. Therefore, environmental science is a multi-disciplinary study, includes life sciences, physical sciences, chemical sciences, geology, geography, meteorology, forestry, agriculture, soil science, hydrology, ecology, public health, engineering etc. Tremendous industrial and mining activities, deforestation and population ...
A K Lahiry


Report on Sub-group 5 in Raleigh, 6 May 1980
1980 - IRG/WP 1123
S Cymorek


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


In-situ pressure injection for preservation of rubber wood (Hevea brasiliensis Muel Arg.)
1992 - IRG/WP 92-3688
Rubber wood is widely used for the manufacture of furniture, doors for housing and packing cases. However in an untreated condition it is highley susceptible to sapstain and decay fungi and borers. Its utility gets considerably reduced if the wood is not treated well in time. Preservative treatment has to be given within the period of felling and transport to prevent not only loss of structural pr...
H S Ananthapadmanabha, V R Sivaramakrishnan


Inorganic wood preservative levels in soil near a noise barrier treated with different preservatives after 8 years in service
2005 - IRG/WP 05-50234
In March 1996 nine test sections of a noise barrier were installed near Stockholm Sweden. The test sections include untreated Scots pine, spruce and larch and Scots pine, treated with different wood preservatives. After 8 years in service, the untreated spruce, pine and larch boards in contact with the soil were significantly decayed, with an estimated service life of about 5-10 years, while the u...
P A Cooper, Y T Ung, M-L Edlund, J Jermer, O Söderström


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


Depletion of wood preservatives after four years' marine exposure in Mt. Maunganui harbour, NZ
1994 - IRG/WP 94-50036
This paper reports on chemical analysis of marine test samples exposed in Mt. Maunganui harbour, New Zealand from 1977 to 1981. Depletion data for a Class II CCA, a CCA-A formulation, acid copper chromate and ammoniacal copper arsenate are presented. The results suggest differences in the rate of loss of individual preservative components among the four formulations and redistribution of individua...
K J Archer, A F Preston, C M Chittenden, D R Page


The Fifth Annual Report of the International Research Group on Wood Preservation 1973-1974
1974 - IRG/WP 531
IRG Secretariat


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


Report of an investigation of damage by wood ants in buildings in Sweden
1976 - IRG/WP 148
Wood ants in buildings occur everywhere in Sweden, particularly in maritime districts and in vicinity of larger lakes. The damage caused by Camponotus herculeanus does not differ from that caused by Camponotus ligniperda. The former occurs in all Sweden, the latter only in southern Sweden. The damage is to be found almost exclusively in dwelling houses (week-end cabins and "all-the-year round" hou...
V Butovitsch


Analysis of organotin fungicides in wood preservative solutions and double-vacuum treated wood
1983 - IRG/WP 3250
A new analytical method using high-performance thin-layer chromatography (HPTLC), for the assay of organotin compounds in preservative-treated wood, is presented. The organotin compounds are extracted from the ground wood sample with a mixture of hydrochloric acid and ethanol. After HPTLC-separation, exposure of the thin-layer plate to ultraviolet light, and dipping of the plate into a 0.1% pyroca...
W Hintze, S V Ohlsson


The leachability, biological resistance, and mechanical properties of wood (Pinus sylvestris L.) treated with CCA and CCB preservatives
1999 - IRG/WP 99-30207
Scots pine (Pinus sylvestris L.) specimens treated with CCA and CCB preservative solutions (1.0%) were subjected to several fixation processes and leached elements from the specimens were determined. In addition, the specimens exposed to different fixation temperatures were subjected to soil-block test using two brown-rot fungi and one white-rot fungus in order to investigate the effects of fixati...
S N Kartal


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Previous Page | Next Page