Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya


Chemical analysis for TBTN in LOSP-treated wood and preservative fluids
1994 - IRG/WP 94-20027
Tributyltin napthenate (TBTN) is being substituted for tributyltin oxide (TBTO) in LOSP preservative formulations because its lower reactivity/better stability allows co-formulation with synthetic pyrethroids. Better stability may reduce molecular degradation both in-service and during analysis. It was considered necessary to check whether TBTO analysis methods were suitable for use on TBTN treate...
D P Wraight, M J Kennedy


Phytotoxicity of selected wood preservatives
1999 - IRG/WP 99-50133
The treated wood is used commonly around our environment. The aim of the study was to determine the reaction of plants to the wood preservatives and wood treated with preservatives. The study was made comparatively with ten types of organic and water-borne preservatives. The white mustard (Sinapis alba L.) was chosen for use as bioindicator and the tests were carried out to determine the response ...
P Witomski, J Wazny


Amines – Promising Wood Preservatives
2002 - IRG/WP 02-30287
Environmental concerns require a new approach in the field of wood protection. Band of many traditional wood preservatives has lead to intense researches for new environmental-friendly wood preservatives. Amines seem to be promising substitutes for classical biocides. Fungicidal and leaching resistance as well as some other chemical analysis of beach and Norway spruce samples treated with ethanola...
M Humar, F Pohleven, Š Kesnar, P Kalan


Review of remediation methods of sites contaminated by wood preservatives - testing of filter material for use in permeable barrier technology
1999 - IRG/WP 99-50141
Several treatment methods are currently available for treatment of contaminated sites. Soil and water can be treated by immobilisation, separation or destruction of contaminants. It has been common to use intensive treatment methods starting with soil excavation to reach strict purification goals. However, technical and financial reasons make it difficult to reach the desired treatment criteria. A...
G Rasmussen, H Iversen, S Andersen


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Copper-resistant fungi on pressure impregnated wood in Denmark
1994 - IRG/WP 94-10078
The occurence of Amorphotheca resinae Parbery and its asexual stage Cladosporium resinae (Lindau) de Vries on CCA and CCB treated wood has previously been shown. In the autumn 1993 some other blue stain fungi were found on CCP and CCB treated pine timber, such as Ophiostoma minus (Hedgc.) H. and P. Sydow, Ophiostoma pilifera (Fr.) H. and P. Sydow and Ophiostona piceae (Munch) H. and P. Sydow. The ...
J Bech-Andersen, S A Elborne


The course of fixation of Cu-Cr-As wood preservatives
1972 - IRG/WP 307
Copper-chrome-arsenic (CCA) preservatives in contact with wood result in an instant extensive increase of pH, because of ion-exchange and adsorption reactions with the wood. During precipitation of the active elements the pH continuously increases but reaches a maximum, when all chrome is consumed. Some of the early reaction products are unstable and slowly convert via dissolution into stable comp...
S-E Dahlgren


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Development of an Australasian protocol for assessment of wood preservatives
1994 - IRG/WP 94-20043
The Australasian Wood Preservation Committee (AWPC) is currently developing a suite of assessment procedures (protocols) for the biocidal efficacy of wood preservatives for approval in Australasia (Australia, New Zealand, Papua New Guinea, Fiji). Protocols are being prepared for the six hazard levels recognised in the relevant standards of member countries and represent the minimum procedures requ...
W D Gardner, H Greaves, M E Hedley, K J McCarthy, J Norton


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


International standards can we make them simple?
1996 - IRG/WP 96-20092
The earth is round and therefore limited in space. A consequence is that we - earthlings - are convicted to mutual understanding with a basic need to pay attention to others. Leading countries have been developing standards for years (i.e. USA/CANADA - AUSTRALIA/NEW ZEALAND - SOUTH AFRICA - EUROPE). They are keen and proud to argue on their peculiarities and advantages. A survey of the various sch...
G Ozanne


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Health hazards and environmental aspects when using Cu-HDO-containing wood preservatives in vacuum pressure plants
1993 - IRG/WP 93-50001-11
Apart from the biological efficacy of wood preservatives, the health and environmental aspects concerning the utilisation of wood preservatives, the use of treated timber and the disposal of impregnated wood are of high significance today. Therefore, information on a possible aerial concentration of wood preservatives, on the mobility of active substances in soil leached from treated timber in ser...
W Hettler, S Breyne, M Maier


The Use of Insect Hormones as Non-Neurotoxic Insecticides in Wood Preservatives
2002 - IRG/WP 02-30277
The ecdyson and juvenile hormone analogues show a clear difference in their effect on the house borer, Hylotrupes bajulus. In the tested dosages, the ecdyson analogues have only a slight ovicidal effect but a very clear effect on old larvae. With a dosage of 1250 mg/m², Halofenozid achieved 100% mortality after 27 weeks and Tebufenozid after 40 weeks. The two juvenile hormone analogues, Fenoxy...
E Graf, M Barkhoff, R Hamberg, H Büttner, M Pallaske


Data requirements for wood preservatives in the EU Biocides Directive
2001 - IRG/WP 01-50166-08
Directive 98/8/EC of the European Parliament and of the Council concerning the placing of biocidal products (the Biocidal Products Directive, BPD) lays down the requirements on data needed for authorisation of a biocidal product and approval of its active substance(s). The dossier must contain data needed for the proper risk assessment of the biocidal product. A detailed technical guidance documen...
H Braunschweiler


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


The preventive actions of three commercial wood preservatives against Dinoderus minutus
1984 - IRG/WP 1233
Dinoderus minutus is one of the most common pest insects for the bamboos. For preventing the damages of this insect, the preventive treatment of bamboos with preservatives is necessary. But because of the environmental reasons, only limited insecticides are available in Japan. The author determined the preventive effects of three commercial products against Dinoderus minutus by the medium of the B...
K Suzuki


The influence of gaseous oxygen concentration on fungal growth rates, biomass production and wood decay
1998 - IRG/WP 98-10283
The effects of air and several levels of oxygen balanced with nitrogen (% oxygen (v/v) nitrogen to 100%) on growth rates, biomass production and wood decay were investigated. The best technique for measuring daily growth rates in anaerobic jars was found to be by using 40 mm petri dishes which were attached to the walls of the jars. At the end of the test period the same petri dishes were also use...
S M Kazemi, D J Dickinson, R J Murphy


Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda