Decay resistance of wood treated with bio-friendly preservative systems
2016 - IRG/WP 16-30698
Due to more restrictive toxicological requirements and increased ecological awareness of consumers, wood preservatives containing biocides are no longer desired on the market. Therefore, research on new environmentally friendly formulations is of great importance. One of the possible solutions is to develop new preservatives based on natural substances, which are harmless to humans, animals and th...
B Mazela, G Cofta, W Perdoch, L Ross Gobakken, P Kwaśniewska-Sip


Increasing the hardness of wood-composite panels by nanosilver
2016 - IRG/WP 16-40715
Effect of silver nanoparticles on hardness in medium-density fiberboard (MDF) was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg, based on the dry weight of wood fibers; the results were then compared with the control panels. The size range of silver nanoparticles was 30-80 nm. Composite mats were hot-pressed for 6, 8, and 10 m...
H R Taghiyari, J Norton, K Heidarhaee


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Decay resistance of beech wood and plywood treated with different type of phenol-formaldehyde (PF) resins
2016 - IRG/WP 16-40717
In this study treatment of beech and poplar wood veneers with (PF) resin industrial scale and screening tests of nine different phenol-formaldehyde (PF) resins were made. Specifically, the effect of different phenol-formaldehyde (PF) resin types on the resistance of beech wood against brown- and white-rot fungi was evaluated. Criteria for selection of optimal (PF) resin were based on minimum WPG ...
V Biziks, S Bicke, H Militz


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Depictions on Wood: Acceptation and Internalization of Wood, which is an intercultural interaction tool, as “A Valuable Object” (Wood is Life)
2016 - IRG/WP 16-40719
Wood is a valuable material for the production of a wide variety of products, and also is a precious material in relation to its ability to provide a more appropriate and acceptable service to users. As wood is uniquely suited for a variety of uses, it has been used extensively for many purposes since ancient times, and even today it is used for a wider variety of purposes than it used to be due t...
I Usta


Depictions on Wood: Acceptation and Internalization of Wood, which is an intercultural interaction tool, as “A Valuable Object” (WoodLover Approach)
2016 - IRG/WP 16-40720
The charm, beauty, aesthetic value, easily processable structure of wood, which is a natural and organic material obtained from trees, possibility to be designed and constructed in desired form and style make it a material widely used for many purposes in our daily life as an indispensable part of our lives from past to present and make it a valuable object as it is an intercultural interaction to...
I Usta


Investigation of enzymatic effect on pit membranes by light and scanning electron microscopy
2016 - IRG/WP 16-40721
Spruce wood, one of the refractory wood species has pit membranes, which has an influence on the permeability of wood providing liquid flow between the wood cells. However, these membranes tend to close under the fiber saturated point (FSD), which makes impregnation more difficult. In this study spruce sapwood samples were treated with two different commercial enzymes to improve the permeability o...
S Durmaz, Ü C Yildiz, M Öztürk, B Serdar


A Comparison on Penetration of Silica Sol in Scots pine and Southern pine wood
2016 - IRG/WP 16-40722
Penetration is one of the most important issues to be considered in wood impregnation with various kinds of chemicals in liquid form. Scots pine (Pinus sylvestris) and Southern pine (Pinus spp.) are two frequently used wood species for treatment, such as preservative treatment. With the development of treating systems, some micro- or nano-sized aqueous modifiers are emerging in the market, which p...
Mingyang Sun, Jinzhen Cao


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Modifying wood with paraffin wax emulsion impregnation and thermal modification: hydrophobization effect and mechanism of the combined treatment
2016 - IRG/WP 16-40726
The aim of this study was to enhance the water repellency of wood by a combined treatment of paraffin wax emulsion (PWE) impregnation and thermal modification. Two different treating procedures were used to modify the southern pine (pinus spp.). One is first PWE impregnation and then thermal modification, another is first thermal modification and then PWE impregnation. The treated samples were imm...
Wang Wang, Jinzhen Cao, Cong Chen


Combustion and thermal characteristics of Korean wood species
2016 - IRG/WP 16-40727
This study examined the combustion and thermal characteristics of domestic woods in Korea. Wood was confirmed by a cone calorimeter according to the KS F ISO 5660-1 standard. The combustion properties of the wood were measured in terms of the heat release rate (HRR), total heat released (THR), mass lose rate (MLR), and ignition time (time to ignition; TTI). Also, the thermal properties were measur...
Huyun Jeong Seo, Jung-eun Park, Dong Won Son, Won-Joung Hwang


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


The durability of natural and thermomodified black poplar wood and Scots pine sapwood after two years of external exposition
2016 - IRG/WP 16-40730
Natural biological durability of many European wood species is considered to be relatively small, particularly in a ground contact conditions. This is due to the exposure of the wood to the range of biological and atmospheric destructive factors. This may to limit the scope of application of the wood of these species, particularly in construction. The biocides are often used for wood protection in...
A Fojutowski, A Kropacz, A Noskowiak


Dynamic mechanical analysis of viscoelastic properties of heat treated glycerol-impregnation poplar wood
2016 - IRG/WP 16-40732
The viscoelastic properties of glycerol-impregnated poplar wood after heat treatments at various temperatures were examined by dynamic-mechanical analysis. The spectra of storage modulus (E’) and loss tangent (tgδ) in the frequency at 10 Hz were measured at the temperature range from -100 to 300℃. Compared to no peak in E’ spectra and two relaxation processes in tanδ spectra of...
Li Yan


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Role of cell wall specific moisture content on the brown-rot fungal attack on wood
2016 - IRG/WP 16-40736
Wood is a hydroscopic resource because the cell wall polymers contain hydroxyl and other oxygen-containing groups that attract moisture through hydrogen bonding. Moisture content varies with changing moisture content in its environment. The moisture content in wood is responsible for many of the performance properties we observe. The strength properties of wood are dependent on the moisture con...
R M Rowell


Formation of hydrophobic wood surface by means of thermal treatment and surface modification with alkyl ketene dimer (AKD)
2016 - IRG/WP 16-40738
One of the major shortcomings of wood-based materials compared to technical materials is attributed to their poor dimensional stability in changing climates and in contact with liquid water. Heat treatment induces chemical change with a consequent decreasing of reactivity of the material showing unwanted surface inactivation. Alkyl ketene dimer (AKD) is a widely used sizing agent in papermaking, w...
T Lovaglio, T Meints, L Todaro, W Gindl-Altmutter


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


Enhancing wood properties through bio-based and non-biocidal co-polyesters
2016 - IRG/WP 16-40740
The commonly used wood preservation treatments are nowadays facing huge environmental issues, as well as increasing public concern. As regards those concerns, legislation tends to regulate the use of biocidal preservation chemicals. Thus, it does appear crucial to provide alternatives to the use of biocides to allow different outdoor uses of wood such as for, posts, decking, and cladding or even ...
C L’Hostis, M-F Thévenon, E Fredon, P Gérardin


Optimising wood chemical modification with lactic acid oligomers by screening of processing conditions and chemical additives
2016 - IRG/WP 16-40741
Oligomer systems based on lactic acid (OLA), were impregnated in wood and polymerised in-situ by heat treatment to improve the properties of the treated wood especially regarding anti-swelling efficiency (ASE), hygroscopicity, water leaching resistance and durability. This article relates the optimisation of the heat treatment conditions and the consideration of selected chemicals for improvement ...
C Grosse, M-F Thévenon, M Noël, P Gérardin


New perspectives for wood protection: enzyme-based treatments
2016 - IRG/WP 16-40742
Wood protection research is continuously looking for more benign and effective treatments. One of the main concerns deals with the toxicity of the active compounds employed in the formulations of the preservatives, since they could become a health and environmental issue. Secondly, long-lasting treatments are preferred in order to increase the service life of the treated wood. Weathering condition...
C Fernández-Costas, S Palanti, M Á Sanromán, D Moldes


Exterior birch plywood: potentiality of the thermo-hydro treatment
2016 - IRG/WP 16-40743
It has been found in the present study that, in laboratory fungi tests after leaching with water (EN 84), exterior birch (Betula spp.) plywood, as birch solid wood, is subjected to degradation by rot fungi. This limits the use of such plywood outdoors or in building structures in high humidity conditions. The possibility to improve the birch plywood fungal resistance was investigated in two ways: ...
B Andersons, I Andersone, A Meija-Feldmane, I Irbe, A Janberga, J Grinins


Creosote leaching from timber bridges in Norway – a practical classification approach
2016 - IRG/WP 16-40744
Creosote is widely used as a wood preservative for highway timber bridges in Norway. However, excessive creosote leaching at various highway timber bridge sites leads to a bad reputation for the use of creosote treated timber constructions and the use of wood in general. Macro- and micro anatomical factors such as amount of heartwood, annual ring width, annual ring orientation, ray- height and com...