Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat


Changes of EPR spectra of wood, impregnated with copper based preservatives, during exposure to Antrodia vaillantii
2000 - IRG/WP 00-10355
Spruce wood (Picea abies) samples were impregnated with two different aqueous solutions: copper(II) octanoate with ethanolamine or copper(II) sulfate (cCu = 1,0 x 10-2 mol/l). Impregnated and unimpregnated test pieces were exposed to wood rotting fungus Antrodia vaillantii. Some strains of this fungus are known as copper tolerant. After four weeks of exposure to A. vaillantii, we could not detect ...
M Humar, M Petric, F Pohleven, M Šentjurc


Dominant genera of fungi isolated from the surfaces of Sugi (Cryptomeria japonica D. Don) heartwood lumbers exposed at six test sites from northern to southern regions of Japanese islands
1999 - IRG/WP 99-10304
The surfaces of wood materials are disintegrated not only by sunlight and rainwater but also by microbes when exposed above ground condition. This paper deals with the investigation of fungi isolated from the surfaces of Sugi heartwood lumbers (W100 by T10 by L300 mm) exposed at an angle of 45° without ground contact for 16 months at the six test sites from northern to southern regions of Japan. ...
S Doi, M Mori, M Kiguchi, Y Imamura, M Hasegawa, S Morita, S Nakamra, Y Kadegaru


Experiences with environmental risk assessment within the Biocidal Products Directive
2005 - IRG/WP 05-50224-21
The Biocidal Products Directive (98/8/EC, the BPD) aims to authorize biocidal products based on risk assessment for both man and the environment. Active substances for wood preservation products and rodenticides were selected for the first list under the review program (Regulations EC 1896/2000 and EC 2032/2003) because several member states had experience with the evaluation and authorization of ...
P Blancquaert


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


Accelerated testing for out of ground contact using natural biological preconditioning: Part 2
1997 - IRG/WP 97-20108
Small blocks of scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. An EN 84-type leach trial was carried out on unexposed samples. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. The experiment ran for 12 months. The colonisation of t...
S Molnar, D J Dickinson, R J Murphy


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


Biocidal Products Directive 98/8/EC and PT 08
2005 - IRG/WP 05-50224-1
The ECB Biocides Work Area is responsible for the scientific and technical issues concerning the approval of active substances in biocidal products as laid down in Directive 98/8/EC concerning the placing of biocidal products on the market. The first part of the presentation will deal with the Review Programme, especially it's legal context, the status of submitted dossiers and the p...
K van der Jagt


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


What is OECD doing to promote harmonization of biocide regulations
1999 - IRG/WP 99-20182
OECD began work on biocides in 1997 to help Member countries co-operate in the assessment and registration of these products. The work is a part of OECD's Pesticide Programme, and is co-ordinated by the Biocides Steering Group. The goal is to harmonize regulatory approaches to allow countries to conduct evaluations of biocides more efficiently. More efficient evaluations can advance the p...
M Paneli, N Grandy


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Exposure of CCA and ACZA treated parallel strand lumber to marine borer attack in northeastern and southeastern waters of the United States of America
2006 - IRG/WP 06-30400
Southern pine and Douglas fir Parallel Strand Lumber (PSL) panels were treated with chromated copper arsenate (CCA) or ammoniacal copper zinc arsenate (ACZA), respectively and exposed in a marine environment in Massachusetts (northeastern USA coast) for 7 years. Similarly treated panels were also exposed to a site on the Atlantic coast Florida (southeastern USA) for the same period. In the northe...
B Goodell, P Merrick, J Jellison, Y Qian


Marine exposure assessment in southern Portugal of the natural resistance of a number of lesser known species of tropical hardwoods to teredinid and limnoriid borers
2007 - IRG/WP 07-10614
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing in the sea on the basi...
J R Williams, S M Cragg, L M S Borges, J D Icely, G S Sawyer


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Tropical In-Ground Durability of CCB-treated Keruing and other Structural Sarawak Timbers after 8 – 10 Years Exposure
2007 - IRG/WP 07-30439
The heartwood of 12 mainly low-durability native timber species of Sarawak [4 Dipterocarpus (Keruing) species, Anisoptera grossivenia (Mersawa kunyit), Canarium apertum (Seladah), Dacryodes incurvata (Seladah laut), Dryobalanops oblongifolia (Kapur kelansau), Mesua macrantha (Mergasing), Podocarpus micropedunculatus (Kayu cina), Shorea compressa (Engkabang langgai), and Pterospermum javanicum (Ba...
A H H Wong, Ling Wang Choon


Water repellency and dimensional stabilIty of wodd treated with waterborne resin acids/TOR
2007 - IRG/WP 07-40364
Wood used in above ground applications such as decking undergoes undesired dimensional changes leading to the lumber warping, cupping, splitting, etc. This is a major concern to consumers but it can be reduced by treating lumber with a water repellent. The ability of resin acids, hydrophobic compounds naturally present in southern yellow pines, was examined as a possible water repellent. A wate...
T P Schultz, D D Nicholas, J Shi


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Whole-of-house protection from subterranean termite attack and damage after four years of field exposure
2008 - IRG/WP 08-10665
This study reports the condition of the whole-of-house termite protection test in tropical Australia after four years. The study was designed to provide maximum protection to whole-of-house timbers in a natural situation posing the highest hazard from subterranean termite populations. The houses were constructed either on concrete slabs or suspended floors using untreated and treated timber fram...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J Hann, C Y Adam


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung