Anti-Fungal Activity on Some Wood extracts as a Wood Protectant
2016 - IRG/WP 16-30684
In this study, six different wood barks were used, where obtained bark extracts were blended with potato-agar in order to investigate their antifungal properties. To determine the inhibition effectiveness of extractives, two different fungi; Coniophera puteana and Trametes versicolor were selected. Fungal activity was carefully observed for the duration of seven days. Following biological testing,...
Ö Özgenç, S Durmaz


Screening of fastener resistance in contact with untreated wood using different test designs
2016 - IRG/WP 16-30686
The performance of fasteners in wooden constructions is an important aspect especially regarding corrosion resistance. In an early stage corrosion of fasteners in untreated timber becomes often visible as a discoloration on the surface of the timber resulting in bad appearance of the product followed by complaints. In order to develop an accelerated test for the assessment of fastener performance ...
E Melcher, S Wolf, U Cera


Laboratory and Field evaluation on Resistance of Thiacloprid-treated Pine Species to Termites in Mexico
2016 - IRG/WP 16-30687
The usage of Neonicotinoids for wood preservatives is common practice in several countries. Especially the active ingredient Imidacloprid is well established for this application due to its high efficacy against termites. (2Z)-3-(6-chloro-3-pyridylmethyl)-1,3-thiazolidin-2-ylidene-cyanamide, also known as Thiacloprid showed a good efficacy against Reticulitermes santonensis De Feytaud in efficacy ...
P Meckler, T Jaetsch, I Rodriguez


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


The durability of natural and thermomodified black poplar wood and Scots pine sapwood after two years of external exposition
2016 - IRG/WP 16-40730
Natural biological durability of many European wood species is considered to be relatively small, particularly in a ground contact conditions. This is due to the exposure of the wood to the range of biological and atmospheric destructive factors. This may to limit the scope of application of the wood of these species, particularly in construction. The biocides are often used for wood protection in...
A Fojutowski, A Kropacz, A Noskowiak


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


Diversity of hindgut symbiotic flagellate protist communities of the European subterranean termite in Portugal
2016 - IRG/WP 16-10875
The flagellate protist communities are an important part of the termite, as they lead the lignocellulose digestion. Termites (Reticulitermes grassei) were sampled from forest and urban environments in mainland Portugal where they are native and in Faial Island, Azores (invasive populations). Termites’ gut contents was analysed morphologically and the diversity of the flagellate protist community...
S Duarte, T Nobre, M Duarte, P A V Borges, L Nunes


Encapsulation of poles to prevent moisture uptake – a laboratory test
2016 - IRG/WP 16-40753
Premature failure of utility poles due to decay in soil contact is the main reason for early removal of utility poles, a measure that implies extra costs for utilities. Remedial treatments and barriers are common methods to prolong the service life of utility poles. The first part of this paper gives an overview of mode of action and commercial application of barrier systems as described in the li...
K-C Mahnert, U Hundhausen


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Novel wood treatments improve resistance to the wood-boring marine isopod Limnoria quadripunctata
2017 - IRG/WP 17-10899
The marine isopod Limnoria quadripunctata degrades wooden structures in the sea and causes significant economic damage. Broad-spectrum biocides and naturally resistant tropical hardwoods have failed to prevent feeding by Limnoria and have caused ecological damage. Wood modification is now the favoured method, and resin-based modifications have been effective, while the efficacy of silica-based mod...
H Bowen, M Montibus, M Kutnik, S M Cragg


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


COST FP 1303 Cooperative Performance Test – Results after two years outdoor exposure
2017 - IRG/WP 17-20620
COST Action FP 1303 ‘Performance of Bio-Based Building Materials’ started in October 2013 and an ambitious program was set up for four years. Among this a collaborative field test was planned. The idea of the cooperative performance test was to distribute a fairly simple test set up to as many places in Europe as possible in order to collect performance data reflecting the full range of climat...
B Lesar, M Humar, C Brischke, L Meyer-Veltrup, D Jones, N Thaler, J M Abascal, G Alfredsen, B Brunnhuber, E Grodås, M Irle, J Kers, M Klamer, K-C Mahnert, E Melcher, S Palanti, M Noël, E Suttie, N Pfabigan, M Touza


Guidance on the European Biocidal Products Regulation Concerning Efficacy of Wood Preservatives
2017 - IRG/WP 17-20627
In Europe wood preservatives belong to Product Type 8 (PT8) of the Biocidal Products Regulation (BPR, EU n. 528/2012), which regulates the authorisation of biocidal active substances and products in the European market. The applicant, who aims to obtain authorization to place a product onto the European market, needs to submit data to substantiate the label claims for the intended uses. Label cla...
I Stephan, M Kutnik, E Conti, M Klamer, L Nunes, J Van Acker, R Plarre


Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Decay resistance variability of European wood species thermally modified by industrial process
2017 - IRG/WP 17-40807
Thermal modification is now considered as a new ecofriendly industrial wood modification process improving mainly the material decay resistance and its dimensional stability. Most industrial thermal treatment processes use convection heat transfer which induces sometimes heterogeneous treatment temperature propagation within the oven and lead to the heterogeneity in treatment efficiency. Thus, it ...
K Candelier, L Pignolet, S Lotte, A Guyot, E Cuny, B Bousseau, M-F Thévenon


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...