Fouling and Boring Organisms Deteriorating Various European and Tropical Woods at Turkish Seas
2010 - IRG/WP 10-10741
This study aims to investigate the diversity of fouling and boring organisms damaging wood material at Turkish coasts. Trials were carried out at six harbour sites throughout the seas surrounding Turkey. Wood samples were hanged down at a depth of six meters in the sea, for a period of one year. Identification of the organisms obtained from wood plates revealed the presence of five wood borer and ...
S Şen, H Sivrikaya, M Yalcin, A Kerem Bakır, B Öztürk


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Implementation of a Quality Assurance System for thermally modified timber (TMT) by the Association of Central European TMT-Producers
2011 - IRG/WP 11-40558
Due to increasing market shares of thermally modified timber (TMT) in Europe, a working group of ten central European TMT manufacturers (TMT-WG) was founded in 2010 to cover public relations and marketing activities. Since the present level of product testing and property declaration was not satisfying, a “task group TMT-quality” was put into action in 2010 to develop a comprehensive quality a...
C R Welzbacher, W Scheiding


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Use of Acoustic Emission (AE) to detect activity of common European dry-woodboring insects: some practical considerations
2013 - IRG/WP 13-10803
Old house borer (Hylotrupes bajulus), Furniture beetle (Anobium punctatum), and Deathwatch beetle (Xestobium rufovillosum) are common dry-woodboring insects occurring throughout Europe. With the aim to prevent unnecessary use of biocidal products, to protect valuable wooden elements and objects from unwanted influences, and to have a more objective method, SHR has started to study the use of acous...
J G M Creemers


Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik


Extraction and analysis of DNA from green and seasoned timber as basic methods for determination of wood species and origin
2013 - IRG/WP 13-20523
Against the background of the European timber trade regulation EUTR, commenced to law by March 2013, the determination of wood species and tracing of its origin is getting a great importance. A promising approach for establishing fast and reliable tracking systems for wood products is DNA analysis. A critical point is the extraction of analysable DNA from the wood and its lignified cell walls. Thu...
K Jacobs, H Mende, W Scheiding


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


Potential valorization of wood extractives from waste products of steam distillation of Aniba rosaeodora: antitermitic activity
2013 - IRG/WP 13-30629
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. The wood is also composed with alkaloid compounds like anibin. These compo...
N Amusant, A Digeon


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Performance of some wood modification treatments against marine borers
2014 - IRG/WP 14-40668
Since some years, new treatment technology to protect wood against wood destroying fungi is introduced. Limited knowledge on their resistance to water organisms is available. Therefore, the resistance of chemically modified wood was assessed in a field test according to the European Standard EN 275 over a period of 3 resp. 5 years at sites in the North Sea and the Baltic Sea. Scots pine (Pinus syl...
A Klüppel, C Mai, H Militz, S Cragg


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Search for an anti-sapstain treatment for fresh radiata pine wood in compliance with European BPD norms: Field Tests
2015 - IRG/WP 15-30673
In response to the impending restrictions on the use of pesticide active ingredients developed to control the staining of fresh wood, as a result of regulation issued in 2009 by the European Union, a project was proposed to test an alternative anti-sapstain treatment that meets both the European restrictions and the performance required for an export-quality radiata pine fresh wood treatment. A se...
P Montes C, T Hanke W


Effect of natural variability of European Oak wood on heat treatment process and potential implication on wood durability
2015 - IRG/WP 15-40693
Environmental pressures appeared in France and in most European countries during the last decade has led to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative method during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Development of decay hazard maps based on decay prediction models
2016 - IRG/WP 16-20588
Durability plays a very central role in timber engineering, especially when working with wood in use class 3 and above where the risk of decay is high. As one of the primary decay influencing factors, the external condition, i.e. the local climate, is often graded by some type of climate index value. Predominately, climate indices are based on a direct relationship between weather data and decay. ...
J Niklewski, E Frühwald Hansson, C Brischke, D Kavurmaci


Engineering for Rural and Civil Development. Uni Performance of wood exterior structures above ground contact in Spain built with softwood species. The situation of cases in northern Spain
2016 - IRG/WP 16-20597
Across Europe is very common to find exterior structures build in sawn and glue-laminated wood. Most of these exterior structures used softwood wood species such as fir, spruce, larch and pine. In Spain wood exterior structures, as for example bridges, became more and more popular since eighties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spa...
D Lorenzo, J Fernández-Golfín, M Touza


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Diversity of hindgut symbiotic flagellate protist communities of the European subterranean termite in Portugal
2016 - IRG/WP 16-10875
The flagellate protist communities are an important part of the termite, as they lead the lignocellulose digestion. Termites (Reticulitermes grassei) were sampled from forest and urban environments in mainland Portugal where they are native and in Faial Island, Azores (invasive populations). Termites’ gut contents was analysed morphologically and the diversity of the flagellate protist community...
S Duarte, T Nobre, M Duarte, P A V Borges, L Nunes


Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Guidance on the European Biocidal Products Regulation Concerning Efficacy of Wood Preservatives
2017 - IRG/WP 17-20627
In Europe wood preservatives belong to Product Type 8 (PT8) of the Biocidal Products Regulation (BPR, EU n. 528/2012), which regulates the authorisation of biocidal active substances and products in the European market. The applicant, who aims to obtain authorization to place a product onto the European market, needs to submit data to substantiate the label claims for the intended uses. Label cla...
I Stephan, M Kutnik, E Conti, M Klamer, L Nunes, J Van Acker, R Plarre


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Previous Page | Next Page