Determination of total fluoride in preservative-treated wood by ion selective electrode, without steam distillation
1996 - IRG/WP 96-20086
An analytical method was developed to determine total fluoride in wood treated with aqueous fluoride or borate-fluoride formulations. Ground wood was mixed with 60% sodium hydroxide solution and oven-dried overnight before furnacing at 600°C. The cool fused product was dissolved in warm water before adding a powerful complexant/buffer solution containing sulphosalicylic acid and EDTA. Fluoride wa...
M J Kennedy


Preference of the Formosan subterranean termite for wood previously damaged by conspecifics
1988 - IRG/WP 1338
In a laboratory choice test, groups of termites from five colonies of Coptotermes formosanus Shiraki were presented with wood blocks which had sustained previous termite damage: 1) by nestmates, 2) by conspecifics from another colony, 3) by another termite species, Reticulitermes virginicus Banks, and 4) no damage. Coptotermes formosanus preferred wood previously damaged by conspecifics over that ...
J P La Fage, K S Delaplane


Moisture condition in treated wood exposed outdoors. A progress report after 5 years
1992 - IRG/WP 92-3720
Wood treated with water-borne preservatives, mainly CCA (copper, chromium and arsenic) and CCB (copper, chromium and boron) is often said to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed (Johansson 1977). In 1986 a project was started to compare water absorption during outdoor exposure between wood stakes of pine, Pinus sylvestris L, and spruce, P...
M-L Edlund


Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Dynamics of pressure changes in wood during impregnation
1990 - IRG/WP 3615
Conventional methods of impregnation have to be improved for achieving better penetration of refractory wood species. Basic requirements for an adjustment of treatment schedules are, amoung others, a profound knowledge of the course of pressure changes in the wood during treatment. A new method of pressure measurement was developed which supplies exact and reproducible data. The results show that ...
R D Peek, S Goetsch


Development on Damage Functions of Wood Decay for Building Envelope Design
2005 - IRG/WP 05-10556
For the hygrothermal analyses of building envelope systems for insulation design, we tried a natural decay test of wetted wood specimens without any inoculation of fungi. Three principal experimental types: under steady-state conditions (Experiment A), at a cyclic water dripping under Non-steady conditions (Experiment B) and at a cyclic water dipping under-steady conditions (Experiment C), were ca...
H Suzuki, Y Kitadani, K Suzuki, A Iwamae, H Nagai


Photo-discoloration and Degradation of Wood and its Stabilisation by Modification with Benzoyl Chloride
2004 - IRG/WP 04-40274
Photo degradation of Pinus roxburghii (chir pine) and Hevea brasiliensis (rubber wood) was studied under artificial accelerated weathering conditions in a Xenon test chamber. The irradiated samples were analyzed for color changes and chemical changes. Analysis of colour changes in wood surfaces by UV-Vis. irradiation was carried out using a colour measuring (CIELAB) system and chemical changes ...
K K Pandey


Studies on the destruction by marine wood boring organisms of fishing boats in the Eastern Black Sea of Turkey
1977 - IRG/WP 427
The present paper concerns the problem of fishing boats which are attacked by wood boring organisms in the Black Sea of Turkey. The aims of this study are: 1) to identify the marine wood boring organisms attacking fishing boats in the Northern Black Sea of Turkey; 2) to identify the wood species that are used in boat building construction and assess their durability; 3) to assess the degree of att...
R Ilhan, O A Sekendiz


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


Sterilization of mango wood (Mangifera indica L.) without heat
1995 - IRG/WP 95-30065
Researches revealed that boric acid can play an important role for sterilizing wood instead of heating. Wet (green) mango boards (Mangifera indica L.) were pressure treated in treating cylinder at initial vacuum of 508 mm Hg for 15 minutes and impregnation pressure of 7 kg/cm² for 4 hours with 5% solution (w/v) of 1:1:1 commercial grade (95% pure) sodium dichromate, copper sulphate and boric acid...
A K Lahiry


Ammoniacal wood preservative for use in non-pressure treatment of spruce and aspen poplar. Part 1
1984 - IRG/WP 3273
End-matched lumber of Picea glauca (Moench)Voss (white spruce) and Populus tremuloides Michx. (aspen poplar) timbers was treated by a thermal diffusion process in open tank treating vessels using an ammoniacal copper-arsenate wood preservative. The process proved technically feasible with respect to controlling the vapourization of ammonia from open tanks during treatment at high temperatures. Tre...
C D Ralph, J K Shields


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Canadian code of good practices - Recommendations for design and operation of wood preservation facilities
1990 - IRG/WP 3582
The rationale and procedures for the development of a set of recommendations for design and operation of wood preservation facilities in Canada are discussed. Multi stake holders involvement in problem identification, problem assessment, state of the art knowledge database, implementation and periodic assessment procedures are important considerations for the successful development of a Code of Go...
V N P Mathur, G Das


List of wood-destroying fungi in Iran
1976 - IRG/WP 138
This list gives information on the wood-destroying fungi collected in the Iranian forests and from felled logs and boards in sawmills until now. They are mainly from the region of the Caspian Forests and from the climatically dry region between Teheran and Azarbaidjan, North Iran. It is understood, that this document may help to give more knowledge outside the country about the specific problems o...
P Soleimani


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Novel observations on the micromorphology of soft rot attack of wood
1996 - IRG/WP 96-10176
Electron microscopic examinations of decaying Pinus radiata horticultural posts which had been treated with CCA preservative prior to being placed in service about nine years ago showed the presence of soft rot fungi and tunnelling bacteria. Some novel observations on the micromorphology of the soft-rotted areas of tracheid walls are described here. The micromorphology of soft-rotted areas was hig...
A P Singh, R N Wakeling


Practicability of bioassays in the evaluation of environmental risks in wood protection
1996 - IRG/WP 96-50071
As an example for the proofing of the practicability of bioassays in the evaluation of environmental risks in wood protection the ecotoxicological behaviour of CCF-impregnated timber was examined. After vacuum pressure impregnation specimen from shaped pine poles were tested on ecotoxicological effects of leachable compounds using sensitive aquatic organisms like fish, Daphnia and algae as bioindi...
H-W Wegen


The reliability of colouring methods for the determination of biflourides and boron in spruce wood
1994 - IRG/WP 94-20036
From practical reasons, qualitative spraying methods are widely used for the detection of bifluorides and boron in wood. The main aim of this research was to detect whether the concentration of the active ingredient in the coloured area is equal or greater than the toxic value against basidiomycetes. Both colouring methods, Z-A reagent for fluorides and curcuma reagent for boric acid, are a reliab...
R Grell, M G Sanders, W J Homan, H Militz


Rapid analytical methods for wood waste - An overview
1998 - IRG/WP 98-50104
The proper handling of wood after service is a today's problem. Untreated wood could be reused or may be used as fuel. For treated wood special care is demanded to avoid environmental impacts. Thus, analytical methods are requested to detect rapidly whether and to what extend wood is contaminated, covering a wide spectrum of organic and inorganic agents used during the last 50 years. Trad...
A Peylo, R-D Peek


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Issues Facing Wood Preservation in New Zealand Today
2003 - IRG/WP 03-30326
In New Zealand, the three major issues facing the wood preservation industry today are: Extension of use of LOSP preservatives, chiefly tributyltin naphthenate, for treatment of products in Hazard Class H3 exposed to the weather for which LOSP have not been traditionally used. Concerns have been expressed about the long-term durability of such products. Restrictions on the use of CCA preservativ...
M E Hedley


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Fixation of chromated copper arsenate (CCA) wood preservative in Australian hardwoods: A comparison of three Eucalyptus species
1996 - IRG/WP 96-30107
New environmental guidelines for the management of CCA treatment plants were released in Australia in 1995. This has stimulated interest in techniques for controlling or accelerating the fixation of CCA in freshly treated timber products. The ability to understand, then effectively control and/or accelerate fixation of CCA in treated timber products can be an economic, technical and environmental ...
J Holmes


Biocontrol and bioprotection of wood decay and sapstain fungi
2003 - IRG/WP 03-10474
The most serious damages caused in the wood industries by decay and sapstain fungi, and the growing international pressures on the use of biocides products with toxic active ingredients harmful to human health and the environment, have made it necessary to search for alternative chemical products to protect the wood, and for the possibility to use micro-organisms as biological controllers. This la...
M T De Troya, F Rubio, M Villarreal, F Arenal, F Llinares, V Rubio, D Muñoz-Mingarro, N Acero