IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 124 documents. Displaying 25 entries per page.


Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2013 - IRG/WP 13-20535
A round robin involving 15 European participants was set up in 2006. The round robin consists of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. When comparing EN 84 preconditioning (two weeks water leaching) with natural preconditioning (1 year in field, above ground) according to CEN/TS 15397, no significant difference...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, B Mazela, E Melcher, R Möller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Performance of untreated wood and wood impregnated with copper-ethanolamine based preservative solutions in Northern Adriatic Sea
2013 - IRG/WP 13-30623
Sea water applications of wood are among the most challenging ones. Impregnated wood is exposed to leaching and to variety of marine borers, Limnoria sp. and Teredo sp. being the most important. In the present research, durability of pine wood impregnated with copper-amine based preservative solution (Silvanolin) of different concentrations, exposed to the sea water, was investigated according to ...
M Humar, M Petrič, J Adamek, B Lesar


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Performance of some wood modification treatments against marine borers
2014 - IRG/WP 14-40668
Since some years, new treatment technology to protect wood against wood destroying fungi is introduced. Limited knowledge on their resistance to water organisms is available. Therefore, the resistance of chemically modified wood was assessed in a field test according to the European Standard EN 275 over a period of 3 resp. 5 years at sites in the North Sea and the Baltic Sea. Scots pine (Pinus syl...
A Klüppel, C Mai, H Militz, S Cragg


Biological Performance of Triadimefon in combination with Tebuconazole in laboratory and field tests
2015 - IRG/WP 30668
The usage of Triazole-combinations for wood preservatives is common practice in several countries. Especially the combination of Tebuconazole and Propiconazole is preferred for this application due to its broad spectrum of efficacy against wood destroying fungi. 1-(4-Chlorphenoxy)-3,3-dimethyl-1-(1,2,4-triazol-1-yl)-butanon, also known as Triadimefon provides a good efficacy against the wood destr...
P Meckler, T Jaetsch


The situation of the industrial protection of wood in Argentina (La situación de la protección industrial de la madera en Argentina)
2015 - IRG/WP 15-30675
Argentina holds 33 million hectares of native forests and 1.2 million hectares of cultivated forests, which make it the 3rd Latin American country with the largest surface of cultivated forests of the region. (Ministry of Industry, 2012). The industrial impregnation of wood through vacuum pressure was first implemented in our country in the year 1932, and currently there are over 100 active plants...
D A Gherscovic


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Can CCA be substituted as reference preservative?
2018 - IRG/WP 18-20641
While field testing of wood protective formulations remains probably the best method to find out the effective preservative concentration, the use of chrome-copper arsenate (CCA) as reference becomes debatable due to environmental and legislative reasons. This emerges from the European standardization bodies who have discussed reference alternatives that can omit the use of CCA. The present debate...
N Terziev, M Jebrane, P Larsson Brelid, N Morsing, P-O Flaete, P Torniainen, J S Kim, G Daniel


Influence of different triazoles as co-biocides in wood preservatives on efficacy and the environmental impact
2018 - IRG/WP 18-50333
In this study we investigated the efficacy and impact on the environment of different co-biocide triazoles in wood preservatives. Four different formulations (all containing 9.5% Copper) contained individual and combinations of cyproconazole, tebuconazole, propiconazole as co-biocides. Four formulations were tested according to EN 113 and EN 84 (ageing) to determine the brv for each formulation. T...
M Klamer, T Jensen, S Bang-Achton, E Morsing


Resistance against marine borers: About the revision of EN 275 and the attempt for a new laboratory standard for Limnoria
2020 - IRG/WP 20-20669
Wood protection technology in the marine environment has changed over the last decades and will continue to do so. New active ingredients, newer formulations, and novel wood-based materials including physically- and chemically-modified wood, together with increasing concerns over environmental impacts of wood preservatives, urgently demand a major revision of EN 275 “Wood preservatives – Deter...
S Palanti, S Cragg, R Plarre


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Copper-octanoate - a potential reference preservative replacement for CCA in field test standards?
2022 - IRG/WP 22-20688
Finding a CCA reference replacement for use in standardised test methods is of high priority since this chemical is being phased out and may in the near future be banned also for experimental and approval purposes. In this paper we assess the possibility to replace CCA reference preservative with an historical copper octanoate product. There is a huge amount of lab and field test data available fo...
R Ringman, M Westin, M Klamer, A Christof, F Friese


Durability against fungal decay of sorbitol and citric acid (SorCA) modified wood
2022 - IRG/WP 22-40928
Most European-grown wood species are susceptible to biological degradation, specifically, they suffer from a poor resistance against wood-destroying fungi. Therefore, prior to outdoor exposure, wood has to be treated either by applying a protective coating on its surface or by full-volume impregnation with antifungal chemicals. However, due to environmental and health concerns, the most frequently...
K Kurkowiak, L Emmerich, H Militz


Mini-stakes – an alternative test method for EN 252?
2023 - IRG/WP 23-20691
Market approval of wood treatment products requires knowledge and prove of long-term durability. Efficiency of wood treatment with a specific product is evaluated based on variety of tests, including penetration evaluation, leaching studies as well as decay tests. EN 252 standard test is a core method for wood durability evaluation in a ground contact, both for commercial product approval and scie...
R Digaitis, P Larsson Brelid, N Terziev, M Klamer, A W Christof, J Stenaek, N Morsing


Adhesion and performance of exterior wood coatings on chemically and thermally modified wood – Results from 5.5 years outdoor exposure
2023 - IRG/WP 23-40964
Non-durable softwood and hardwood species were treated with the water-soluble cyclic N-methylol compounds 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) and methylated DMDHEU. One half of the modified specimens were coated with a waterborne acrylic coating system prior a natural weathering for 5.5 years according to EN 927-3 (2020). By frequent evaluations, the impact of chemical modifications ...
L Emmerich, H Militz


On the use of miniaturized wood specimens in fungal decay experiments – mini-blocks versus EN 113 test specimens
2024 - IRG/WP 24-11044
Preliminary evaluation and classification of wood durability against decay fungi using laboratory monoculture experiments has been a longstanding practice because these tests offer quicker results than field tests. Various methods, including miniaturized specimen formats and different incubation periods, have been explored to expedite decay processes and assess wood preservation efficacy. The 'min...
C Brischke, G Alfredsen


Previous Page