10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Overview of the treated wood quality control program in the United States with the recent challenges and advances
2017 - IRG/WP 17-20616
In the past two decades, there have been significant and rapid changes in wood protection technologies for residential applications which have moved away from long established heavy duty metal oxide based products such as chromated copper arsenate (CCA). The successor generation of wood protection systems usually contain copper as the primary biocide, in combination with carbon-based co-biocides s...
L Jin


New Standards for Approval of Modified Wood within the Nordic Wood Preservation Council (NWPC)
2017 - IRG/WP 17-20624
In the Nordic countries, there is a long tradition for quality labelling of preservative treated wood. Until now the labelling has been restricted to pine and other easy to treat wood species, but with the introduction of a new set of standards it is now possible to obtain the Nordic Wood Preservation Council’s (NWPC) quality labelling also for modified wood. In this paper, we will introduce th...
N Morsing, E Engelund Thybring, M Klamer


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Can CCA be substituted as reference preservative?
2018 - IRG/WP 18-20641
While field testing of wood protective formulations remains probably the best method to find out the effective preservative concentration, the use of chrome-copper arsenate (CCA) as reference becomes debatable due to environmental and legislative reasons. This emerges from the European standardization bodies who have discussed reference alternatives that can omit the use of CCA. The present debate...
N Terziev, M Jebrane, P Larsson Brelid, N Morsing, P-O Flaete, P Torniainen, J S Kim, G Daniel


Influence of different triazoles as co-biocides in wood preservatives on efficacy and the environmental impact
2018 - IRG/WP 18-50333
In this study we investigated the efficacy and impact on the environment of different co-biocide triazoles in wood preservatives. Four different formulations (all containing 9.5% Copper) contained individual and combinations of cyproconazole, tebuconazole, propiconazole as co-biocides. Four formulations were tested according to EN 113 and EN 84 (ageing) to determine the brv for each formulation. T...
M Klamer, T Jensen, S Bang-Achton, E Morsing


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Durability and climate change - implications for wood building structures
2019 - IRG/WP 19-50361
Sustainable building practices are rooted in the need for reliable information on the long-term performance of building materials; specifically, the expected service-life of building materials, components, and assemblies. This need is ever more evident given the anticipated effects of climate change on the built environment and the many governmental initiatives world-wide focused on ensuring that ...
M Lacasse


Durability of tropical species from Peru according to European Standards
2020 - IRG/WP 20-10964
Natural durability is defined as the intrinsic resistance of wood against the attack of destructive organisms. There are standardized methods to estimate a durability value. In Europe, the standard EN-350 is responsible for establishing the basic guidelines, as well as the necessary tests to determine this value, which is essential to know the degree of protection needed for the tested wood to ext...
J Valdivia, P Gómez, M T Troya, L Robertson, J A Martín, A Loayza


Resistance against marine borers: About the revision of EN 275 and the attempt for a new laboratory standard for Limnoria
2020 - IRG/WP 20-20669
Wood protection technology in the marine environment has changed over the last decades and will continue to do so. New active ingredients, newer formulations, and novel wood-based materials including physically- and chemically-modified wood, together with increasing concerns over environmental impacts of wood preservatives, urgently demand a major revision of EN 275 “Wood preservatives – Deter...
S Palanti, S Cragg, R Plarre


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Development of procedures for sampling, testing, and classification to determine the biological durability of wood and wood products
2020 - IRG/WP 20-20676
This paper informs about a research project, which deals with several shortcomings and a lack of clarity within EN 350:2016. The project started in January 2020, will run for 3 years, and is operated by the Institute of Wood Technology Dresden (IHD) and the University of Goettingen (UGOE). Determination and classification of durability of wood and wood products against wood-destroying organisms ...
W Scheiding, K Jacobs, S Bollmus, C Brischke


Durability against fungal decay of sorbitol and citric acid (SorCA) modified wood
2022 - IRG/WP 22-40928
Most European-grown wood species are susceptible to biological degradation, specifically, they suffer from a poor resistance against wood-destroying fungi. Therefore, prior to outdoor exposure, wood has to be treated either by applying a protective coating on its surface or by full-volume impregnation with antifungal chemicals. However, due to environmental and health concerns, the most frequently...
K Kurkowiak, L Emmerich, H Militz


Mini-stakes – an alternative test method for EN 252?
2023 - IRG/WP 23-20691
Market approval of wood treatment products requires knowledge and prove of long-term durability. Efficiency of wood treatment with a specific product is evaluated based on variety of tests, including penetration evaluation, leaching studies as well as decay tests. EN 252 standard test is a core method for wood durability evaluation in a ground contact, both for commercial product approval and scie...
R Digaitis, P Larsson Brelid, N Terziev, M Klamer, A W Christof, J Stenaek, N Morsing


Effect of Moisture Cycles and Timber Treatment on the Performance of Screwed Connections
2023 - IRG/WP 23-20694
The impact of moisture in timber structures is associated with the deterioration of timber, and loss of mechanical performance. Methods have been developed to treat timber using chemicals to inhibit deterioration, however, water intrusion has much more immediate effects on the mechanical properties of timber associated with swelling and shrinkage of the wood. The effects of moisture on the mechani...
L Yermán, M Xiao, Z Yan, L-M Ottenhaus


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Laboratory durability testing of preservative treated wood products – first attempts and observations
2023 - IRG/WP 23-20697
In the past, durability classes (DC) had been assigned to wood species, sometimes also to homogenously modified wood-based materials such as thermally modified wood. More recently, some standards allow for classifying the biological durability of chemically modified wood, preservative treated wood and wood composites. Even treated products may be subject to durability classification, but necessary...
C Brischke, M Sievert, M Schilling, S Bollmus


Adhesion and performance of exterior wood coatings on chemically and thermally modified wood – Results from 5.5 years outdoor exposure
2023 - IRG/WP 23-40964
Non-durable softwood and hardwood species were treated with the water-soluble cyclic N-methylol compounds 1,3-dimethylol-4,5-dihydroxyethyleneurea (DMDHEU) and methylated DMDHEU. One half of the modified specimens were coated with a waterborne acrylic coating system prior a natural weathering for 5.5 years according to EN 927-3 (2020). By frequent evaluations, the impact of chemical modifications ...
L Emmerich, H Militz


On the use of miniaturized wood specimens in fungal decay experiments – mini-blocks versus EN 113 test specimens
2024 - IRG/WP 24-11044
Preliminary evaluation and classification of wood durability against decay fungi using laboratory monoculture experiments has been a longstanding practice because these tests offer quicker results than field tests. Various methods, including miniaturized specimen formats and different incubation periods, have been explored to expedite decay processes and assess wood preservation efficacy. The 'min...
C Brischke, G Alfredsen