Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Five years field test results for CCA and ACQ preservatives fixed in different climates
1999 - IRG/WP 99-30208
During assessment of the ground contact stakes in the Norwegian test field, we have found that very often the first visual rot attack is in the zone of the stakes were the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour. To investig...
F G Evans


A real scale evaluation method and results on termite resistance of housing wall systems and floor framings
1999 - IRG/WP 99-10314
For evaluating the termite resistance of real scale houses especially housing wall systems and floor framings, a experimental building was prepared. After initial feeding of termite, this house was constructed. In this experimental building, several parts which were built by different wall systems and floor framing. The room temperature of these parts were controlled. Water can be provided in the ...
K Suzuki, K Okada, K Hagio, Y Tanaka


Blue stain in timber in service. Preliminary results of the IRG collaborative tests to compare natural and artificial weathering
1978 - IRG/WP 286
The collaborative programme was initiated at IRG Meetings in Wildhaus, 1976. The six collaborators were BAM (Berlin), Cuprinol Ltd (UK), EMPA (Switzerland), GORI (Denmark), PRL (UK) and Imperial College (UK). Experimental plans were finalised in December 1976 and panels treated by Cuprinol Ltd early in 1977. Natural weathering was carried out by BAM, Cuprinol, EMPA, GORI and PRL during April-Septe...
A F Bravery, D J Dickinson


Soft rot tests with soils of different origins
1984 - IRG/WP 2226
In the BAM a comparative soft rot test with 9 different types of soil (one soil each from Canada, New Zealand and Switzerland and 6 soils from laboratories in Germany) were carried out. The pH values of the different soils ranged from 3.2 to 7.1, and the amounts of organic matter were between 4 and 44% (w/w). The test specimens - Pine sapwood blocks treated with different concentrations of a CCA p...
M Gersonde, W Kerner


Physiological properties of fungal test strains according to the European Standard EN 113
1986 - IRG/WP 2258
For the discussion of the European standard EN 113 the EMPA's procedure of culturing the test fungi and the corresponding virulence of the test fungi as well as the wood moisture content at the end of the test are shown. It is mainly shown that within the standard the choice of the solvent may not be left at the test lab if reproducible results shall be obtained. The different solvents in...
E Graf, B Zgraggen, P Manser


A review of the implementation of results-based standards for preservative treated timber
1999 - IRG/WP 99-20156
European standards for the specification of preservative treated timber are written in terms of the results achieved in the commodity by the treatment process. This is described in terms of penetration and retention of preservative. Results from a study on the commercial application of this approach in the UK show the difficulties associated with applying the new European standards; particularly w...
E D Suttie, A S Hughes, R J Orsler


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Information from the COIPM wood group. (With Appendix: Préserver les matériaux en milieu marin sauvegarder l'environment marin telles sont la vocation et la mission du C.O.I.P.M.)
1989 - IRG/WP 4156
During the last COIPM Meeting, up to date information on cooperative work to test the resistance of plastic wrapping for pilings were submitted and discussed. In 1986 untreated wood samples wrapped with shrinkable polyolefin sleeves were submerged in 9 stations, situated in temperate and tropical waters. After 1 or 2 years of immersion the samples showed no sign of penetration by marine borers and...
A Gambetta


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


LCA examination of preservative treated timber products and alternatives; initial results
1995 - IRG/WP 95-50040-04
Co-operative development of an LCA methodology suitable for application to preservative treated products has been carried out, based on scoping assessments of two products, CCA treated fenceposts and creosote treated distribution poles. The general results of these scoping exercices are described, based on the CCA case study. These include the identification of critical stages in the life-cycle on...
W Hillier, R J Murphy, D J Dickinson, J N B Bell


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


Melamine resins as preservatives results of biological testing
1996 - IRG/WP 96-40061
Based on previous work of the authors on resins, the upgrading of wood with a true solution of a methanol etherificated melamine resin in low aqueous concentration was performed. For the relative assessment of the biological resistance against brown and white-rot fungi were used not only untreated controls of pine sapwood (Pinus sylvestris L.), but also heartwood of European larch (Larix decidua M...
A O Rapp, R-D Peek


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


A comparison of shower test results from CCF, CCZF, CCB and Cu-quat treated timber
1995 - IRG/WP 95-50054
The shower test quantifies the amount of specific preservative components which leach from treated timber under simulated open storage conditions. The test method measures leaching from both organic and inorganic salt treated timber. Shower tests of CCF, CCZF, CCB and Cu-quat treated timber which have been performed over the last 5 years by TNO are reviewed and compared. Leached components are qua...
M J Boonstra, A J Pendlebury, P Esser


The results of detection on CCA components of the soils contacted with CCA-treated woods - A trial study for the availability of the burial Method as a disposal CCA treated wood waste
1993 - IRG/WP 93-50005
The objecteve of this experiment is to get a knowledge that, when CCA treated wood wastes were buried in a soil as a disposal, the soil would be or not be contaminated by the components of CCA preservatives in wood wastes. The specimens used were cutting logs and chips made of the CCA treated electric pole waste. The soil was buried to the 15 cm depth and the log specimens were set in the soil for...
K Suzuki, H Sonobe


The role of chromium in wood preservatives - The situation and new results concerning biological efficacy
2006 - IRG/WP 06-30397
A heavy discussion about the status of chromium-containing compounds in wood preservatives has ensued in the European Union since the Biocidal Product Directive 98/8/EG has come into force.The origin of this discussion is the fact that according to the Biocidal Product Directive chromium trioxide and sodium dichromate have been identified as active ingredients and therefore the placement of wood p...
P Jüngel, H Härtner, E Melcher


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim