New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli


Results of chemical analyses in the field of wood preservation in the Bundesanstalt für Materialprüfung
1973 - IRG/WP 321
The results of qualitative and quantitative chemical analyses of wood preservatives are often the basis for evaluating the various works in the field of wood preservation. In the past 10 to 15 years a number of such works was carried out in the Bundesanstalt fur Materialprüfung, Berlin-Dahlem, dealing with the identification and effectiveness of wood preservatives and with methods of wood preserv...
H J Petrowitz


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis


Japan's comments on ISO/DIS 12583-1/2
1996 - IRG/WP 96-20100
The paper describes an accelerated field test for the evaluation of timber preservative formulations against subterranean termites. The method has been adopted by the South African wood preservation industry as a screening method for the approval of wood preservatives for use under SA conditions. The method which is based upon the fungal cellar test offers a rapid means of evaluating the comparati...
P Turner, D Conradie


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


Performance of preservative-treated hardwoods with particular reference to soft rot. Report of condition of specimens installed in Victoria, Australia
1980 - IRG/WP 3155
J Beesley, R McCarthy


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 2nd Interim Report
1981 - IRG/WP 477
Three reference wood species - Alstonia scholaris, Fagus sylvatica and Pinus sylvestris, untreated and treated with 3%, 6% and 10% CCA and CCB solutions were supplied to all participants for submergence at local sites. Regular examination of samples is being carried out - 6 months, 12 months and then annually for 7 years....
R A Eaton


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Non-pressure treatability of plywood by CCA, CCB and boron
2005 - IRG/WP 05-40295
Study on diffusibility and absorbability of CCA, CCB and boric acid in 3 mm thick 3-ply hardwood plywood at water saturated and air-dry conditions and dipped at same concentration (5%) and same duration of time (12 hours) revealed complete diffusion of all the preservatives at water saturated condition. Only the CCA-C was found absorbed by the plywood at air-dry condition. The rate of absorption a...
A K Lahiry


A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker


Insect resistance of preservative treated tropical plywood against Lyctus
1990 - IRG/WP 1453
Seven plywood types composed of tropical wood species, vulnerable to Lyctus, were treated with various commercial water-borne and oil-borne preservatives. A wide range of preservative retentions was obtained by treating boards with dip treatment, steeping, double-vacuum and vacuum-pressure impregnations. Selected samples were subsequently tested for their insect resistance against Lyctus africanus...
J Van Acker, M Stevens, M Pallaske


A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada


The Third Annual Report of the International Research Group on Wood Preservation 1971-1972
1972 - IRG/WP 511
IRG Secretariat


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma