IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3715 documents. Displaying 25 entries per page.


Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Production of treated wood in Brazil in 1982 and 1983
1985 - IRG/WP 3327
The data of Brazilian production of treated sleepers, poles, crossarms, fence posts and other commodities are given for the years of 1982 and 1983. This report updates information given to the Group in Document No: IRG/WP/3321 Wood Preservation in Brazil, STU information no 445...
M S Cavalcante


Current and future options for managing used preservative-treated wood
1995 - IRG/WP 95-50042
The amount of preservative-treated wood available for disposal will continue to increase exponentially in the next several decades as landfill availability declines. At the same time, recent legal ruling on competitiveness among utilities and disposal of ash has clouded the economic outlook for combustion of treated wood for energy recovery. This report identifies current and future options for ma...
R C De Groot, C Felton


nvestigation of anomalous fixation and leaching of CCA-treated red maple
2004 - IRG/WP 04-30341
The fixation of CCA-C preservative was investigated in red maple sawdust (Acer rubrum L.) at target retentions of 4.0, 6.4, 9.6 and 30.0 kg/m3. The effect of water-soluble extractives on the course of fixation was evaluated comparing the non-extracted with pre-extracted samples treated to 6.4 and 30 kg/m3. Leaching of the CCA components was monitored after complete fixation for all retentions. Fix...
S Radivojevic, P A Cooper


Ultrastructural and TEM-EDAX studies on the degradation of CCA treated radiata pine by tunnelling bacteria
1985 - IRG/WP 1260
An ultrastructural study was carried out on bacterial attacked Pinus radiata stakes treated with a high level (24.7 kg/m³) of Tanalith NCA preservative. The purpose of the investigation was to determine whether the organism possessed intracellular and/or extracellular detoxification mechanisms in order to overcome the high levels of copper, chrome and arsenic present within the wood fibre walls. ...
G F Daniel, T Nilsson


Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


An interim report on studies of the tolerance by Sphaeroma (Crustacea: Isopoda) of CCA-treated timber
1982 - IRG/WP 491
In Papua New Guinea any untreated timber exposed to seawater close to mangrove stands is liable to be attacked in the intertidal zone by the crustaceans Sphaeroma terebrans or Sphaeroma triste. Even CCA-treated timber is sometimes vulnerable. The mouth-parts of these animals are adapted for boring, but whether wood particles are ingested remains to be resolved. Some limbs of Sphaeroma terebrans ap...
S M Cragg, J D Icely


Environmental issues: Messages for the wood preservation industry
1985 - IRG/WP 3353
A review of the origins and structure of environmental legislation throughout those territories of the world where wood preservation is a major industry is given. The implications of media, industry and legislation interaction is discussed and suggestions made as to the key issues the wood preservation industry should concentrate its attentions on in the immediate future....
D G Anderson, P Waldie


Wood in concrete. Summary of discussion at IRG 14, Surfers Paradise, Australia
1984 - IRG/WP 3264
The performance of untreated and preservative treated wood when placed in direct contact with concrete was considered in a discussion session at IRG 14. While published reports in this area are scarce, research is in progress internationally and a variety of practices are currently available to minimize any additional hazard posed by contact with concrete. This report summarizes the points raised ...
R J Murphy


Analysis of organotin fungicides in wood preservative solutions and double-vacuum treated wood
1983 - IRG/WP 3250
A new analytical method using high-performance thin-layer chromatography (HPTLC), for the assay of organotin compounds in preservative-treated wood, is presented. The organotin compounds are extracted from the ground wood sample with a mixture of hydrochloric acid and ethanol. After HPTLC-separation, exposure of the thin-layer plate to ultraviolet light, and dipping of the plate into a 0.1% pyroca...
W Hintze, S V Ohlsson


Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French


Comparative evaluation of the barrier effect against Hylotrupes bajulus L. of different types of wood preservative
1986 - IRG/WP 1307
This paper settles the difference of contact action against females of Hylotrupes bajulus the likelihood of egg-laying, the ovicide effect and the hazards of development of newly hatched larvae between some preservatives belonging to three differents types: mineral waterborne products, organic products and emulsions. The results show that against females, the action is fast with organic products, ...
M-M Serment


The formation of organotin carboxylates in bis(tributyltin) oxide - treated Pinus sylvestris sapwood
1990 - IRG/WP 3618
Tributyltin compounds have been successfully used for many years as wood preservatives, although their chemical nature in timber have not been fully elucidated. This study by 119Sn and 13C NMR spectroscopy has shown that, on impregnation into Pinus sylvestris sapwood, bis(tributyltin) oxide, (Bu3Sn)2O, is rapidly converted to tributyltin carboxylates, Bu3SnOCO·R, via reaction with components of t...
S J Blunden, R Hill


Oxygen index levels and thermal analysis of wood treated with melamine-formaldehyde-boron combinations
1997 - IRG/WP 97-30135
Melamine formaldehyde (MF) resin was impregnated into scots pine (Pinus sylvestris L.) specimens with aqueous solutions of 5, 10 and 20% concs. Boric acid (BA) and borax (BX) was added to MF resin at the concentration levels of 0.25, 1.00 and 4.70% to each level of resin concs. BA and BX mixture was prepared at the 5:1 (w/w) ratio considering resultant pH of solutions and better fire resistance. U...
M K Yalinkilic, W-Y Su, Z Demirci, E Baysal, M Takahashi, S Ishihara


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Depletion of wood preservatives after four years' marine exposure in Mt. Maunganui harbour, NZ
1994 - IRG/WP 94-50036
This paper reports on chemical analysis of marine test samples exposed in Mt. Maunganui harbour, New Zealand from 1977 to 1981. Depletion data for a Class II CCA, a CCA-A formulation, acid copper chromate and ammoniacal copper arsenate are presented. The results suggest differences in the rate of loss of individual preservative components among the four formulations and redistribution of individua...
K J Archer, A F Preston, C M Chittenden, D R Page


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


Previous Page | Next Page