Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Draft of a mongraphic card for Serpula himantioides (Fr.) Karst. according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 174
L Harmsen


Trends in environmental management in industry. Implications for wood preservation activities
1993 - IRG/WP 93-50001-34
J A De Larderel


A new accelerated field test for termites
1983 - IRG/WP 1178
A new accelerated field test method for termites is described. Two series of tests were conducted with this accelerated method and the results were very encouraging....
W E Conradie, A Jansen


Oxalic acid production of fifteen brown-rot fungi in copper citrate- treated southern yellow pine
2001 - IRG/WP 01-10388
Non-arsenical copper-based wood preservatives have grown in number since the 1980's as a response to environmental concerns posed by arsenicals. Interest in copper tolerant decay fungi has increased accordingly. Oxalic acid (OA) production by brown-rot fungi has been proposed as one mechanism of copper tolerance. Fifteen brown-rot fungi representing the genera Postia, Wolfiporia, Serpula,...
F Green III, C A Clausen


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


Programme section 3, Wood protecting chemicals
1996 - IRG/WP 96-30119
IRG Secretariat


Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist


The present classification of wood degradation factors
1993 - IRG/WP 93-10031
Contemporary classification of biotic and abiotic wood degradation factors is presented in two aspects: etiological and simptomatical one....
J Wazny


OECD's latest activities on wood preservatives
2001 - IRG/WP 01-50166-05
PPT-Presentation...
M Paneli


Work program of CEN/TC 38 (April 1993). Durability of wood and wood-based products
1993 - IRG/WP 93-20012
R Hüe


Wood extractive concentration and sem examination of pretreated southern yellow pine wood chips with blue-stain fungi for mushroom production
2001 - IRG/WP 01-10407
Mushroom-producing white-rotting basidiomycetes either do not colonize or else colonize very poorly on freshly prepared southern yellow pine wood chips. This study evaluates the resinous extractive content of southern yellow pine before and after treatment with colorless mutant blue-stain fungi. The blue-stain fungi penetrate into the sapwood of southern yellow pine and utilize nonstructural resin...
S C Croan, J Haight


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


A review of environmental emissions from building and construction materials in comparison with preserved wood
2005 - IRG/WP 05-50224-11
A review of the public domain literature concerning emissions to the environment from materials which are used in the construction of buildings (e.g. Concrete, Asphalt, Galvanised Steel), in comparison with preserved wood, and a review of the approaches taken by the construction sector in assessing the risk from environmental emissions, in comparison with the approaches taken by the wood preservat...
E F Baines


Errata to Document No: IRG/WP/3276
1984 - IRG/WP 3285
W E Conradie


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


A field test with Benzotar, an industrial residue, as a wood preservative
1985 - IRG/WP 3349
Benzotar, a residue of production of benzoic acid, was tested in field as a wood preservative. Results, after 6.5 years of exposure, showed that this product presents properties that improve the performance of wood in ground contact. This paper describes these results and presents a discussion an some aspects of its potential utilization in Brazil....
S Milano, L R Silva


Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen