IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 275 documents. Displaying 25 entries per page.


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


A review of the analytical methods used in determining the decay resistance of heat treated wood
2015 - IRG/WP 15-40690
Heat treatment as a wood process is increasingly used because of its non-biocide behaviour and its low environmental impact. This sort of treatment is based on biopolymer chemical degradation by heat transfer. This process improves mainly the dimensional stability and the decay resistance of wood. Wood becomes darker after this type of treatment and thus gives it an aesthetic appearance. These i...
K Candelier, M-F Thévenon, A Pétrissans, S Dumarçay, P Gérardin, M Pétrissans


Durability of reaction to fire performance of FRT wood products in different end use applications – Methods and results
2015 - IRG/WP 15-40705
Fire retardant treatments (FRT) may considerably improve the reaction to fire properties of wood-based products and the highest fire classifications for combustible products can be reached, but the maintained reaction to fire performance e. g. in exterior applications needs to be addressed in order to form a basis for new and reliable wood products with improved fire performance. A European Techn...
B Östman, L Tsantaridis


Cultural heritage – research into innovative solutions and methods for historic wood conservation
2016 - IRG/WP 16-10874
Nowadays, interdisciplinary knowledge, tools and techniques are increasingly used to protect and conserve monuments representing our cultural heritage. This is of great importance especially in case of conservation and restoration of wooden historic artefacts which, as a result of physical, chemical and biological corrosion, have lost their technical, aesthetic and decorative properties. If those ...
M Broda, B Mazela


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


A review on prediction methods of wood natural durability
2017 - IRG/WP 17-10892
Natural durability of timber may be defined as “inherent ability of timber to attack by wood destroying organisms (bacteria, fungi, insects, marine borers) without preservative treatment. On the base of biological tests, EN-350-2 standard (Afnor, 1994), describe the classification of wood species according to their natural durability. But these specifications are not adapted in the case of wood ...
N Amusant, C Flora, J Beauchène, E Houël, C Duplais


Comparison of 1H qNMR and NIR spectroscopic methods to predict heartwood decay resistance in Dicorynia guianensis Amsh
2017 - IRG/WP 17-20601
Dicorynia guianensis is by far the most exploited wood in French Guiana, as it is an abundant tree species associated with good technological properties. However, the decay resistance of D. guianensis wood against lignivorous fungi pathogens is sometimes variable. Therefore, the development of tools to predict the decay resistance of D. guianensis heartwood is relevant in wood science and agrofore...
C Flora, G Frédéric, M-F Thevenon, Y Estevez, C Duplais, N Amusant


Three-Dimensional Digital Image Correlation of Strains in Profiled Wood Decking Exposed to Wetting & Drying
2017 - IRG/WP 17-20611
We use three dimensional digital image correlation to measure the strains that develop at the surface of profiled radiata pine (Pinus radiata D. Don) deck boards subjected to a wetting and drying cycle. We hypothesise that surface profiling will change the pattern of strain distribution at the surface of deck boards by concentrating stresses at the base of profile grooves. Five groups of three deck board samples were produced from five different pieces of machine stress-graded radiata pine wood. Two wavy profiles, ribble or ripple, were tested. Flat unprofiled boards acted a control. Each board was fixed to a rigid frame and subjected to a wetting and drying cycle. Full field surface strain data was collected using 3D digital image correlation. Strains varied across the surface of both flat and profiled boards. Profiling changed surface strain patterns; strain maxima and minima developed in the profile ridges and grooves during wetting, respectively, but this pattern of strains reversed during drying. Such a pronounced reversal of strains was not observed when flat boards were exposed to wetting and drying, although there was a shift towards negative strains when flat boards were dried. We conclude that profiling changes surface strain distribution in deck boards exposed to wetting and drying, and causes high strains to develop in the grooves of profiled boards. These findings help explain why checks in profiled deck boards are mainly confined to profile grooves where they are difficult to see, and the success of profiling at reducing the negative effects of checking on the appearance of wood decking.
J Mallet, S Kalyanasundaram, P D Evansa


Towards durability classification of preservative treated wood – first attempts using different European standards
2018 - RG/WP 18-20638
EN 350 (2016) gives guidance on methods for determining and classifying the durability of wood and wood-based material against biological wood destroying agents. “Wood-based materials are those derived from trees and include amongst others: untreated wood, heat treated wood, chemically modified wood, glue laminated wood, wood-based panels, wood polymer composites and wood treated with wood prese...
S Bollmus, A Gellerich, C Brischke, H Militz


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Influence of Drying Condition of Wood on Rusting of Nail
2019 - IRG/WP 19-40887
Recently in Japan, the durability of metal joint in wooden structures become important. Revised Building Standard Law was enacted in 2000 and Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2008 in Japan. Since then, the durability of the metal joints in the wooden houses becomes important. But there are not any detailed regulation for the durability of the metal...
H Ishiyama, N Wada, T Nishimura, T Mori


Knowledge exchange and transfer from academia to industry in the field of wood protection research – Activities of the IRG-WP Communications Committee
2019 - IRG/WP 19-50354
The International Research Group on Wood Protection (IRG) was founded in 1969 as a structured group of like-minded scientists and technologists focused on generating knowledge of the science of wood deterioration, and novel solutions to provide sustainably and environmentally responsible products for the protection of wood-based materials. The primary function of the IRG is to provide opportunitie...
F Latorre, B Abbott, C Brischke, M Humar, D Jones, E Larnoy, L Nunes, A Preston, T Singh


New methods for estimating the volume of shipworm tunnels supported by image analysis
2020 - IRG/WP 20-20668
In marine environment, the main threat for wood is the bioerosion by woodborers, both peracarid crustaceans (such as gribbles Limnoria and pincher scuds Chelura) and bivalve molluscs (shipworms, Teredinidae). The damage caused by gribbles on wood structure is surficial and easy identifiable, whereas the damage caused by shipworms is internal, therefore not evident, inducing unexpected crashes wit...
I Guarneri, M Sigovini, E Keppel, D Tagliapietra


Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Green approach in wood mineralization for improvement of fire properties
2022 - IRG/WP 22-30769
Various treatments have been developed in order to improve fire properties of wood. Because the use of some flame retardants can release toxic compounds in the event of a fire, leading to poisoning or even death of people from smoke inhalation, the use of no-toxic and more ecologically acceptable flame retardants is preferable. Mineralization of wood with the incorporation of carbonates has proven...
A Pondelak, R Repič, L Škrlep, N Knez, F Knez, A S Škapin


Improving wood durability by mineralisation and thermal modification
2022 - IRG/WP 22-40948
A significant increase in the fungal durability of wood was achieved by using a modification procedure combining two environmentally friendly methods: thermal modification and mineralisation. It offers an ecological alternative to other biocidal treatments. European beech (Fagus sylvatica) and Norway spruce (Picea abies) were selected as model wood species and exposed to four different fungi: Gloe...
R Repič, A Pondelak, D Kržišnik, M Humar, A S Škapin


Field test methods as long-term aging – report of selective wood properties
2023 - IRG/WP 23-40962
Wood samples from a long-term field test are a valuable compendium of information about the material in the context of its aging processes. In the current work, wood samples from the round-robin test within the ECOMOD project were used as a material for the natural aging process (III and IV class of utility). The research scope was to determine selected properties of this wood which can be partial...
W Perdoch, M Benc, B Mazela, A Szulc, J Cegiela


Impacts of elevated moisture levels and subsequent drying on screwed
2023 - IRG/WP 23-40970
Mass timber (glue-laminated timber, cross laminated timber (CLT) and laminated veneer lumber) are increasingly used in mid-to high rise structures in Australia where the climate is mainly sub-tropical with elevated moisture levels and high termite risk. Moisture intrusion poses a major challenge anywhere but becomes more critical under these conditions. Untreated/non-durable materials are consider...
C M T Roder, C D Gerber, J J Morrell


The impact of pre-drying on treatment level variations of esterified solid wood analysed by X-ray densitometry
2023 - IRG/WP 23-40977
Wood modification requires homogenous treatment levels within the wood matrix to prevent insufficiently treated areas being subject to biodeterioration. Esterification of wood by citric acid and sorbitol can show differences in density caused by uneven chemical distribution during the curing phase and can be detected by x-ray densitometry. This study used density profiling to investigate the influ...
A Treu, S O Amiandamhem, E Larnoy


Utilising novel service life prediction methods for robust and precise Life-Cycle-Costing (LCC)
2023 - IRG/WP 23-50384
Life-Cycle-Costing (LCC) is one of the basic indicators for the assessment of sustainability and cost effectiveness in construction applications. Project WoodLCC was thus conceived to enable LCC through input from models for detailed service life planning of wooden components and buildings. The project is a continuation of the service life planning research conducted in Europe over the last three ...
P B van Niekerk, G Alfredsen, T Kalamees, R Modaresi, A Sandak, J Niklewski, C Brischke


Phytosanitary heat treatment of wood in a laboratory drying oven and, in a pilot-scale kiln using the house longhorn beetle (Hylotrupes bajulus) larvae as a model
2024 - IRG/WP 24-20722
International trade in wood products brings the risk of the movement of tree pests which can cause devasting ecosystem and economic damage. International phytosanitary guidelines were created to help countries that import wood products. Import requirements intend to minimize pest spreading. Thus, the ISPM 15 (International Standards for Phytosanitary Measures No. 15) which specifies the “Regulat...
B Rubio, C L’Hostis, M Montibus, I Paulmier, C Brunet, L Charron, J-P Gaussorgues, C Guiberteau, V Vlahakis, F-R de Cibon, I Le Bayon


Previous Page