A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown on inert surfaces
1997 - IRG/WP 97-10194
A range of wood inhabiting and wood decay fungi have been studied for their production of extracellular mucilage when grown on inert surfaces, for comparison with their growth on wood. The species tested were: Coniophora puteana, Coriolus versicolor, Chaetomium globosum, Trichoderma harzianum, Ceratocystis coerulescens, Ophiostoma piceae, Mucor sp. and Penicillium sp. They were grown on plastic me...
A R Abu, R J Murphy, D J Dickinson


The practice of using concrete on wood piling for marine use in Thailand
1982 - IRG/WP 492
The practice of using concrete on wooden poles has been carried on in Thailand for a long time in pile-houses and pier constructions which have been situated in, or partly in the sea. In such instances, the hewed round and/or square-sawn heartwood poles of naturally durable timber species have been coated with concrete of about 5 to 10 cm or more in thickness, and to about 100 cm above the highest...
B Anuwongse


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


Limiting Conditions for Decay in Wood Systems
2002 - IRG/WP 02-10421
Hygrothermal models can predict temperature and moisture conditions in wall components subjected to real weather data, but specific data and a fundamental understanding of how temperature and wood moisture content dictate the progression of decay under these conditions is required for modellers to predict consequences of decay on building performance. It is well understood that wood will decay abo...
P I Morris, J E Winandy


Proposed model for the penetration and decay of wood by the hyphal sheath of the brown-rot fungus Postia placenta
1989 - IRG/WP 1391
Scanning electron microscopy (SEM) of Pinus sp. decayed by the brown-rot fungus Postia placenta confirmed the existence of extracellular membranous structures previously described by transmission electron microscopy (TEM). These structures appear to be an integral part of the hyphal sheath and assume a variety of forms including lamellar sheets, fibrils, and vesicles. These structures were observe...
F Green III, M J Larsen, L L Murmanis, T L Highley


A study of the colonization of wood blocks in a laboratory unsterile soil test
1988 - IRG/WP 2318
CCA treated and untreated beech blocks were exposed to a defined horticultural loam using the method proposed for the collaborative soft rot test in the soft rot sub-group of Working Group Two. At intervals during the incubation wood samples were removed and fungal isolations were made using selective media. Fungi were identified and tested for their cellulolytic ability and their decay capacity i...
M T De Troya, S M Gray, D J Dickinson


Detection of Termite Attack to Wood Stakes in a Monitoring Station Using Ceramic Gas Sensors and Acoustic Emission (AE) Sensor
2003 - IRG/WP 03-20271
To evaluate the termite activity in monitoring stations non-destructively, metabolic gas from termites and acoustic emission generated by feeding of termites were measured. Ten cylindrical stations with small wood stakes of Japanese red pine (Pinus densiflora) were buried around a house attacked by Coptotermes formosanus SHIRAKI. A sample air in the station was collected by sucking through a drill...
Y Yanase, Y Fujii, S Okumura, T Yoshimura, Y Imamura, T Maekawa, K Suzuki


Relationship of wood durability and extractives
2003 - IRG/WP 03-10493
The durability of the following five wood species, Zelkova carpinifolia, Ulmus glabra, Pterocarya fraxinifolia, Carpinius betulus and Acer laetum, were studied. Wood blocks were exposed to Coriolus versicolor under laboratory conditions according to DIN 52176 standard. After 16 weeks incubation the heart wood of Z carpinifolia showed 2,19 % weight loss, U glabra 41,69 %, C betulus 45,64 %, A laetu...
S M Kazemi


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


A comparison of effectiveness of three waterborne preservatives against decay fungi in underground mines- An appraisal
2005 - IRG/WP 05-30366
To understand the effectiveness of waterborne preservatives and to explore the behaviour of roof supporting poles after pressure treatment, an experiment was conducted and thorough investigation was carried out during the last decade in the underground mines. Prior to commencement of the experiment, a survey was conducted at different depths in underground mines and collected decayed wood samples ...
P Narayanappa


Inadequacies in preservative retention and formulation as contributory causes of premature failure of CCA-treated vineyard posts
1984 - IRG/WP 3280
Analyses of severely decayed or failed vineyard posts and examination of stake test data on effectiveness of copper-chrome-arsenate (CCA) preservatives have suggested two contributory causes of premature failure of vineyard posts: 1. Preservative retentions in posts are such that after 15 years' exposure some decay is inevitable. 2. The high arsenic, low chrome formulations with which the...
M E Hedley


Antifungal properties of metabolites produced by Trichoderma isolates from sawdust media of edible fungi against wood decay fungi
1994 - IRG/WP 94-10051
Trichoderma isolated from a sawdust medium of Pholiota nameko produced filtrates which had antifungal activities to four wood decay fungi tested on the agar plates. Filtrates produced from another isolate, from a sawdust medium of Lentinus edodes, had antifungal activities only to the white rot fungi, Coriolus versicolor and Pycnoporus coccineus. These results did not agree with those from earlier...
S Doi, M Mori


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


Laboratory evaluation of potential antisapstain treatments for Pinus radiata
1983 - IRG/WP 3237
Twelve formulations were tested in the laboratory using a 'mini' board test for effectiveness on Pinus radiata (D. Don) against sapstain, mould and decay fungi. Three formulations, sodium pentachlorophenoxide (NaPCP) plus borax, Haipen 50 WP, and Mitrol 375, are used commercially in New Zealand. Busan 1009 (0.5% product), IWD Product A (0.2% ai), IWD Product B (0.3% ai), Fennotox...
J A Drysdale


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker