IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 269 documents. Displaying 25 entries per page.


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


A preliminary assessment of the penetration into wood achieved by bodied mayonnaise emulsion wood preservatives
1992 - IRG/WP 92-3725
Five different commercial formulations of bodied mayonnaise emulsions were applied to samples of Scots pine (Pinus sylvestris) sapwood as recommended by the manufacturers. Penetration and loading characteristics were determined by measuring the distribution profiles of the active ingredients after various intervals of time. The changes in the general appearance of the emulsions on the surface of t...
G E Holland, R J Orsler


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


Effects of alkali treatment on some mechanical and chemical properties of creosote treated oaks
1991 - IRG/WP 2366
To date, there is a lack of information on the effects of chemical treatment on the performance of creosote preservative treated oak sleepers. This factorial experiment was designed to analyze three main effects: species (Quercus alba and Quercus rubra) creosote treatment (treated and untreated), and alkali (NaOH) soaking (0, 1, and 10 percent). The modulus of elasticity (MOE) and fiber stress at ...
P Chow, A J Reinschmidt, E J Barenberg, L C Chang


Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...
A P Singh, Yoon Soo Kim


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Proposals for further co-operative studies on determining toxic values against wood-destroying Basidiomycetes
1985 - IRG/WP 2247
Document IRG/WP/2194 reported the status of the programme of co-operative experiments up to and including December 1982. During discussions at IRG-13 in Turkey members endorsed the decision to complete the programme of tests and conduct repeat tests. At IRG-14 in Brisbane the report was noted but no further action agreed. At IRG-15 in Sweden a number of interested parties in the European/Scandinav...
A F Bravery


Production of exraxellular hydrogen peroxide and oxalic acid by brown-rot fungus Poria placenta
1995 - IRG/WP 95-10112
Hydrogen peroxide and oxalic acid have been suggested to be essential in the degradation of wood carbohydrates by brown-rot fungi. Hydrogen peroxide has been suggested to be one of the diffusible low molecular weight agents produced by brown-rot fungi for the degradation of wood carbohydrates by generating highly active radicals. The production of hydrogen peroxide and oxalic acid by Poria placent...
A-C Ritschkoff, M Rättö, J Buchert, L Viikari


Degradation of lignin model compounds with coordinated copper in the presence of peroxide
1998 - IRG/WP 98-10282
A novel diffusible system capable of decomposing lignin model compounds with copper, coordinators and peroxides has been proposed. When pyridine was used as a copper coordinator, two synthetic dyes, Poly-R and RBBR were intensively decolorized with Cu(II) and H2O2 in aqueous solutions at room temperature. Although reactions with Cu(II) and H2O2 produce a strong oxidant, hydroxyl radical, via a Fen...
K Koller, K Messner, T Watanabe


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


The rôle of lignin in the nutrition of several Australian termites
1983 - IRG/WP 1191
The ability of Nasutitermes exitiosus (Hill), Coptotermes acinaciformis (Frogatt), Coptotermes lacteus (Froggatt) and Mastotermes darwiniensis (Froggatt) to degrade 14C-lignin preparations was examined. The lower termites were unable to degrade lignin. Nasutitermes exitiosus was able to cause a 5-8% degradation of hardwood lignins and a synthetic lignin. It failed to degrade the lignin of Pinus ra...
L J Cookson


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


Giftwirkung einiger organischer Zinn-Verbindungen auf Eilarven von Hylotrupes bajulus (L.). [Toxic efficacy of some organic tin compounds against egg larvae of Hylotrupes bajulus (L.)]
1978 - IRG/WP 2120
The toxic values of 12 organic tin compounds towards newly hatched larvae of Hylotrupes bajulus were determined after 4- and 12-week test periods in comparison with bis-tri-n-butyltin oxide (TBTO). Tri-n-butyltin benzoate as well as the 2-, 3- and 4-methyl benzoate of tributyltin oxide were equally effective as TBTO and the latter two were somewhat more effective after a 12-week test period. Almos...
G Becker


The degradation of wood by metal fastenings and fittings
1972 - IRG/WP 302
As well as the hazards of biological decay, timber used in boat building is subject to the effects of chemical decay associated with the corrosion of metallic fastenings. The title has been deliberately chosen to emphasize that in wooden construction the troubles are not just those of corrosion of the fastenings, but also the destructive secondary effects on the wood caused by the products of the ...
L C Pinion


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


New approaches to practical evaluation method of bio-degradation of wooden construction - Non-destructive detection of defects using radar technique
2000 - IRG/WP 00-20214
There have been a number of researches and developments on the techniques and apparatus for the nondestructive evaluation of the biological deterioration in wood and wooden constructions, such as decay or insect attack in house, public buildings or in historically important architectures. As for the detection of the decay in wood, techniques using sound in audible or in ultrasonic frequency ranges...
Y Fujii, Y Komatsu, Y Yanase, S Okumura, Y Imamura, M Tarumi, H Takiuchi, A Inai


Lignin degradation by a non-enzymatic system supposed to be active in white rot fungi
2000 - IRG/WP 00-10340
Electron microscopic investigations have shown that ligninolytic enzymes of white-rot fungi are only able to penetrate the wood cell wall in late stages of degradation. Thus, the selective degradation of lignin of certain white-rot fungi can only be explained on the basis of a low molecular weight, highly diffusible system. A system, consisting of copper, a coordination compound and either H2O2 or...
P Lamaipis, W Gindl, T Watanabe, K Messner


Aspects of leaching
1976 - IRG/WP 267
With respect to Document No: IRG/WP/246, and the recommendation that an economic leaching test can be based on a non-changing volume of water (500 ml/block), I would like to relate our experiences with this suggestion. Following 14 days of continuous immersion in de-ionized water it was found that blocks treated with moderate and above concentrations of a preservative gave no problems, but those b...
R S Smith


Marine trials with water-borne salts and organotin compound
1986 - IRG/WP 4128
Pinus sylvestris blocks treated with water-borne salts (CCA, CCB, CCF) and organotin compounds (TBTO, TBTCl) were submerged in the sea at Follonica station. The results obtained after 12 years of immersion are presented. The samples treated with CCA, CCB and CCF at the lowest concentration (2%) were destroyed after 7-9 years and the samples treated with CCB and CCF at the highest concentrations (4...