IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1463 documents. Displaying 25 entries per page.


Detection of defects in standing poles by X-ray techniques
1980 - IRG/WP 2132
The application of X-ray techniques to wood pole inspection procedures has been evaluated. Internal defects were accurately identified using X-ray inspection methods. These methods and their possible influence on the safety and economic aspects of wood pale utilization are discussed....
W D Gardner, R S Johnstone, W Pitt


A technique for the quantitative isolation of Actinomycetes from decayed wood
1980 - IRG/WP 1116
A technique combining comminution and high-speed homogenisation has been developed for the preparation of suspensions of micro-organisms in colonised wood. When standard inocula of Streptomyces spores were applied to wood, constant proportions of the inocula were recovered. This method was used in conjunction with selective culture media to isolate actinomycetes from wood which had been buried in ...
A A W Baecker, B King


Proposal for further work on pretreatment decay
1988 - IRG/WP 1374
Pretreatment decay is a world wide problem sometimes ignored by pole producers. Words like "poles are not worse now than they were 50 years ago" or "we have always handled poles in this way without trouble" are weak defences. All other industries try to make their products better, so why not the impregnation industry? Or is the pole industry right? What do we know about the long term effect of pre...
M-L Edlund


Long-term effectiveness of fumigants in controlling decay in Douglas fir waterfront timbers
1986 - IRG/WP 3364
The persistence, movement, and effectiveness of chloropicrin and Vapam (sodium N-methyl dithiocarbamate) in large, horizontal Douglas fir timbers were evaluated 7 years after fumigation. Chloropicrin prevented reestablishment of decay fungi; reinvasion occurred in some Vapam-treated timbers. Residual fungistatic effect was detected up to 1.2 m from the fumigation site in chloropicrintreated timber...
T L Highley


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings


Performance of surface-treated hardwoods and softwoods out of ground contact
1990 - IRG/WP 3592
A number of fungicides were tested as brush treatments for protection of southern pine, Douglas-fir, maple, and red oak against decay above ground. Cross-brace and L-joint test units were treated just before assembly and exposed from 3-10 years. Untreated Douglas-fir cross-brace units were not decayed at either the Mississippi or Madison, WI, site. Untreated red oak cross-brace units were not deca...
T L Highley


Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Decay patterns observed in butylene oxide modified ponderosa pine attacked by Fomitopsis pinicola
1983 - IRG/WP 1183
Small blocks of ponderosa pine chemically modified by butylene oxide to three different weight percent gains (WPG) were decayed for 2 months with the brown rot fungus Fomitopsis pinicola. Wood substance loss and the type of decay pattern recognised were fairly similar both for control and blocks treated to 8 and 15 WPG. No difference in attack was observed between radial or tangential walls in lat...
T Nilsson, R M Rowell


The effect of sapwood on the rate of deterioration of fence posts
1986 - IRG/WP 1277
In order to evaluate the effect of the presence of sapwood on the rate of deterioration of fence posts, 30 specimens with and without sapwood of Eucalyptus citriodora, Eucalyptus paniculata, Eucalyptus saligna and Eucalyptus tereticornis were exposed in three test sites in the State of São Paulo, Brazil. The results of the inspection carried out in 1985, after 5 years of exposure, are reported in...
M S Cavalcante, G A C Lopez, E S F Mucci, R G Montagna


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


What can DNA fingerprinting, aggression tests and morphometry contribute to the identification of colonies of the Formosan subterranean termite
2000 - IRG/WP 00-10371
Multilocus DNA fingerprinting, aggression tests and morphometry were compared to evaluate their potential for the identification of colonies of the Formosan subterranean termite, Coptotermes formosanus (Isoptera: Rhinotermitidae) in Hawaii. DNA fingerprinting separates the termites from all studied collection sites. Since the genetic similarity between termites from different collection sites lies...
C Husseneder, J K Grace


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


A critical review of the AWPA standard method (M12-72) for laboratory evaluation to determine resistance to subterranean termites
1986 - IRG/WP 1298
The American Wood Preservers' Association standard (M12-72) for evaluation of candidate wood preservatives against subterranean termites is reviewed and suggestions for revision are made. The most serious flaws in the current test procedure involve a failure to recognize inter- and intraspecific variation and a lack of quantification of test results....
J P La Fage, M Jones


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Collaborative soft rot tests: Summary of comments on 'Proposals for a standardized soil burial test'
1971 - IRG/WP 202
J G Savory


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff


Description of the damage produced by xilophagus Curculionides in Spain
1989 - IRG/WP 1408
Cossoninae are a reduced subfamily of Curculionidae. These xilophagus insects produce significant damage in Spain, mainly affecting old buildings. Their activity is a real problem for the preservation of the country's historical-artistic heritage. The three Cossoninae species most widespread in Spain are described for the first time as well as the conditions under which they develop. The ...
E L Rodríguez Trobajo


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Previous Page | Next Page