IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1386 documents. Displaying 25 entries per page.


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Properties-enhanced albizzia particleboards by incorporating fungicide and insecticide in the glue
1994 - IRG/WP 94-30060
Preservative-treated particleboards were prepared by using tropical fast-growing albizzia and adding fungicides and insecticides to the adhesive-glue. the physical and biological properties of these boards were evaluated. No significant reduction in bending or internal-bond strength due to incorporation of the chemicals was detected. Treated particleboards effectively resisted attack by Coptoterme...
B Subiyanto, S Yusuf, Y Imamura, S Fushiki, T Saito, T Katuzawa


Decay in window joinery in Sweden
1977 - IRG/WP 390
Systematic investigations of decay in window joinery in Sweden have not been undertaken until very recently. One might guess that one of the reasons for the minor interest is that this type of joinery did not rot strikingly faster than people expected. In the last 10-15 years, however, house owners, tenantowners, building societies and others have repeatedly argued that windows do rot more than in...
B Henningsson


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven


Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Alkaline building materials and controlled moisture conditions as causes for dry rot Serpula lacrymans growing only in houses
1985 - IRG/WP 1272
Dry rot Serpula lacrymans ( Fr.) S.F. Gray is commonly found in houses, though never with certainly in nature, like other wood destroying fungi which grow both indoors and outdoors. In investigating series of dry rot instances it was shown that this fungus is always found in covered places, close to a moisture source, the distance being from 0 a maximum of 600 cm. Owing to the dry rot has been abl...
J Bech-Andersen


A bioassay for appraising preservative protection of wood above ground
1978 - IRG/WP 2124
A bioassay, using the mold fungus Aspergillus niger, gave results that were correlated with amounts of pentachlorophenol and tributyltin oxide in pine sapwood treated with solutions ranging in strength from 0.016 or below to 5%. Limited bioassay estimates of penta in commercially treated millwork corresponded to estimates by lime ignition. The assay fungus exhibited somewhat greater tolerance of t...
T C Scheffer, L Gollob


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Multicomponent biocide systems protect wood from decay fungi, mold fungi, and termites for interior applications
2004 - IRG/WP 04-30333
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of proper moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under condit...
C A Clausen,V W Yang


Co-operative research project on L-joint testing. Sampling after 18 months exposure
1984 - IRG/WP 2233
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure (due 1 December 1983 for those L-joints exposed on schedule on 1 April 1983), and including tables on which to record the test results. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is therefore proposed that the next sampling, a...
J K Carey, A F Bravery


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Detection and estimation of Hylotrupes bajulus L. wood damages by ultrasonics
1990 - IRG/WP 2350
To evaluate the validity of the ultrasonic application in the detection and evaluation of wood damages produced by Hylotrupes bajulus L. larvae, some laboratory tests were made with small wood samples. The pulse through transmission method was used. The transit time of ultrasonic pulses in transversal sections, radial and tangential, of the samples was measured. The increment of the transit time o...
G Prieto


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


A bioassay to determine preservative retention in hardwoods and southern pines
1982 - IRG/WP 2183
In this paper the author discusses and suggests a new method of evaluating preservative retention in treated woods by means of bioassays. Twelve North American species were tested with different retention levels of pentachlorophenol (PCP) and copper/chrome/arsenic (CCA) preservatives. The results observed in this work show that among other fungi, Aspergillus niger responds to both preservatives, w...
J C Moreschi


A test method to simulate above-ground exposure
1978 - IRG/WP 2112
The simulated above-ground exposure technique described is worthy of consideration as a simple procedure to determine the relative decay resistance of preservative-treated wood exposed to a moderate decay hazard. The method may readily be modified to allow testing of other materials such as plywood by simply enlarging the slots cut in the modified feeder strips. The method by no means completely s...
J A Butcher


Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden


Previous Page | Next Page