IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1060 documents. Displaying 25 entries per page.


Laboratory evaluation of potential antisapstain treatments for Pinus radiata
1983 - IRG/WP 3237
Twelve formulations were tested in the laboratory using a 'mini' board test for effectiveness on Pinus radiata (D. Don) against sapstain, mould and decay fungi. Three formulations, sodium pentachlorophenoxide (NaPCP) plus borax, Haipen 50 WP, and Mitrol 375, are used commercially in New Zealand. Busan 1009 (0.5% product), IWD Product A (0.2% ai), IWD Product B (0.3% ai), Fennotox...
J A Drysdale


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


The effect of precolonisation of blocks with common pole resident fungi on subsequent biological control of Lentinus lepideus by Trichoderma spp
1989 - IRG/WP 1387
Results of previous field studies have indicated that the spread of Trichoderma throughout the groundline regions of the interiors of creosoted poles are adversely influenced by the presence of large populations of resident mould organisms. Failure of the control fungus to develop and colonize all of the decay susceptible groundline region means that sucessful control of decay is most unlikely. Th...
A Bruce, T L Highley


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Feasibility of using biological control agents to arrest and prevent colonization of Douglas fir and southern pine by decay fungi
1988 - IRG/WP 1345
The use of microfungi to control basidiomycetous decay has been evaluated in Europe for many years, where it has produced mixed results against Lentinus lepideus Fries, the fungus presumed to be the major cause of decay in Scots Pine poles. In the United States, remedial decay control has been largely chemical, with little use of alternative decay control strategies. Increasing restrictions on che...
J J Morrell, C M Sexton


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui


Invasion and colonisation of bamboo culm material by stain and decay fungi
2002 - IRG/WP 02-10453
Two distinct stages of the fungal infection of bamboo culms can be identified: entry into the culm itself (invasion) and further colonisation by spread within the culm wall tissue. This laboratory study aimed to characterise different invasion strategies of a variety of fungi. Well-known isolates of white- (Coriolus versicolor, Schizophyllum commune), brown- (Coniophora puteana, Gloeophyllum tra...
G Kleist, I Morris, R J Murphy


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka


A survey of the incidence of decay in copper-chrome-arsenate treated trellis support posts used in horticulture in New Zealand
1984 - IRG/WP 1225
Copper-chrom-arsenate treated softwood posts used as trellis support structures in 5 major horticultural districts of New Zealand were systematically examined for presence of decay. Principal crops on properties examined were grapes and kiwifruit; a minority of properties grew hops, boysenberries, and dwarf apples. Occurrence and severity of decay were variable within specific age classes of posts...
M E Hedley, J A Drysdale


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Growth of selected wood decay fungi on various agar-supplemented media
2003 - IRG/WP 03-10456
The growth rates of a selection of wood decay fungi (brown and white rots) on various agar-supplemented media have been determined and compared. The agar media investigated were Malt extract agar (MEA), Potato dextrose agar (PDA), YMPG agar (yeast extract, malt extract, bacto-peptone, glucose, asparagine and thiamine), YMPG agar (without amino acids) and Beech wood powder agar (BWA). The tested wo...
S A Amartey, M Humar, F Pohleven


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Previous Page | Next Page