Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


Questionnaire: Facility for accelerated stake tests in unsterile soil
1981 - IRG/WP 2166
An acceptable name for this type of test facility has not yet been devised, but it has previously been referred to as a FUNGUS CELLAR or as a TROPICAL DECAY HOUSE. The attached pamphlet (What's New in Forest Research No.65) describes in broad terms the facility used for this purpose at FRI in New Zealand. Over the last two or three years several laboratories and commercial firms have inst...
J A Butcher


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Documentation on Merulius (Serpula) lacrimans (Wulf.) Fr. according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1972 - IRG/WP 108
J Segmüller, O Wälchli


Development of decay in untreated, second-growth Douglas-Fir using two exposure techniques in North Queensland
1997 - IRG/WP 97-20110
The results of two exposure techniques for evaluating the development of wood decay in untreated, mill-run lumber from second-growth Douglas-fir containing both sapwood and heartwood are presented. Nominal 50 mm by 100 mm by 2.5 m (2 in. by 4 in. by 8 ft) lumber, No 2 and better, was obtained from a production run in a mill that was processing second growth, Coastal Douglas-fir in western Oregon, ...
J Norton, S Kleinschmidt, R C De Groot, D Crawford


Resistance of painted pine sapwood to mould fungi. Part 1. The effect of waterborne paints and fungicides on mould growth
1997 - IRG/WP 97-10233
The efficacy of different fungicides in acrylate and alkyd paints to protect pine sapwood against mould fungi was studied. The acrylate and alkyd paint systems with and without a preservative dipping treatment prior to painting were also used. Differences in the efficacy of the fungicides to protect the paint film were found. The paint films with isothiazolon and IBPC were resistant against mould ...
H Viitanen, P Ahola


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....
H M Barnes, T L Amburgey, R W Landers


A simple non-destructive means of testing poles in situ
1982 - IRG/WP 2167
Anonymous


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


The dry rot and other fungi in houses. Part 4
1995 - IRG/WP 95-10124
J Bech-Andersen


Ibuprofen inhibits in vitro growth of brown-rot fungi
1996 - IRG/WP 96-10160
Ibuprofen, a phenyl propionic acid derivative (2-(4-isobutylphenyl)propionic acid) inhibited growth in vitro of 17 brown-rot fungi at a concentration of 100 µg/mL, while exhibiting no growth inhibition for 8 white-rot fungi at the same concentration. Propionic acid did not inhibit fungal growth in vitro. Morphological changes were noted in fungi that were able to grow in the presence of ibuprofen...
C A Clausen


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


Biodeterioration and preservation of rubberwood (Hevea brasiliensis)
1994 - IRG/WP 94-10084
Plantation-grown rubber trees (Hevea brasiliensis) in the tropics is fast emerging as a significant provider of quality hardwood for a variety of non-structural products, as the aesthetics of the timber is its creamed colour resembling perhaps the priced but depleting Ramin wood or even American beechwood. However rubberwood logs and sawn materials are highly sensitive to sapstain, fungal decay an...
L T Hong, A H H Wong


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Investigations on the life cycle and nutrition of Criocephalus rusticus L
1974 - IRG/WP 127
The longhorn beetle Criocephalus rusticus L or Arhopalus rusticus (L) is widely distributed in Europe and Asia. It attacks softwoods. The primary host trees are pines, ie freshly felled, unbarked logs, dying standing trees and stumps. After feeding under the bark the larvae enter the sapwood and also the heartwood. Timber to be used for building purposes may be rendered useless by their tunnelling...
H Kühne


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel