Antifungal activity and synergistic effect of cinnamaldehyde combined with antioxidants against wood decay fungi
2007 - IRG/WP 07-30445
The objective of this study was to investigate the antifungal activity and synergistic effect of cinnamaldehyde combined with antioxidants against wood decay fungi. Five antioxidants, propyl gallate, octyl gallate, quercetin, eugenol and catechin were tested against various wood decay fungi. Octyl gallate and eugenol were found to be the only two antioxidants processed antifungal activities. IC50 ...
Fu-Lan Hsu, Tsair-Bor Yen, Hui- Ting Chang, Shang-Tzen Chang


Biodeterioration of cultural monuments in the Republic of Macedonia
2008 - IRG/WP 08-10640
Research on the biodeterioration of the cultural heritage in the Republic of Macedonia was conducted from 2004 to 2006, one month per year. The expertise was focused on the biodeterioration caused by wood-inhabiting fungi and moulds. A total of 38 cultural monuments, including 37 monasteries and churches and one fortress, were inspected in the areas of the towns of Skopje, Ohrid, Demir Hisar, Deba...
I Irbe, M Karadelev, I Andersone, B Andersons


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Wood decay fungi from New Zealand leaky buildings – PCR identification (Part 2) and aerial spore trapping
2008 - IRG/WP 08-10649
Prior to this study, it was not know which species of decay fungi caused decay in New Zealand leaky buildings. Use of molecular biology methodology, polymerase chain reaction (PCR), and subsequent DNA sequencing, as well as classical mycological techniques based on morphology, has enabled identification of decay fungi and has provided insight into their relative importance based on isolation frequ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Efficacy of Neem (Azadirachta indica) Leaves Against Wood Decay Fungi
2008 - IRG/WP 08-30450
Many plant-derived substances have fungitoxic, pecticidal and insecticidal ability. Neem leaves are very popular in this respect since the ancient time. The present study is to investigate the fungitoxic activities of neem leaves extractives against wood decay fungi. Three different solvents, i.e. acetone, methyl alcohol, ethyl alcohol, were used to isolate the extract of neem leaves. The extracti...
A Humayan Kabir, M A Rahman, M Firoz Alam


Antifungal activity of different molecular weights of a biopolymer chitosan against wood decay fungi
2008 - IRG/WP 08-30456
In recent years chitosan has been investigated as a natural polymer for wood preservation against fungal decay. From an environmental point of view, chitosan seems to possess a potential approaches as wood protecting agent. In this study, three different molecular weights of chitosan compounds (with approximately the same degree of deacetylation 83 ± 2 %) were evaluated as in vitro and in vivo as...
A S O Mohareb, M E I Badawy


Molecular Methods: a Reliable Tool for the Identification of Wood Decay Fungi in Construction Timber
2008 - IRG/WP 08-20386
In the present study, we tested the practical value of several DNA-based methods to identify at the species level the most common wood-decaying fungi infecting buildings. We successfully extracted and amplified fungal DNA from pure cultures of twelve species of wood-inhabiting fungi, from oak and pine wood infected in laboratory with known strains, and from unknown field samples of wood collected ...
M Maître, M Kutnik, I Le Bayon, L Harvengt


Investigation into the antifungal properties of herbal remedies for potential use in the wood preservation industry
2008 - IRG/WP 08-30462
The efficacy of herbal remedies as potential antifungal agents was evaluated against two sapstain and three decay fungi. Sapstain fungi included Sphaeropsis sapinea, and Leptographium procerum, and decay fungi were Oligoporus placenta, Coniophora puteana, and Schizophyllum commune. Out of six herbal remedies tested, three showed moderate to high antifungal activity. Caprylic acid had high antif...
D O’Callahan


Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


Natural durability and anatomical features of teak (Tectona grandis) from plantations in Costa Rica
2008 - IRG/WP 08-10671
Teak (Tectona grandis) possesses superior mechanical properties and durability and is thus frequently used as an alternative to impregnated timber in Europe. Demand on teak has resulted in severe exploitation of the tropical teak forests in recent decades, but today the imported timber originates mainly from plantations and is certificated according to the Forest Stewardship Council (FSC) policy. ...
U J Wolfsmayr, N Terziev, G Daniel


Aislamiento, identificación y evaluación enzimática de hongos de pudrición de madera de la Región de los Lagos
2008 - IRG/WP 08-10680
So far, systematic investigations have not been developed to determine the fungal diversity associated with wood in Chile. In addition, little is known about the mycoflora capabilities or their enzymatic processes in biotechnology although different research has hinted at the great potential of these microorganisms in various industrial processes. The aim of this work is to isolate, identify and e...
R Ortiz, J Navarrete, C Oviedo, R Blanchette


A Comprehensive Review of Copper as a Biocide, with a Focus on Micronized Copper
2008 - IRG/WP 08-30486
This paper reviews the wood preservative biocide active ingredient copper and delvers into new and previously unpublished data regarding the new micronized formulations which are now in vogue and widespread use in N. America in all residential treated lumber markets. Included in this review is the overall discussion of copper containing formulations used for pressure treated wood used over the las...
M H Freeman, C R McIntyre


Effect of a biological treatment on below ground decay of Douglas-fir pole sections
2008 - IRG/WP 08-40433
The use of exogenous sugars to accelerate microbial growth and eventually limit available oxygen in soil surrounding wood in soil contact was investigated on untreated Douglas-fir poles exposed over a 3 year period in Western Oregon. Isolation frequencies differed markedly between treated and untreated poles and the treatment did appear to shift the frequency of some basidiomycetes. The treatment ...
C Freitag and J J Morrell


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Effect of juglone from Juglans mandshurica bark activity of wood decay fungi
2009 - IRG/WP 09-30502
Juglone was extracted from Juglans mandshurica bark via vacuum-assisted steam stripping. The extract was characterized by Fourier Transform Infrared Spectroscopy (FTIR), 1H Nuclear Magnetic Resonance (NMR) and Gas chromatography/mass spectrometry (GC-MS). The extraction process was easy to perform and produced excellent yields (0.22 g juglone/100 g of bark) of a high purity extract (96.42% juglone...
Dongmei Yang, Shuangyue Li, Shujun Li, Wenqiang Su, Yan Jin, Molong Sun


Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril


Synthesis of a rosin amide and its resistance to wood decay fungi
2009 - IRG/WP 09-30517
Rosin was reacted with diethyltriamine (DETA) after being modified by acryl acid with the weight ratio of 4.5:1 and a rosin amide (RA) derivative was produced at the conditions as follows: modified rosin and DETA mole ratio of 1:3.5, dimethylbenzene as water carrying agent, reaction temperature of 160-180°C, and reaction time of 8h. The chemical structure of the product as RA was identified by F...
Shuangyue Li, Shujun Li, Jing Wang


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Assessment of decay risk of airborne wood-decay fungi
2012 - IRG/WP 12-10787
The decay risk of airborne wood-decay fungi was investigated by using an air sampler. Japanese cedar disks measuring about 8 cm in diameter and 3 mm in thickness with moisture content at about 100 % were placed in a “BIOSAMP” air sampler and exposed to 1000 liters of air. Air sampling was carried out from June to September at the same sampling site in Tsukuba, Japan. The exposed disks were the...
I Momohara, Y Ota, K Sotome, T Nishimura


The resistance of thermo-oil modified wood against decay and mould fungi
2009 - IRG/WP 09-40448
Thermally modified wood in comparison to natural wood demonstrates some advantageous functional properties like decreased hygroscopicity, higher dimensional stability. It also has increased durability and improved resistance to fungal decay. However thermal modification of wood may lead to reduced strength properties what may limit the use of wood in mechanically beared constructions. The changes ...
A Fojutowski, A Kropacz, A Noskowiak


The invasion channels of damage fungi in bamboo lumber
2010 - IRG/WP 10-10712
The micro-agents on bamboo lumber damage are mould, stain, and decay fungi. This research is about invasion channels of bamboo lumber damage fungi by scanning electron microscope (SEM). The results showed that the conidia of mould were only accumulated on the surface of bamboo and no hyphae detected in bamboo vascular bundle, and hyphae of stain penetrated into bamboo and grew in metaxylem vessel...
Xingxia Ma, Mingliang Jiang, Daochun Qin