IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1489 documents. Displaying 25 entries per page.


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


The effects of copper proximity on oxalate production in Fibroporia radiculosa
2014 - IRG/WP 14-10823
Copper remains a key component used in wood preservatives available today. However, the observed tolerance of several critical wood rotting organisms continues to be problematic. Tolerance to copper has been linked to the production and accumulation of oxalate, which precipitates copper into insoluble copper-oxalate crystals, thus inactivating copper ions. The purpose of this study was to assess d...
K M Jenkins, C A Clausen, F Green III


Molecular characterization and biodiversity of wood-decaying fungi in French Guiana
2014 - IRG/WP 14-10825
Fungi from tropical regions are currently under-represented in the classification system. Indeed, difficult access to tropical forests and irregular occurrence carpophores make it complicated to study fungus species in such environments, unlike in European zones where fungal diversity and taxonomy are better known. The purpose of this work was to enhance classification by integrating new data that...
A Zaremski, L Gastonguay, C Zaremski, J Beauchene


Protein extraction from wood decay fungus Postia placenta
2014 - IRG/WP 14-10827
Wood decay fungi (often distinguished as white rot and brown rot) belonging to the basidiomycetes, are common inhabitants of forest litter, where they play an important role in carbon cycling. Brown rot fungi are perhaps the most important organism involved in the degradation of wood products, and of considerable economic importance. Brown rotted wood loses strength very early because of the rapid...
A Pilgård, P Arnold, K Richter


Identification of soft-rot fungi existed in the samples from the galley excavated at Yenikapi
2014 - IRG/WP 14-10833
The shipwrecks of the Middle Byzantine period were excavated during the construction of the Marmaray railway and metro station in Yenikapı between 2004 and 2012. This has become the largest investigations because of the size and the number of the shipwrecks and its associated artifacts. In the previous report, the electron micrographs of the samples revealed that a wide range in the degree of...
T Wada, C Köse, K Igarashi


Microbial Community Analysis of Naturally Durable Wood in an Above Ground Field Test
2014 - IRG/WP 14-10826
This paper presents preliminary results of an above ground field test wherein eight naturally durable wood species were exposed concurrently at two sites in North America. Surface samples were taken at regular intervals from non-durable controls and compared to their more durable counterparts. Terminal Restriction Fragment Length Polymorphism was performed to characterize the microbial (bacteria, ...
G T Kirker, S V Diehl, P K Lebow


The Chelator Mediated Fenton System in the Brown Rot Fungi: Details of the Mechanism, and Reasons Why it has Been Ineffective as a Biomimetic Treatment in some Biomass Applications – a Review
2014 - IRG/WP 14-10828
The chelator-mediated Fenton (CMF) reaction requires the action of two types of chelating compounds. The first chelator, oxalate, solubilizes and then sequesters iron, and the second chelator reduces iron. Iron reduction must be controlled near the fungal hyphae to prevent damaging Fenton chemistry from occurring in that location. Similarly, iron reduction must be promoted within the wood/plant ce...
B S Goodell, M Nakamura, J Jellison


Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene


Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack). In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram


A screening of factors that might influence the result of laboratory decay tests
2014 - IRG/WP 14-20548
Laboratory fungal decay tests provide important tools for performance testing of wood materials. But they are also hampered with some uncertainties regarding reproducibility. In addition to variation between fungal species and strains the test conditions are also believed to have some influence. The aim of this study was to screen the effect of a selection of test parameters that might influence t...
E Larnøy, G Alfredsen, A Treu, S Kolstad


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers


Effectiveness of Copper Indicators in Treated Wood Exposed to Copper Tolerant Fungi
2014 - IRG/WP 14-20554
Wood treated with a copper based wood preservative will typically turn a green color. While the depth of copper penetration can be readily discerned from the green color of the copper it is standard practice in research and commercial treating plants to make use of a color reagent such as Chrome Azurol S, Rubeanic acid or PAN indicator to reveal the penetration more clearly. When copper treat...
L Jin, K Brown, A Zahora, K Archer


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


The resistance of Accoya® and Tricoya® to attack by wood-destroying fungi and termites
2014 - IRG/WP 14-40658
The resistance of high acetyl WPG solid timber (Accoya®) and medium density fibreboard (Tricoya®) to attack by wood-destroying fungi and termites was investigated under both laboratory and field conditions. Laboratory decay studies were conducted in Australia and New Zealand. Field studies were conducted in Australia, Japan, New Zealand, Thailand and USA. The results of the laboratory and field ...
J Alexander, J Hague, F Bongers, Y Imamura, M Roberts


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


Comparison of untreated plywood and untreated LVL in a field trial against Coptotermes acinaciformis and in laboratory trials against Tyromyces palustris and Coniophora puteana
2014 - IRG/WP 14-40671
In Australasia, efficacy data obtained on plywood is generally acceptable for laminated veneer lumber (LVL) and vice versa. This is particularly the case with glueline treatment approvals. The rationale is that the two wood products have predominately the same basic structure with the key difference being orientation of the veneer. LVL typically has all veneers in parallel while plywood typical...
A Siraa, K Day, S Millward, P Lobb


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


Previous Page | Next Page