Influence of ring width and wood density on durability of oak heartwood
2008 - IRG/WP 08-10639
Oak (Quercus sp.) is considered as one of the most durable European wood species. The most important factor influencing oak durability was extractive content. In our work, we were interested in if oak-wood durability is affected by ring-width and related density. Therefore, oak heartwood specimens made of boards with different ring widths were exposed to five different fungal species Daedelea quer...
M Humar, P Oven, F Pohleven


Biodeterioration of cultural monuments in the Republic of Macedonia
2008 - IRG/WP 08-10640
Research on the biodeterioration of the cultural heritage in the Republic of Macedonia was conducted from 2004 to 2006, one month per year. The expertise was focused on the biodeterioration caused by wood-inhabiting fungi and moulds. A total of 38 cultural monuments, including 37 monasteries and churches and one fortress, were inspected in the areas of the towns of Skopje, Ohrid, Demir Hisar, Deba...
I Irbe, M Karadelev, I Andersone, B Andersons


Decay Resistance Properties of Hemicellulose-Extracted Oriented Strand Board
2008 - IRG/WP 08-10644
There is increasing interest in using cellulosic biomass as the basis for a renewable source of energy. Although the traditional focus has been on cellulose, researchers are also exploring the possibility of using hemicelluloses because they can be removed with hot water leaving the wood product intact for other applications. However, there is concern that removing hemicelluloses from the precur...
C Howell, J Paredes, S Shaler, J Jellison


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Evaluation of natural durability of solid wood and mixed heartwood-sapwood Cypress (Cupressus sempervirens L.) plywood against Basidiomycete fungi
2008 - IRG/WP 08-10645
The aim of this research was to study the response of mixed plywoods composed of durable heartwood and non-durable sapwood to fungal attack. For this purpose, the species of Cupressus sempervirens (cypress) was chosen for its well-known durable heartwood. The evaluation of durability of plywood panels against fungi was done according to ENV 12038 and the fungi used were Coriolus versicolor (CV) an...
F Faraji, M F Thévenon, N Lemenager, B Thibaut


Performance of sintered glass screening as a potential physical barrier against subterranean termites in the laboratory and after 4 years of field test
2008 - IRG/WP 08-10646
This paper describes the performance of sintered glass screenings as a potential physical barrier against the subterranean termites, Coptotermes acinaciformis and Mastotermes darwiniensis in the laboratory and after four years of field testing in active above-ground mound colonies of Coptotermes lacteus. The laboratory results suggest that sintered glass is a viable control option against Copto...
J R J French, B M Ahmed (Shiday)


Wood decay fungi from New Zealand leaky buildings – PCR identification (Part 2) and aerial spore trapping
2008 - IRG/WP 08-10649
Prior to this study, it was not know which species of decay fungi caused decay in New Zealand leaky buildings. Use of molecular biology methodology, polymerase chain reaction (PCR), and subsequent DNA sequencing, as well as classical mycological techniques based on morphology, has enabled identification of decay fungi and has provided insight into their relative importance based on isolation frequ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Characterization of protein patterns from decayed wood of loblolly pine (Pinus taeda L.) by proteomic analysis
2008 - IRG/WP 08-10654
The primary biotic decomposers of wood belong to the basidiomycetes. The members of this group can attack and biodegrade both wood in the forest and in service. By the time wood decay is visible, there has already been a significant loss of strength. The identification of basidiomycetes and other organisms on wood only tell us what is present, not what is actively decaying the wood. When organisms...
Young-Min Kang, L Prewitt, S Diehl


Decay resistance of propionylated Iranian beech against the white rot fungus Tramets versicolor
2008 - IRG/WP 08-30449
In this study, the decay resistance of propionylated beech was investigated against the white rot fungus Trametes versicolor. Iranian beech (Fagus orientalis) was modified with propionic anhydride at different temperatures, concentrations and times without using any catalyst. Different weight percentage gains (WPGs) were obtained under different conditions. The decay resistance of the esterifed wo...
M R M Farahani, S M Hosseini


Efficacy of Neem (Azadirachta indica) Leaves Against Wood Decay Fungi
2008 - IRG/WP 08-30450
Many plant-derived substances have fungitoxic, pecticidal and insecticidal ability. Neem leaves are very popular in this respect since the ancient time. The present study is to investigate the fungitoxic activities of neem leaves extractives against wood decay fungi. Three different solvents, i.e. acetone, methyl alcohol, ethyl alcohol, were used to isolate the extract of neem leaves. The extracti...
A Humayan Kabir, M A Rahman, M Firoz Alam


Utilizing Cypress to improve the decay and termite resistance of OSB panels
2008 - IRG/WP 08-10658
OSB panels were manufactured with mixture of pine and cypress heartwood and lignin and tannin based resins in order to propose an eco-friendly wood composite. The resistance of OSB panels was tested against Reticulitermes santonensis according to the EN 118 and EN 117 standards and field tests methods. OSB made from cypress showed more resistance against the tested termite, the resistance decrease...
N Amusant, O Arnould, A Depres, R H Mansouris, T Pizzi, C Baudassé


In vitro evaluation of an integrated approach using Trichoderma harzianum and chitosan for the control of sapstain
2008 - IRG/WP 08-10659
In vitro assays were undertaken to evaluate the control of two sapstain fungi, Leptographium procerum and Sphaeropsis sapinea by a combination of chitosan or chitosan oligomer (CODP-14) and a naturally mutated strain of Trichoderma harzianum. Spore germination and hyphal growth of the test fungi were assessed on media amended with chitosan or chitosan oligomer with and without T. harzianum using ...
C Chittenden, T Singh


Antifungal activity of different molecular weights of a biopolymer chitosan against wood decay fungi
2008 - IRG/WP 08-30456
In recent years chitosan has been investigated as a natural polymer for wood preservation against fungal decay. From an environmental point of view, chitosan seems to possess a potential approaches as wood protecting agent. In this study, three different molecular weights of chitosan compounds (with approximately the same degree of deacetylation 83 ± 2 %) were evaluated as in vitro and in vivo as...
A S O Mohareb, M E I Badawy


Microbial Community Analysis Using Terminal Restriction Fragment Length Polymorphism (T-RFLP) Analysis: Field Study Results
2008 - IRG/WP 08-20377
The effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on the fungal community in southern yellow pine (SYP) were assessed using terminal restriction fragment length polymorphism (T-RFLP) analysis. Field stakes treated with 0.25% and 0.37% ammoniacal copper quat (ACQ-C), 0.1 and 0.25% CTN, and 0.1 and 0.25% CTN combined with 2% BHT were installed with untreated controls in field s...
G T Kirker, S V Diehl, M L Prewitt, W J Diehl


A comparison of rates of decay and loss in stiffness of radiata pine and Douglas fir framing lumber
2008 - IRG/WP 08-20378
Stiffness loss with time was recorded for untreated radiata pine and Douglas fir framing size lumber and preservative treated radiata pine which dad been pre-inoculated with Oligoporus placenta, a brown rot decay fungus isolated from decaying untreated radiata pine framing. Between stiffness measurements, samples were contained in a plastic tank located outside at ambient temperature. Index of Con...
M Hedley, D Page, J van der Waals


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Field Liners as physical barriers to prevent wooden utility pole decay in soil: An accelerated field simulation trial
2008 - IRG/WP 08-20384
Field Liners (FL’s), plastic sleeves used to protect in-ground wooden poles from fungal and termite damage, have been tested before as physical barriers to prevent contact between soil and wood and to retain wood preservative treatment. These earlier studies concentrated mostly on creosote preserved poles and early generation FL’s which were cumbersome in their application. The newer generatio...
A R Howgrave-Graham, L J Cookson, T Hale


Molecular Methods: a Reliable Tool for the Identification of Wood Decay Fungi in Construction Timber
2008 - IRG/WP 08-20386
In the present study, we tested the practical value of several DNA-based methods to identify at the species level the most common wood-decaying fungi infecting buildings. We successfully extracted and amplified fungal DNA from pure cultures of twelve species of wood-inhabiting fungi, from oak and pine wood infected in laboratory with known strains, and from unknown field samples of wood collected ...
M Maître, M Kutnik, I Le Bayon, L Harvengt


Investigation into the antifungal properties of herbal remedies for potential use in the wood preservation industry
2008 - IRG/WP 08-30462
The efficacy of herbal remedies as potential antifungal agents was evaluated against two sapstain and three decay fungi. Sapstain fungi included Sphaeropsis sapinea, and Leptographium procerum, and decay fungi were Oligoporus placenta, Coniophora puteana, and Schizophyllum commune. Out of six herbal remedies tested, three showed moderate to high antifungal activity. Caprylic acid had high antif...
D O’Callahan


Laboratory evaluation of four benzoylphenylureas against two species of Reticulitermes Holmgren, 1913 (Isoptera: Rhinotermitidae) from Southwest Europe
2008 - IRG/WP 08-30472
The use of benzoylphenylureas in baits for the control of termite pest is currently increasing. The chemical compounds used have been tested mainly with American termites. The effectivity against non-American termite species must be analyzed because the worldwide use of those compounds. In this paper four benzoylphenylureas (hexaflumuron, diflubenzuron, triflumuron and noviflumuron) have been test...
M Gaju-Ricart, M Urbano-Luque, R Molero-Baltanás, C Patiño-Martínez, C Bach de Roca


Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


Laboratory Evaluation of Flurox, a Chitin Synthesis Inhibitor, as a Bait Toxicant Against Microcerotermes diversus (Silvestri ) (Isoptera: Termitidae)
2008 - IRG/WP 08-30477
Microcerotermes diversus (Silvestri) is the most economically destructive termite in structures in southwest, Iran . One sustainable control strategy that usually help in reducing the subterranean termite damage in buildings , which is safe to the user and the environment is the use of IGRs in a suitable bait matrix. In the laboratory assays described here, the delayed toxicity of Flurox (a Chitin...
B Habibpour


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III