Chelator production and cellobiose dehydrogenase activity of wood inhabiting fungi
2000 - IRG/WP 00-10363
Multiple components have been postulated to be involved in the Fenton-based biological degradation of wood by brown rot fungi. Chelators have been implicated in essential iron reduction steps. Cellobiose dehydrogenase activity and quinone reducing activity have also been implicated in brown rot biodegradation. When biochelator production by three white rot fungi, three brown rot fungi and three wo...
Weihong Qi, J Jellison


Determination of boron levels in solution and in treated wood
1994 - IRG/WP 94-20041
Four methods of measuring boron levels in solutions were investigated. The methods compared included the azomethine-H method which is commonly used in soils and plant tissues, the methods outlined in the Australian Standard AS 1605 (1974) and in Wilson (1958), and the atomic absorption spectrophotometry method. Defect-free radiata pine (Pinus radiata D. Don) sapwood and wood flakes were treated to...
F J Romero, P Vinden, P Kho


Siderophore production by Trichoderma spp. and its importance in the biological control of wood decay fungi
1994 - IRG/WP 94-10070
Competition for iron as well as other micro-nutrients is an essential component of the microbial ecology of many ecosystems. A wide range of micro-organisms including fungi and bacteria have been shown to increase their ability to efficiently capture iron through the production of specialised iron chelating compounds called siderophores. Since iron is in low supply in wood and has been implicated ...
U Srinivasan, A Bruce, T L Highley


Patterns of decay in CCA-treated horticultural post populations - A fungus cellar simulation
1986 - IRG/WP 1286
The distribution of decayed posts in 10-, 14-, and 18-year-old vineyards supported a hypothesis to explain variability in intensity of decay found among posts in New Zealand horticultural properties. The development of decay patterns between samples in a simulated vineyard plot established in the Forest Research Institute fungus cellar gave additional support to the hypothesis that decay within la...
M E Hedley


Premature failure of CCA treated vineyard posts from brown rot
1993 - IRG/WP 93-10016
A survey of CCA (AWPA Type C) treated posts used as grape vine trellis supports, to determine the extent and type of decay was carried out at a terraced vineyard in the Hawkes Bay region of the North Island of New Zealand. Of 357 posts examined out of a total of 970 in the vineyard, 47% had moderate to severe decay or had failed, 20% had established decay, 10% had a trace of decay and 23% had no s...
R N Wakeling, A P Singh


Biological control of decay
1975 - IRG/WP 135
One approach to the biological control of decay in standing poles, live trees or seedlings is with microbial immunising commensals or IC.·These are microorganisms able to grow in the wood without damaging it and as a result of such growth to protect against certain types of decay. Scytalidium and Trichoderma spp have been tested in the field. The latter species have shown an establishment rate in...
J Ricard


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Properties-enhanced albizzia particleboards by incorporating fungicide and insecticide in the glue
1994 - IRG/WP 94-30060
Preservative-treated particleboards were prepared by using tropical fast-growing albizzia and adding fungicides and insecticides to the adhesive-glue. the physical and biological properties of these boards were evaluated. No significant reduction in bending or internal-bond strength due to incorporation of the chemicals was detected. Treated particleboards effectively resisted attack by Coptoterme...
B Subiyanto, S Yusuf, Y Imamura, S Fushiki, T Saito, T Katuzawa


Decay in window joinery in Sweden
1977 - IRG/WP 390
Systematic investigations of decay in window joinery in Sweden have not been undertaken until very recently. One might guess that one of the reasons for the minor interest is that this type of joinery did not rot strikingly faster than people expected. In the last 10-15 years, however, house owners, tenantowners, building societies and others have repeatedly argued that windows do rot more than in...
B Henningsson


Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven


The remaining concentration of inorganic wood preservative components in EN 252 stakes after ground contact
2000 - IRG/WP 00-50159
In order to determine the biological efficiency and the remaining concentration of different inorganic and organic active ingredients during service, EN 252 specimens were impregnated with 3 copper based wood preservatives. The stakes were installed in the test field of the DESOWAG GmbH, Rheinberg, for at least 7 years. At the end of the field test some of these stakes were divided into 10 uniform...
E Melcher, H-W Wegen


Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Alkaline building materials and controlled moisture conditions as causes for dry rot Serpula lacrymans growing only in houses
1985 - IRG/WP 1272
Dry rot Serpula lacrymans ( Fr.) S.F. Gray is commonly found in houses, though never with certainly in nature, like other wood destroying fungi which grow both indoors and outdoors. In investigating series of dry rot instances it was shown that this fungus is always found in covered places, close to a moisture source, the distance being from 0 a maximum of 600 cm. Owing to the dry rot has been abl...
J Bech-Andersen


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Susceptibility of antisapstain fungicides to rain wash-off
1994 - IRG/WP 94-30046
Results of trials using miniature timber packets and simulated rain wash-off are described. Six fungicidal actives in five commercial antisapstain formulations were involved, and a clear influence of rainfall timing after antisapstain treatment was demonstrated. Differences between actives and formulations were most marked where water-spray was applied in the first hour after treatment, though eve...
R N Wakeling, D J Cross, D R Eden, P N Maynard


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Multicomponent biocide systems protect wood from decay fungi, mold fungi, and termites for interior applications
2004 - IRG/WP 04-30333
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of proper moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under condit...
C A Clausen,V W Yang


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


The identification of organic compounds in wood using thermal desorption GC-MS - possibilities and limitations
2001 - IRG/WP 01-20224
There is a clear need for the analytical characterisation and identification of organic compounds and their derivatives in different phases especially in timber. In this context the paper describes a rapid and powerful gas chromatographic method for the determination of insecticides, biocides and "other" organic substances in treated and/or modified wood. The main advantage of this procedure is th...
P Jüngel, E Melcher


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...