Fungicidal properties of boron containing preservative Borosol 9
2004 - IRG/WP 04-30348
The fungicidal properties of new boron containing wood preservative Borosol 9 is described in this paper. These properties were of particular interest as this new boron containing preservative, exhibit very good performance against wood damaging insects. But because the tested boron formulation contain also nitrogen compounds, we wanted to verify if nitrogen as a nutrient could promote...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan


Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin


Analysis of volatile emissions as an aid in the diagnosis of dry rot
1992 - IRG/WP 92-2393
The dry rot fungus, Serpula lacrymans was grown in pure culture on malt extract and on sapwood of pine. The volatile compounds emitted from the cultures were determined by diffusion sampling on tubes filled with Tenax TA, thermal desorption and gas-chromatography-mass-spectrometry in order to find markers for attack of the fungus....
J Bjurman, J Kristensson


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Investigations on the life cycle and nutrition of Criocephalus rusticus L
1974 - IRG/WP 127
The longhorn beetle Criocephalus rusticus L or Arhopalus rusticus (L) is widely distributed in Europe and Asia. It attacks softwoods. The primary host trees are pines, ie freshly felled, unbarked logs, dying standing trees and stumps. After feeding under the bark the larvae enter the sapwood and also the heartwood. Timber to be used for building purposes may be rendered useless by their tunnelling...
H Kühne


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


The leachability and specificity of the biological protection of timber using Scytalidium sp. and Trichoderma spp
1986 - IRG/WP 1302
The results of field experiments, using biological control against internal decay of creosoted poles, are briefly reviewed and the evidence concerning the leachability of the antibiotics produced by these species is presented. A pure culture miniblock decay test on biological control treated pine sapwood is described and the results compared to previously published data. The protection against Len...
P I Morris, N A Summers, D J Dickinson


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson


Monographic information on Serpula incrassata (Berk. and Curt.) Donk
1980 - IRG/WP 1128
J G Palmer, W E Eslyn


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


First draft of a monographic card for Gloeophyllum abietinum (Bull. ex Fr.) Karst
1973 - IRG/WP 116
T Hof


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Defining fungal decay types - Final proposal
1988 - IRG/WP 1355
The term soft rot is proposed for all forms of decay caused by Ascomycetes and non-basidiomyceteous Fungi imperfecti. The terms brown rot and white rot should be used only for decay caused by Basidiomycetes. Brown rot is characterized by extensive depolymerization of the cellulose and limited lignin degradation. White rot is characterised by significant degradation of the lignin component in wood....
T Nilsson


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 313 E
H Alliot


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen