IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3490 documents. Displaying 25 entries per page.


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Fungal and bacterial attack of CCA-treated Pinus radiata timbers from a water-cooling tower
1991 - IRG/WP 1488
Transmission electron microscopy of decaying CCA-treated Pinus radiata timbers from an industrial water cooling tower showed presence of a thick biofilm covering some areas of the wood. The biofilm contained various morphologically distinct forms of microorganisms embedded in a slime. The study provided evidence of the activity of soft rot fungi and tunnelling and erosion bacteria in wood cells. T...
A P Singh, M E Hedley, D R Page, C S Han, K Atisongkroh


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Third update and first report
1996 - IRG/WP 96-10174
At the 24th annual meeting of IRG in Orlando, USA, in May 1993 an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives, copper-chrome-arsenic (CCA) and copper naphthenate (Cu-Na) against the subterran...
J R J French


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker


Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland


Evaluation of new creosote formulations after extended exposures in fungal cellar tests and field plot tests
2000 - IRG/WP 00-30228
Although creosote, or coal tar creosote, has been the choice of preservative treatment for the railroad industry since the 1920s, exuding or "bleeding" on the surface of creosote-treated products has been one incentive for further enhancements in creosote production and utility (Crawford et al., 2000). To minimize this exuding problem, laboratories such as Koppers Industries Inc., USA, and Commonw...
D M Crawford, P K Lebow, R C De Groot


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli


The Third Annual Report of the International Research Group on Wood Preservation 1971-1972
1972 - IRG/WP 511
IRG Secretariat


The Fourteenth Report of the Internatinal Research Group on Wood Preservation 1984-1985
1985 - IRG/WP 5218
R Cockcroft


Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez


Insects in dry wood (other than termites)
1977 - IRG/WP 153
S Cymorek


Progress towards controlling soft rot of treated hardwood poles in Australia
1977 - IRG/WP 289
H Greaves


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis


The Seventh Annual Report of the International Research Group on Wood Preservation 1975-1976
1976 - IRG/WP 551
IRG Secretariat


Programme section 3, Wood protecting chemicals
1997 - IRG/WP 97-30159
IRG Secretariat


Effect of medium-term degradation of beech wood by erosive (Phanerochaete chrysosporium) and lignin-selective (Ceriporiopsis subvermispora) strains of white rot fungi on its selected physical properties
2004 - IRG/WP 04-40292
At the Faculty of Wood Sciences and Technology a fungal delignification of normal and tension beech wood by erosive and lignin-selective strains white-rot fungi has been studied. The pre-treatment of both kind of wood samples was accompanied by partial delignification and apparent changes of their physical properties influencing the polar liquids penetration....
R Solár, S Kurjatko, M Mamonová, J Hudec


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Protocol for evaluation and approving new wood preservative
1985 - IRG/WP 2159
M E Hedley, J A Butcher


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt


Insect resistance of preservative treated tropical plywood against Lyctus
1990 - IRG/WP 1453
Seven plywood types composed of tropical wood species, vulnerable to Lyctus, were treated with various commercial water-borne and oil-borne preservatives. A wide range of preservative retentions was obtained by treating boards with dip treatment, steeping, double-vacuum and vacuum-pressure impregnations. Selected samples were subsequently tested for their insect resistance against Lyctus africanus...
J Van Acker, M Stevens, M Pallaske


Previous Page | Next Page