IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3490 documents. Displaying 25 entries per page.


Technical viability of deltamethrin as a pre-treatment wood preservative
1993 - IRG/WP 93-30012
This paper presents the results of tests conducted on freshly-cut logs and lumber during the seasoning period to verify the effectiveness of Deltamethrin on insect control. The tests were carried out in Quedas do Iguaçú, Paraná (southern region of Brazil) and Breves, Pará (northern region of Brazil) during the-dry and rainy seasons, and used different species of wood and insecticide/fungicide ...
A M F Oliveira, S Milano, J L A Bahia, F Teleginski


The environment and the timber preservation in the Benelux countries
1990 - IRG/WP 3580
The environment has become a major issue in all industries. To focus on the timber preservation industry an analysis is made of the production chain. Suggestions are made for diminishing or excluding emissions of agents of pollution. After a review of the legislation in Holland, some important statements are made on the production process, the products involved and the waste materials. Finally raw...
C De Mey, R Leegwater


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Treatment details for the field experiment to determine the performance of preservative treated hardwoods with particlar reference to soft rot
1977 - IRG/WP 384
These notes are compiled to complement and supplement Document No: IRG/WP/367 which described the plan for the treatment of the stakes, using a CCA preservative, for the field experiment. This document gives extra details of the treatment characteristics of the different timber species and as such may give IRG members useful information on the sapwood permeability of a range of hardwoods. The repo...
F W Brooks, M R Gayles


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Inorganic preservatives in wood dust - Cause of nasal cancer?
1997 - IRG/WP 97-50085
Since 1985 dust particles from beech and oak trees have been classified by the Senate Commission of the German Research Council (DFG) as being ,,working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials ,,with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues ...
A O Rapp, K Brandt, R-D Peek, U Schmitt


Effects of seed origin and site on both wood density and longitudinal fluid uptake of Sitka spruce (Picea sitchensis (Bong.) Carr.) with height in the tree grown in the United Kingdom
2002 - IRG/WP 02-40226
The variation in density and longitudinal fluid uptake was investigated in short specimens of wood taken from eight seed origins of Sitka spruce trees grown at two sites in the UK. Five trees of each seed origin at each site were sampled at three heights (1, 2 and 3 m above ground level). The density of the samples decreased with increasing height within the stem. This corresponded with increasin...
I Usta, M D C Hale


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Wood preservation using furanones derived from marine algae
2004 - IRG/WP 04-10506
Halogenated furanones that are analogues of natural compounds extracted from the red seaweed Delisea pulchra were examined in the laboratory for activity against termites and decay fungi. The furanones were found to have broad spectrum activity, some with solution strengths of 0.01% controlling Coptotermes acinaciformis in a filter paper trial, while 2% solutions impregnated into Pinus radiata blo...
L J Cookson, R de Nys, P Steinberg, N Chew


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...
M Maoz, J J Morrell


Transformation of Ophiostoma picea and Trichoderma harzianum with green fluorescent protein (GFP)
2003 - IRG/WP 03-10477
While microbial colonization of wood is presumed to be characterized by a myriad of interactions between numerous organisms, studying these processes is often difficult owing to the opaque nature of the wood and the inability to readily distinguish among the many species colonizing the material. One method for enhancing the ability to distinguish organisms is to induce specific proteins in one or ...
Ying Xiao, L M Ciuffetti, J J Morrell


Behavioural and morphological adaptations to tidal inundation in the adult wood boring weevil Pselactus spadix Herbst
1999 - IRG/WP 99-10308
Pselactus spadix tunnels wood in the mid intertidal to high intertidal zones and is submersed for several hours with each tide. The submergence and subsequent recovery behaviour, together with sub elytral morphology of P. spadix was investigated and compared to a terrestrial wood borer of the same subfamily Euophryum confine. An investigation of adult activity following submersion in seawater show...
P Oevering, A J Pitman


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Previous Page | Next Page