The mathematical study of test plot data
1987 - IRG/WP 2282
It has long been desirable to have a mathematical expression, which, by the insertion of statistically derived constants, would describe the behavior of test specimens in service. The philosophy of such expressions is briefly discussed, and the history of the concept is outlined. The modern approach to the problem dates from the graphical presentation of dosage-response and deterioration curves by...
W H Hartford


Fixation and leaching of selected Malaysian tropical hardwood after treated with CCA
2001 - IRG/WP 01-40207
The objective of this study is to investigate the fixation and leaching properties of selected Malaysian tropical hardwood (sentang wood (sapwood and heartwood) and rubberwood) after being treated with copper chrome arsenate (CCA) type-C preservative. The samples were treated with retention level of 0.5%, 2.0% and 5.0%. The samples were leached and the leachate were analyzed by AAS and the amount ...
R Hashim, O Sulaiman, Tan Siew Ching, K Yamamoto


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Low-toxicity DNBP wood preservatives
1987 - IRG/WP 3408
Low and very low toxicity single compound preservatives of both excellent insecticidal and fungicidal activity for interior, extrior and ground-contact applications are presented. These are ester derivatives of alkyl dinitrophenols, in particular of 2-sec-butyl-4,6-dinitrophenol (DNBP) and 2-sec-octyl-4,6-dinitrophenol. These esters, of much lower toxicity than DNBP impart to the treated timber co...
A Pizzi, W E Conradie, A Jansen, R Vosloo


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


A comparison of inductively coupled plasma spectroscopy and neutron activity analysis for the determination of concentrations in wood
1993 - IRG/WP 93-10048
As wood decays the ionic composition changes, with increases often being seen in the concentrations of Ca, Mg, Fe, Mn and sometimes K. The concentration of eight cations in red spruce sapwood and heartwood samples was determined independently by inductively coupled plasma spectroscopy (ICP) and by neutron activation analysis (NAA) as part of an effort to standardize our analytical procedures and c...
J Jellison, J Connolly, K C Smith, W T Shortle


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Performance of non-incised CCA-treated hem-fir decking
1993 - IRG/WP 93-40004
The question of what preservative penetration will provide an acceptable service life for treated wood in residential above-ground applications is topical in North American standards committees. Non-incised CCA-treated nominal 2 x 4 inch² hem-fir decking with penetrations close to the proposed CSA O80 2 decking standard of 80% over 5 mm, has remained without decay after 10 years exposure in south...
P I Morris, J N R Ruddick


Butt-end incising to improve penetration and retention of creosote in Eucalyptus saligna power transmission poles in Kenya. Preliminary results
2002 - IRG/WP 02-40249
Incising as a possible technique to improve penetration and retention of creosote in the butt end of Eucalyptus saligna power transmission poles in Kenya was investigated. Debarked, butt-end samples from whole poles were seasoned (15% MC), incised using four patterns of incisions, sealed at the top or small diameter end, and pressure treated with a mixture of creosote-furnace oil (60/40 mix) at a...
R Venkatasamy


A new method for the study of microbiological decay of wood in a strictly anaerobic environment
1988 - IRG/WP 2319
Recent work has suggested that strictly anaerobic bacteria may play a role in the biodeterioration of wood, particularly in aqueous environments. However, no suitable test methods exist for the investigation of this hypothesis. An aqueous minimal medium in specifically adapted conical flasks was sterilised, gassed using a 5.5% H2; 31.8% C02; 62.7% N2 gas mixture to remove oxygen and transferred to...
G M Rogers, A A W Baecker


Incising to improve penetration and retention of creosote in small-diameter Kenyan-grown Cypress (Cupressus lusitanica)
2003 - IRG/WP 03-40253
Turning small-diameter plantation thinnings into value-added products has remained a challenge in many countries, including Kenya. The present study reports on a feasible technique to effectively treat small-diameter cypress for use in ground contact. Samples of pole-size Cypress (Cupressus lusitanica), 106 mm and 138 mm in average diameter, were sampled from thinnings in 7 and 12 year-old plant...
R Venkatasamy


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Further thoughts on standard principles of testing termiticides and/or wood preservatives
1992 - IRG/WP 92-1530
At the last annual meeting in Kyoto, Japan, there was a special session devoted to the standard principles of testing termiticides. There was definitely a perceived need by researchers and industry for some guidelines that spell out basic procedures required for any methodology in testing termiticidal formulations anywhere in the world. In the testing of new potential active ingredients, considera...
J R J French


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller