Effects of fixation conditions and seawater on leaching of wood treated with marine retention CCA
1997 - IRG/WP 97-50088
The effect of post-treatment conditioning temperature and humidity on leaching of chromated copper arsenate (CCA) was compared in seawater and deionized water. Southern pine cubes treated to 40 kg/m3 CCA were stored at 2° C and 82% relative humidity (RH), 24° C and 65% RH, or 32° C and 30% RH for 3, 10, or 17 days. Cubes were then leached in deionized water or artificial seawater. The rate of l...
S T Lebow


Inorganic preservatives in wood dust - Cause of nasal cancer?
1997 - IRG/WP 97-50085
Since 1985 dust particles from beech and oak trees have been classified by the Senate Commission of the German Research Council (DFG) as being ,,working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials ,,with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues ...
A O Rapp, K Brandt, R-D Peek, U Schmitt


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...
M Maoz, J J Morrell


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


A comparison of the leaching resistance of diammine-copper complexes and copper carbonate precipitated in wood
1997 - IRG/WP 97-30158
Previous studies have shown that during treatment of wood with ammoniacal copper solutions, both simple copper precipitates and diammine-copper complexes are formed. The objective of the present study is to determine the relative importance of both forms of copper, on such aspects as preservative leachability and biological performance. In the current experiment, the leachability of copper carbona...
Xiao Jiang, J N R Ruddick


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Equilibrium distribution of toxic elements in the burning of impregnated wood
2001 - IRG/WP 01-50172
The current work focuses on predicting the behavior of arsenic, chromium, and copper in the burning of impregnated wood. A theoretical method is used to study the chemistry of the system, with special interest directed towards the vaporization tendency of the potentially toxic elements. The core of the study is the global equilibrium analysis that simultaneously takes into consideration all chemic...
K Sandelin, R Backman


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


Protection of wood blocks treated with Trichoderma isolates selected on the basis of preliminary agar screening studies
1996 - IRG/WP 96-10154
Previously reported results of agar interaction screening studies for biocontrol agents of wood decay basidiomycetes showed two Trichoderma viride isolates, killed 16 of 19 target fungi (Tucker and Bruce, 1995). Testing of these isolates in wood was required to assess their performance at preventing decay of wood blocks. Standard testing of chemical wood preservatives is used to determine the toxi...
E J B Tucker, A Bruce, H J Staines


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Determination of ethanolamine in impregnated wood
2000 - IRG/WP 00-20198
Leaching of copper based preservatives from wood is usually prevented by adding chromium compounds to copper containing formulations. It seems that suitable substitutes for chromium fixation agents may be amines. In this paper, we report our results on interactions between copper(II) octanoate and ethanolamine (C2H7NO, 2-aminoethanole) with wood or its components. A part of ethanolamine from a woo...
M Humar, M Petric


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


Recycling of treated timber by copper smelter
1994 - IRG/WP 94-50030
A preliminary trial was carried out to see whether copper smelting process is able to recycle CCA treated timber. As a result of the first trial almost a full recovery of both copper and arsenic was achieved. Recovered metals were utilized in manufacturing CCA preservatives. The energy bound in wood is utilized in the flash smelting process and the burning gases are fed to the sulphuric acid plant...
A J Nurmi, L Lindroos