IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3093 documents. Displaying 25 entries per page.


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss


Comparative evaluation of the barrier effect against Hylotrupes bajulus L. of different types of wood preservative
1986 - IRG/WP 1307
This paper settles the difference of contact action against females of Hylotrupes bajulus the likelihood of egg-laying, the ovicide effect and the hazards of development of newly hatched larvae between some preservatives belonging to three differents types: mineral waterborne products, organic products and emulsions. The results show that against females, the action is fast with organic products, ...
M-M Serment


Report of field test results for dichloro-n-octyl-isothiazolone: A potential new wood preservative
1988 - IRG/WP 3495
In a previous report (IRG/WP/3306) we presented preliminary laboratory test results on 4,5-dichloro-2-n-octyl-4-isothiazolone (RH 287). Laboratory data indicated toxic threshold values for RH 287 ranging from 0.37 to 0.50 kg/m³. In this report we present field test results on an IRG L-joint test and an in-ground stake test for RH 287, pentachlorophenol and biocide free test units. (a) L-joint tes...
D E Greenley, B M Hegarty


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


The formation of organotin carboxylates in bis(tributyltin) oxide - treated Pinus sylvestris sapwood
1990 - IRG/WP 3618
Tributyltin compounds have been successfully used for many years as wood preservatives, although their chemical nature in timber have not been fully elucidated. This study by 119Sn and 13C NMR spectroscopy has shown that, on impregnation into Pinus sylvestris sapwood, bis(tributyltin) oxide, (Bu3Sn)2O, is rapidly converted to tributyltin carboxylates, Bu3SnOCO·R, via reaction with components of t...
S J Blunden, R Hill


Oxygen index levels and thermal analysis of wood treated with melamine-formaldehyde-boron combinations
1997 - IRG/WP 97-30135
Melamine formaldehyde (MF) resin was impregnated into scots pine (Pinus sylvestris L.) specimens with aqueous solutions of 5, 10 and 20% concs. Boric acid (BA) and borax (BX) was added to MF resin at the concentration levels of 0.25, 1.00 and 4.70% to each level of resin concs. BA and BX mixture was prepared at the 5:1 (w/w) ratio considering resultant pH of solutions and better fire resistance. U...
M K Yalinkilic, W-Y Su, Z Demirci, E Baysal, M Takahashi, S Ishihara


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Kinetic modelling of adsorption of quaternary ammonium compounds by Scots pine wood sawdust (Pinus sylvestris L.)
2005 - IRG/WP 05-30369
The adsorption of new quaternary ammonium compounds from aqueous solutions onto Scots pine wood (Pinus sylvestris L.) sawdust was studied. The pseudo first- and second- order kinetic models were used for the mathematical description of the sorption dynamic process of QACs onto wood. The highest correlation coefficients were obtained for the pseudo-second order kinetic model, those suggest that che...
J Zabielska-Matejuk


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1977 - IRG/WP 288
G Castan


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


Differences in feeding activity among colonies of Formosan subterranean termite Coptotermes formosanus Shiraki
1983 - IRG/WP 1202
Feeding activities of 7 colonies of the Formosan subterranean termite, Coptotermes formosanus Shiraki, were examined. Wood-consumption rates among colonies differed significantly, ranging from 23.80-78.48 mg/g/day. This large intraspecific variation raised a question of whether differences in feeding activity reported for other termite species were due to interspecific differences. When rates were...
N-Y Su, J P La Fage


Wood preservatives ecotoxicology on Gammarus pulex (L.) - toward an environmental monitoring method and a getting rid of pollution process
2005 - IRG/WP 05-50224-9
Wood preservatives can have a strong impact on freshwater invertebrates when used close to aquatic ecosystems. It has been reported in Jura that different arthropod taxa, specially crustaceans, have disappeared along several kilometers downstream from factories using insecticides and fungicides as wood preservatives. The crustacean Gammarus pulex (L.) is a relevant bioindicator to characterize th...
O Adam, F Degiorgi, G Crini, P-M Badot


Previous Page | Next Page