IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3093 documents. Displaying 25 entries per page.


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Progress in Fire-Retardant Research on Wood and Wood-Based Composites: a China Perspective
2009 - IRG/WP 09-40476
The fire retardant research on wood and wood-based composites, which was carried out in China in the past two decades, was reviewed with 55 references. While many kinds of fire retardants for wood and wood-based composites have been studied, the mainstream is still the compound or the mixture containing phosphorus, nitrogen and boron elements, which can be used in the form of water solution in th...
Wang Qingwen, Wang Fengqiang, Hu Yunchu, Li Jian


Future Directions in Wood and Engineered Wood Products Research in China
2009 - IRG/WP 09-40479
This paper has summarized the research advance of basic wood science and engineered wood products in the 20th century in China and introduced the research advance and directions of basic wood science, engineered wood products and the extensive researches based on the basic wood science such as wood chemical rheology, wood fractal analysis, wood environmental science and nano-wood material etc in t...
Guangjie Zhao


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Application of Nanotechnology in Wood Preservation
2010 - IRG/WP 10-30542
Nanotechnology can enable the development of a wide range of new or enhanced wood-based materials and products that offer cost-effective substitutes for nonrenewable . Wood and other lignocelluloses are heterogeneous natural polymer composites with large variations in physical and chemical properties. These natural materials are composed of cellulose, lignin, and hemicelluloses. The potential use ...
M Akhtari, M Arefkhani


The situation of wood preservation in Italy
2010 - IRG/WP 10-40502
This document summarizes the situation of wood preservation in Italy at the present time. Information on the Italian climate and biological hazard of wood commodities are extracted and updated from a document of Gambetta et al., 1985. Data about wood production and industry are obtained by INFC, National Inventory of Forest and Forest Carbon Sink, by ISTAT, the National Institute of Statistics and...
E Conti, S Palanti


Climate change and wood protection, increasing demand of long life wood products and decreasing production of treated wood
2010 - IRG/WP 10-50269
Several new topics related to wood protection sector has appeared in Japan, as the awareness of climate change becomes bigger and bigger. The “Basic act for housing (2006)” and the “Long-life housing promotion act (2009)” were enforced to form a safe and high quality housing stock and to form a long-service-life housing respectively. Despite of the favorable background for wood protection ...
K Yamamoto, H Kato


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Optimization of the bi-oleothermal treatment process for wood preservation and fireproofing
2011 - IRG/WP 11-40566
The bi-oleothermal© process (combination of oil and heat treatment) is a well mastered alternative method for wood protection. However, the fire behavior and resistance to decay of bi-oleothermally treated wood are not good enough to ensure performance which meets the service standards for outdoor applications such as cladding or decking expected by the market. The aim of the present research pro...
F Simon, M Kutnik, M Goyer, M-F Thévenon, C Alfos, M Céron


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Smart hydrogels from low molecular weight amphiphilic compounds: toward a solution to decrease leachability and increase efficacy of boron preservatives?
2012 - IRG/WP 12-30589
A new catanionic system associating amphiphilic carnosine (AlaHisC8) and lauric acid forms supramolecular hydrogel at very low concentration. This gel was investigated and we have checked the validity of the concept of hydrogels utilization to reduce boron leachability and to develop new wood protection treatments. Impregnation with 5% aqueous borax solution (w/w) and 0.3% gelator agent (...
F Obounou Akong, P Gérardin, C Gérardin-Charbonnier


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Hydrogels: a solution to reduce boron leachability without reduction of its biodisponibility to wood decaying fungi?
2012 - IRG/WP 12-30602
Products used today for wood protection must fulfill to more and more environmental constraints, such as being of low toxicity in answer to the Biocidal Product Directory, but also to involve waterborne treatments to limit rejection of volatile organic compounds in the atmosphere. Boron preservatives have been described as valuable alternatives for wood protection for non-ground contact applicatio...
F Obounou Akong, P Gérardin, M-F Thévenon, S Parant, C Gérardin-Charbonnier


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


First report on the termiticidal activity of extracts of Annona squamosa (Annonaceae) seeds and on its active constituent squamocins
2012 - IRG/WP 12-30605
Termites inflict severe damage on wood commodities and impede usage of several forest species. The biological metabolites could potentially replace synthetic termiticidal products which are becoming more restricted to use. Annona squamosa is well known for its edible fruits - tropical custard apple. Annonaceous tetrahydrofuran acetogenins have attracted much interest due to their broad range of bi...
T S Djenontin, N Amusant, P H Ducrot, D C K Sohounhloué, D Pioch


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


Methylene Chloride compared with white spirit as a treatment solvent for wood preservation – results from decay and termite studies
2013 - IRG/WP 13-30611
Non-aqueous solvents have a long history in the treatment of wood products in various parts of the world. The most familiar solvent treatment is the ‘light organic solvent preservative’ (LOSP) treatment based on low density solvents such as white sprit. Until recently white spirit was the only non-aqueous solvent approved for use in wood preservation in New Zealand. Australia also permitted...
A Siraa, P Lobb, C Molloy


State of progress of utilisation of supramolecular gels for formulations of water-soluble wood preservation salts
2013 - IRG/WP 13-30630
This article is a compilation of the work done so far concerning the utilization of supramolecular hydrogels, built on low-molecular-weight amphiphilic molecules and containing boron salts conferring fungicidal properties. Mixing boron with thermoreversible hydrogels allows the formation of a supra molecular network incorporating boron and important amount of water upon gelification of the solutio...
F Obounou Akong, P Gérardin, M-F Thévenon, C Gérardin-Charbonnier


A Vision of the Chilean Treated Wood Industry
2013 - IRG/WP 13-40619
Chile is an important actor in the world wide forestry industry, activity which represents 3,1% of the Gross National Product (GNP). The wood products sector, which includes pulp and paper, is the second source of export in Chile with USD 6,500 millions income per year. Native species are the main forestry source with 15,9 millions has., but the principal commercial activity is based on 2,3 mil...
F J Latorre, T A Hanke


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Previous Page | Next Page