Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


Leachability of didecyldimethylammonium chloride (a quaternary ammonium compound) from four wood species
1982 - IRG/WP 3204
Sapwood blocks prepared from red pine, ponderosa pine, southern yellow pine and hem-fir (a commercial mixture of western hemlock and amabilis fir) were treated with didecyldimethylammonium chloride, (an alkylammonium compound, AAC). After oven drying the blocks were vacuum impregnated with distilled water and subjected to a static leach cycle for 48 hours. The leachate was analyzed and the amount ...
J N R Ruddick, A R H Sam


The selected properties of Scots pine wood blue-stained by fungus Cladosporium herbarum
2003 - IRG/WP 03-10484
The fungi causing primary blue-stain of wood may change wood properties especially when acting in mixture of few fungi species. There were been undertaken investigation to clear the influence of pure culture of one fungus species on selected physical and mechanical properties of Scots pine wood. The twin samples of fresh cut Scots pine sapwood (Pinus sylvestris L.) were exposed into pure culture o...
A Fojutowski


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 1: Optimisation of the extraction conditions
2000 - IRG/WP 00-30238
As the first phase of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, several solvents and extraction methods were evaluated, initially in the laboratory and then at pilot industrial scale. Extracts were compared by crude total dissolved solids content, by chemical analysis using GC-MS and LC-MS, and by laboratory...
M J Kennedy, Hui Jiang, L M Stephens


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 4: Analysis of extracts and treated wood for active components
2000 - IRG/WP 00-20215
In order to facilitate the commercial implementation of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, it has been essential to develop analytical methodology for the important bioactive components of the heartwood extract. This methodology will be used 1) to standardise the activity of successive production batc...
Hui Jiang, M J Kennedy, L M Stephens


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Assessing the leachability of chlorothalonil and methylene bis thiocyanate from antisapstain treated radiata pine
1998 - IRG/WP 98-30176
Rain wash-off and leaching of antisapstain fungicides from wood may cause pollution of waterways and may also lead to a decrease in the efficacy of a formulation against fungal degrade as chemicals deplete from the timber surface. In the current study, the leachability of chlorothalonil (CTL) and methylene bis thiocyanate (MBT), the active ingredients of a commercial antisapstain formulation, was...
B Kreber, T L Woods


Settlement of fouling organisms on CCA-treated Scots pine in the marine environment
1997 - IRG/WP 97-50094
As part of an EU project to investigate the effects of CCA loading on non-target marine fouling animals, exposure panels of Scots pine treated to 12, 24 and 48 kgm-3 CCA and untreated controls were submerged at seven coastal sites (Portsmouth, UK: Kristineberg, Sweden: La Tremblade (2 sites), France: Ria Formosa, Portugal: Sagres, Portugal: Athens, Greece). Inspections were made at 6 and 12 months...
C J Brown, R A Eaton


Use of mixed populations of microflora to control sapstain on radiata pine
2002 - IRG/WP 02-10427
Most methods of biological control in the wood products field have focused on the use of single species of fungi or bacteria to control sapstain or decay. The approach taken in this study involved applying soil microorganisms, in combination with nutrients and various adjuvants that collectively form the biological control system. Radiata pine branch discs, autoclaved or fresh, were dipped in ...
C Chittenden, R Wakeling, B Kreber


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


An optimum schedule for treating radiata pine
1998 - IRG/WP 98-40105
New Zealand grown radiata pine was treated with copper chrome arsenate preservative using Bethell process. Four different treatment schedules were tried. Keeping the duration of pressure stage constant (either 15 minutes or 45 minutes) and increasing the duration of vacuum (from 15 minutes to 30 minutes) or keeping the duration of vacuum stage constant (either 15 minutes or 30 minutes) and increas...
R Gnanaharan, D R Page


Improvement of intrinsic properties of wood by chemical wood densification - Hydrophobic aspects and durability aspects
1999 - IRG/WP 99-40149
To improve the intrinsic properties of Scot pine wood ((1) hydrophobic surface and (2) durability), two ways of chemical modification have been tested. The first one is the chemical modification of hydroxyl groups by active substances like diisocyanate compounds with a copolymerization step. The second way is a densification by an impregnation of resins and a gamma polymerisation. This second way ...
G Labat, Q K Tran, I Le Bayon


Water repellency of wood treated with alkylammonium compounds and chromated copper arsenate
2000 - IRG/WP 00-30231
The comparative water sorption properties of southern pine treated with CCA and several alkylammonium compounds was evaluated for freshly treated wood and for wood after exposure in a fungus cellar. It was found that CCA imparts considerable water repellency to wood which is reduced somewhat after exposure to wet soil. With the exception of a long chain (C20 -C22) compound, the alkylammonium compo...
D D Nicholas, A Kabir, A D Williams, A F Preston


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora


Leaching of preservative components from pine decking treated with CCA and copper azole, and interactions of leachates with soils
2001 - IRG/WP 01-50171
Radiata pine decking was treated with CCA and copper azole preservatives to Australian H3 retention using conventional and modified Bethel schedules, and air-dried. Treated decking boards and durable hardwood controls were subjected to leaching in weather-exposed decks, and matching 19mm cubes were leached in extended AWPA E11-97 lab tests. Deck runoff and E11 leachate water was analysed after rai...
M J Kennedy, P A Collins


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Sapstain development on Jack pine logs in Eastern Canada
2000 - IRG/WP 00-10358
During 1998-99, a study was initiated to investigate the influence of seasons, log types and storage time on the sapstain development on jack pine logs at two sites in Eastern Canada. Jack pine trees (Pinus banksiana) were harvested into whole-tree and cut-to-length logs in spring and in autumn. Sapstain development was examined in these logs at 2 to 4 week intervals after felling. The mean stain ...
Dian-Qing Yang, R Beauregard


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell